Sulfur Poisoning of Nickel Catalysts: Methane-Deuterium Exchange Reactions

Abstract

dc:description.abstract

The effects of sulfur poisoning on a nickel catalyst have been investigated using CH(,4)-D(,2) exchange reactions to monitor changes in the catalyst activity and selectivity. Mechanisms of the CH(,4)-D(,2) exchange reactions were also examined. The techniques employed include kinetic modeling, poisoning by pulse and flow methods, temperature programmed desorption (TPD), the thermogravimetric analysis (TGA). The catalyst used in the study contains 13% Ni (by weight) supported on a MgAl(,2)O(,4) carrier and has a BET surface area of 1.0 m('2)/g. Substantial increases in the catalyst activity were observed when the samples underwent a standard pretreatment in O(,2) at 475(DEGREES)C for 16 hours followed by a reduction in H(,2) at 525(DEGREES)C for 2 hours. The catalyst activation is believed to result from redispersion of nickel crystallites during oxidation. Two primary products, CD(,4) and CH(,3)D, were observed from the CH(,4)-D(,2) exchange reactions. The independent reactions responsible for the above products are multiple exchange and simple exchange. The multiple exchange is thought to occur via dissociative adsorption of CH(,4) on 7 nickel sites followed by rapid isotopic exchange of adsorbed H atoms with the gas phase deuterium. A kinetic expression based on the above model describes the experimental data quite well. It is proposed that CH(,3)D is the product of a reaction between the gas phase CH(,4), an adsorbed D atom, and an adjacent vacant Ni site. This model is supported by good agreement between the observed rates and the rates predicted by the developed kinetic expression. Sulfur poisoning by both pulse and flow methods (using H(,2)S as the poisoning compound) resulted in a linear decrease in the catalyst activity. However, no variations in either the selectivity (for CD(,4) and CH(,3)D) or activation energies of the exchange reactions were observed. Results from the poisoning experiments and H(,2)S absorption isotherms showed evidence of diffusion control for H(,2)S adsorption. A pore mouth poisoning model adequately describes the catalyst deactivation. The sulfur capacity of the nickel surface has been estimated as 8 x 10('14) S atoms/cm('2) Ni. The poisoned catalyst was partially regenerated by treatment in O(,2) at 475(DEGREES)C for an hour and reduction in H(,2) at 480(DEGREES)C for 2 hours. It was determined from the TPD experiments that, during this treatment, sulfur is removed in the form of SO(,2).

Degree

thesis:*
Name thesis:degree_name
Doctor of Philosophy
Level thesis:degree_level
Doctoral
Discipline thesis:degree_discipline
Engineering
Department thesis:degree_department
Chemical Engineering
Grantor
Rice University
Year dc:date.issued
1981

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Chahar, Bharat Singh

Subjects

dc:subject × 1

Rights

dc:rights
Statement dc:rights
  • Copyright is held by the author, unless otherwise indicated. Permission to reuse, publish, or reproduce the work beyond the bounds of fair use or other exemptions to copyright law must be obtained from the copyright holder.
Language dc:language.iso
eng

Identifiers

dc:identifier.*
Dc Identifier Callnumber
THESIS CH.E. 1981 CHAHAR
Dc Identifier Citation
Chahar, Bharat Singh. "Sulfur Poisoning of Nickel Catalysts: Methane-Deuterium Exchange Reactions." (1981) Diss., Rice University. https://hdl.handle.net/1911/15599

Chain of custody

source
Harvested from
Rice University
Base URL
repository.rice.edu/server/oai/request
Last updated
2026-11-19
Source record
OAI-PMH GetRecord
citation

Chahar, Bharat Singh. Sulfur Poisoning of Nickel Catalysts: Methane-Deuterium Exchange Reactions. Doctoral thesis, Rice University, 1981. https://hdl.handle.net/1911/15599