University of Saskatchewan
Hydrogen in pipeline steels under electrochemical and gaseous environments
Abstract
dc:description.abstractHydrogen embrittlement compromises the structural integrity of pipeline steels in aqueous and gaseous environments, posing significant challenges to the oil and gas industry. The transition toward a hydrogen economy, driven by global warming concerns, has also highlighted the importance of developing failure-resistant and dedicated pipelines for hydrogen gas transportation. As a result, a good understanding of hydrogen behavior in steels under various service conditions is crucial. While electrochemical hydrogen charging in aqueous solutions is easily accessible and quite flexible, testing in pressurized hydrogen gas environment involves several safety and technical limitations. So, establishing equivalence in hydrogen uptake between these charging methods would be beneficial. This study investigates hydrogen uptake behavior and equivalence in pipeline steels subjected to gaseous and electrochemical charging. Through detailed microstructural characterization, mechanical testing, hydrogen diffusion and trapping studies, synchrotron X-ray diffraction, thermal desorption analysis, and other experimental analyses, the relationship between hydrogen ingress and steel microstructures was explored. The results showed that hydrogen ingress, trapping and retention are strongly influenced by various microstructural characteristics of steel. This hydrogen retention capability and accumulation behavior in steels, especially in reversible traps, directly impacted their hydrogen embrittlement susceptibility. High hydrogen retention in a steel sample led to a reduction in ductility of over 98%, resulting in brittle fracture. This transition from plasticity-based to decohesion-based failure was attributed to the hydrogen concentration in the steel exceeding a certain threshold value, which aligns with the hydrogen embrittlement model which proposes a synergistic action between the hydrogen-enhanced localized plasticity (HELP) and hydrogen-enhanced decohesion (HEDE) mechanisms, i.e. the HELP + HEDE model. Dislocation density and phase composition played more significant roles in hydrogen dissociation, absorption, and retention than crystallographic texture and grain size. And an increase in dislocation density (and defect density) through cold rolling enhanced hydrogen uptake by orders of magnitude when compared to microstructures with very low dislocation density, such as fully annealed steels. With regards to crystallographic texture, the <111>//ND and <100>//ND orientations exhibited better corrosion resistance and slightly lower hydrogen uptake compared to random textures. The choice of electrolyte significantly influenced surface corrosion and hydrogen uptake. The 0.1 M NaOH electrolyte showed negligible surface corrosion and hydrogen desorption behaviors comparable to gaseous charging, making it suitable for equivalence studies. In contrast, 0.1 M H₂SO₄ and 3.5 wt.% NaCl electrolytes caused substantial surface corrosion. The corrosion rates of an annealed steel sample in these electrolytes were obtained as 0.231 mm/yr, 0.050 mm/yr and 0.003 mm/yr in the 0.1 M H₂SO₄, 3.5 wt.% NaCl and 0.1 M NaOH electrolytes, respectively. The comparative analysis revealed that both charging methods induce compressive strains in steels, with magnitudes dependent on the steel microstructure and charging parameters. Thermal desorption results confirmed similarities in hydrogen trapping for both methods under specific conditions like suitable electrolyte (0.1 M NaOH). Variations in the surface, subsurface, and bulk hydrogen trapping were observed due to differences in electrolyte composition, recombination poison addition, applied current density, and steel microstructure. Very high hydrogen activity or fugacity on the steel surface facilitated hydrogen accumulation at the surface and subsurface regions, and this accumulation is controlled by the microstructural characteristics of the steel. Using the 0.1 M NaOH electrolyte, this study demonstrated that equivalent hydrogen uptake can be obtained based on the hydrogen fugacity at the steel surface. An equation to describe the hydrogen fugacity vs. overpotential relationship of X70 pipeline steel (bainitic ferrite microstructure) or steels with similar microstructures was proposed and validated. A fixed H₂ gas pressure of 10.34 MPa (1500 psi) yielded hydrogen concentrations comparable to samples charged with an electrochemical overpotential of -0.7 V. Hence, providing a practical benchmark for correlating both charging methods for similar pipeline steel microstructures.
Degree
thesis:*- Name thesis:degree_name
- Doctor of Philosophy (Ph.D.)
- Level thesis:degree_level
- Doctoral
- Discipline thesis:degree_discipline
- Mechanical Engineering
- Department thesis:degree_department
- Mechanical Engineering
- Grantor
- University of Saskatchewan
- Year dc:date.issued
- 2025
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Jack, Tonye Alaso
- Advisor dc:contributor.advisor
-
- Szpunar, Jerzy
- Committee members dc:contributor.committeemember
-
- Oguocha, Ikechukwuka
- Cree, Duncan
- Odeshi, Akindele
- Meda, Venkatesh
- Dalai, Ajay
- Omanovic, Sasha
- ORCID person:identifier.orcid
Subjects
dc:subject × 7Rights
- Language dc:language.iso
- en
Identifiers
dc:identifier.*- Handle dc:identifier.uri
- https://hdl.handle.net/10388/17056