Time-resolved oxide evolution on 304L stainless steel in high-temperature water using In-Situ Raman spectroscopy

Abstract

dc:description.abstract

Austenitic stainless steels are widely used in water-cooled nuclear systems, where oxide films govern corrosion behaviour by controlling transport and interfacial reactions between structural components and high-temperature water. The chemistry, structure, and stability of these oxides can influence corrosion behaviour, corrosion product release, and the surface conditions associated with environmentally assisted degradation. However, oxide evolution is often interpreted from post-exposure characterization, which may not capture transient changes during exposure. This thesis develops and applies in-situ Raman spectroscopy to investigate time-resolved oxide evolution on 304L stainless steel in high-temperature water, with emphasis on material condition and dissolved oxygen history. A high-temperature and high-pressure recirculating autoclave loop coupled with in-situ Raman spectroscopy was commissioned and validated for corrosion studies. The facility enabled optical access to 304L stainless steel specimens through a sapphire window and allowed Raman spectra to be collected during exposure to controlled aqueous environments. Facility validation showed that Raman-visible spinel development could be tracked in real time at 300 °C. The facility was then applied to compare oxide development on as-received, 30% cold-worked, 0.1 dpa proton-irradiated, and 3.0 dpa proton-irradiated 304L stainless steel during exposure to oxygenated water at 300 °C containing 8 ppm dissolved oxygen. The as-received and 0.1 dpa specimens showed similar Raman responses, while the 3.0 dpa specimen showed an enhanced early oxidation response. The 30% cold-worked specimen showed the greatest Raman-visible spinel signal after 48 h, indicating that prior deformation can enhance oxide development under these conditions. The effect of dissolved oxygen history was examined by comparing sustained low dissolved oxygen exposure below 10 ppb with a controlled oxygenation step to 8 ppm dissolved oxygen at 300 °C. Oxygenation produced changes in spinel-band intensity, centroid, and band shape, and the cold-worked material showed a larger and faster response than the as-received material. These results show that the Raman-visible spinel response depends on both the prior condition of the alloy and the dissolved oxygen history of the environment. Overall, this thesis demonstrates that in-situ Raman spectroscopy can track time-dependent oxide changes on 304L stainless steel in high-temperature water and supports a path-dependent interpretation of stainless-steel oxide evolution.

Degree

thesis:*
Department dc:contributor.department
Mechanical and Materials Engineering
Grantor
Queen's University at Kingston
Year dc:date.issued
2026

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Ramsundar, Vindel Simeon
Advisors dc:contributor.supervisor
  • Persaud, Suraj
  • Daymond, Mark

Subjects

dc:subject × 8

Rights

Language dc:language.iso
eng

Identifiers

dc:identifier.*
Handle dc:identifier.uri
https://hdl.handle.net/1974/36922

Chain of custody

source
Harvested from
Queens University
Base URL
qspace.library.queensu.ca/server/oai/request
Last updated
2026-11-19
Source record
OAI-PMH GetRecord
citation

Ramsundar, Vindel Simeon. Time-resolved oxide evolution on 304L stainless steel in high-temperature water using In-Situ Raman spectroscopy. Queen's University at Kingston, 2026. https://hdl.handle.net/1974/36922