Investigating the susceptibility of X80 line pipe weld to hydrogen-induced damage

Abstract

dc:description.abstract

To meet the increasing demand for oil and gas in the years ahead, pipeline infrastructure must resist failure to ensure safe, efficient transport of these resources. Failure in pipeline infrastructure frequently occurs in weld zones due to microstructural heterogeneity in phase compositions, grain boundaries and local misorientations, and the presence of non-metallic inclusions and precipitates. In this study, microstructural pathways for hydrogen-induced damage in X80 line-pipe steel weld were investigated using quantitative microstructural analysis, electrochemical hydrogen charging, the hydrogen microprint technique, electrochemical permeation, and corrosion testing. The ductile-to-brittle transition temperature of the weld metal and base metal was measured using Charpy V-notch impact tests (0 to -65 °C), along with additional supportive results from tensile tests and Vickers microhardness measurements. At the initial examination, the fusion zone and fusion line, zones known as weld metal, were the most susceptible to hydrogen-induced cracking, blistering, and micro pitting, with these damages primarily observed in the weld middle. Based on microstructural observations, such damages were observed at interfaces between allotriomorphic ferrite and acicular ferrite in the fusion zone, and tempered martensite and bainitic ferrite in the fusion line, where increased hydrogen trapping was observed. This microstructural heterogeneity arose from differences in kernel average misorientation between allotriomorphic ferrite and acicular ferrite, and higher kernel average misorientation in bainitic ferrite and tempered martensite, increasing hydrogen trapping. Tempered martensite with spheroidal cementite traps partially less hydrogen than bainitic ferrite with lamellar cementite. Non-metallic inclusions (Al₂O₃, MnS) and (Nb, Ti) (C, N) precipitates were also present within cracks. Compared to the base metal, weld metal exhibited higher hydrogen-trapping site density and solubility, along with reduced corrosion resistance. Additionally, weld metal showed lower low-temperature toughness and lower ductility in the non-hydrogen-charged condition. This reduced toughness and ductility corresponded to higher susceptibility to hydrogen-related degradation.

Degree

thesis:*
Name thesis:degree_name
Master of Science (M.Sc.)
Level thesis:degree_level
Masters
Discipline thesis:degree_discipline
Mechanical Engineering
Department thesis:degree_department
Mechanical Engineering
Grantor
University of Saskatchewan
Year dc:date.issued
2025

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • AMIR JANI, NEMAT
Advisors dc:contributor.advisor
  • Szpunar, Jerzy
  • Odeshi, Akindele
Committee members dc:contributor.committeemember
  • Acharya, Bishnu
  • Yang, Qiaoqin

Subjects

dc:subject × 5

Rights

Language dc:language.iso
en

Identifiers

dc:identifier.*
Handle dc:identifier.uri
https://hdl.handle.net/10388/17219

Chain of custody

source
Harvested from
University of Saskatchewan
Base URL
harvest.usask.ca/server/oai/request
Last updated
2026-11-19
Source record
OAI-PMH GetRecord
citation

AMIR JANI, NEMAT. Investigating the susceptibility of X80 line pipe weld to hydrogen-induced damage. Masters thesis, University of Saskatchewan, 2025. https://hdl.handle.net/10388/17219