Back to search

University of Southampton

Simultaneous time resolved XAS, IR and mass spectrometric characterisation of catalytic systems : an investigation into the structure-function behaviour of supported rhodium catalysts

Abstract

dc:description.abstract

<p>The techniques of Energy Dispersive Extended X-ray Absorption Fine structure (EDE), Diffuse Reflectance Fourier Transform Infrared Spectroscopy (DRIFTS) and mass spectrometry have been successfully combined in an in situ, time resolved manner to investigate the structure function surface chemistry of γ-Al<sub>2</sub>O<sub>3</sub> supported Rh catalysts.</p> <p>Catalysts with a low meal loading (2.5 wt%) were subject to facile disruption upon exposure to CO; the formation of discrete Rh(CO)<sub>2</sub> units was facilitated at higher temperatures. The proportion of dicarbonyl adopting this site was significantly less at higher metal loading (5 wt%), this was reflected by the IR and unchanging EXAFS data. </p> <p>The formation of ‘high wavenumber’ Rh(NO)<sup>-</sup> and Rh(NO)<sub>2</sub> species could be correlated to the rapid, extensive oxidation of Rh at low temperatures upon exposure to NO. The reactive turnover of NO and increased rate of oxidation were observed at higher temperatures, and evidence for a highly transient form of Rh(NO)<sub>2</sub> to yield a linear Rh(NO)<sup>+</sup> ‘spectator’ species was derived. Re-reduction of the oxide proceeded at temperatures as low as 373K.</p> <p>A gas switching regime between CO and NO showed an almost static oxidic Rh phase to exist at low temperatures; structural changes were more substantial at higher temperatures and followed the pattern of switching more closely. With NO in excess the Rh clusters oxidised rapidly to yield the Rh(NO)<sup>+</sup> species; reclustering was observed under CO, which also adopted linear and bridging sites on the metallic particles.</p> <p>The poisoning of the catalysts reported SO<sub>2</sub> to subtly modify the structure of the Rh but did not adversely affect the reduction of NO by H<sub>2</sub>. In contrast, complete and irreversible sulfidation of the nanoparticles rapidly curtailed catalysis upon exposure to H<sub>2</sub>S.</p>

Degree

thesis:*
Name dc:type.qualificationname
Ph.D.
Level dc:type.qualificationlevel
doctoral
Grantor dc:publisher.institution
University of Southampton
Year dc:date.issued
2006

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Jyoti, Bhrat

Rights

Language dc:language
English, eng

Chain of custody

source
Harvested from
University of Southampton
Base URL
eprints.soton.ac.uk/cgi/oai2
Last updated
2026-11-19
Source record
OAI-PMH GetRecord
related terms
citation

Jyoti, Bhrat. Simultaneous time resolved XAS, IR and mass spectrometric characterisation of catalytic systems : an investigation into the structure-function behaviour of supported rhodium catalysts. doctoral thesis, University of Southampton, 2006.