Queen's University at Kingston
Interrelationships between process conditions and material properties in Pellet-Fed Material Extrusion of Polylactic Acid
Abstract
dc:description.abstractPellet-fed material extrusion (PF-MEX) additive manufacturing offers significant advantages over filament-based systems by eliminating the intermediate filament production step, reducing costs, and enabling greater material flexibility. However, mechanical performance in PF-MEX-printed parts is governed by inter-strand bonding quality rather than bulk polymer properties, and for semicrystalline thermoplastics such as polylactic acid (PLA), the competition between crystallization kinetics and molecular interdiffusion at strand interfaces remains poorly understood. This thesis addresses two critical gaps: the lack of interface-sensitive mechanical test methods and the incomplete mechanistic understanding of how processing conditions affect interstrand bonding in semi-crystalline polymers. A modified tensile test using a single-layer coupon consisting of aligned strands was developed and validated as an interface-sensitive test method. This specimen geometry, in which the entire cross-section consists of a single inter-strand plane, consistently produced fracture along strand interfaces, confirming interface-dominated failure and providing superior repeatability compared to an alternative lap shear testing method. Using this test method, build-bed temperature effects on inter-strand bond strength were systematically quantified for an injection-molding grade PLA printed on a Tumaker Mini Modular PF-MEX system. Parts were printed under identical conditions, using deposition substrate temperatures ranging from 25–120°C. A non-monotonic, three-regime response was observed. Region I (25–55°C) exhibited the highest load-bearing capacity (243.5 N at 25°C) through mechanical interlocking via rapid quenching below the glass transition temperature, despite slow crystallization and predominantly amorphous interfaces. Region II (60–80°C) showed minimum bond strength (143.7 N at 65°C), coinciding with maximum crystallinity and fast crystallization kinetics; crystallization arrested healing before adequate interdiffusion, producing clean delamination fracture surfaces. Region III (90–120°C) demonstrated substantial recovery (227.2 N at 90°C, ~70% increase from minimum), as extended high-mobility time above the glass transition enabled significant interdiffusion before crystallization onset, resulting in lower crystallinity (8–12%) and cohesive bulk fracture at 120°C. The central finding is that the crystallization kinetics control interfacial healing in semi-crystalline PLA. This work establishes crystallization kinetics as a quantitatively characterizable determinant of interfacial bonding quality, providing a mechanistic framework for process optimization in PFMEX printing of semi-crystalline thermoplastics.
Degree
thesis:*- Department dc:contributor.department
- Chemical Engineering
- Grantor
- Queen's University at Kingston
- Year dc:date.issued
- 2026
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Abdi, Roxana
- Advisor dc:contributor.supervisor
-
- Marianna, Kontopoulou
Subjects
dc:subject × 3Rights
dc:rights- Statement dc:rights
-
- Attribution-NonCommercial-NoDerivatives 4.0 International
- Licence dc:rights.uri
- Language dc:language.iso
- eng
Identifiers
dc:identifier.*- Handle dc:identifier.uri
- https://hdl.handle.net/1974/36532