Back to search

University of Southampton

Low-temperature Al2O3/ZnO thin-film transistors for 3D heterogeneous integration: interface engineering, bias stress instability, and reliability mechanisms

Abstract

dc:description.abstract

Back-end-of-line (BEOL) process scaling and the emergence of three-dimensional heterogeneous integration (3D-HI) demand thin-film transistors (TFTs) that can be integrated within a limited thermal budget while maintaining high electrical performance (µ<sub>FE</sub> > 10 cm<sup>2</sup> V<sup>−1</sup> s <sup>−1</sup> ), long-term reliability (|∆V<sub>TH</sub>| < 0.5 V after 1 h stress), and low manufacturing cost. Zinc oxide (ZnO) has attracted sustained interest as a channel material owing to its wide bandgap (∼3.3 eV), optical transparency, and compatibility with low-temperature processing. However, the stability of ZnO TFTs remains a major bottleneck, particularly in devices employing atomic-layer-deposited (ALD) aluminium oxide (Al<sub>2</sub>O<sub>3</sub>) gate dielectrics, where the dielectric/semiconductor interface critically governs bias-stress degradation. This thesis systematically investigates the interdependence between Al<sub>2</sub>O<sub>3</sub> deposition temperature (150–300 <sup>◦</sup>C), interface-trap density (D<sub>it</sub>), and bias-stress instability mechanisms in ZnO TFTs. A unified device platform was developed, incorporating both global p-Si bottom gates and patterned AZO bottom gates, enabling separation of intrinsic dielectric effects from gate-geometry-induced field crowding. Cross-sectional transmission electron microscopy (TEM), together with SILVACO/TCAD simulations, confirms the presence of localised electric-field enhancement at wet-etched sharp gate corners, which promotes percolation-type leakage paths and soft breakdown, particularly under high drain bias (V<sub>D</sub> = 15 V), where threshold-voltage shifts exceeding 1.2 V are observed. A clear trade-off between mobility and reliability is identified as a function of Al<sub>2</sub>O<sub>3</sub> deposition temperature. Devices fabricated with Al<sub>2</sub>O<sub>3</sub> deposited at 150<sup> ◦</sup>C exhibit lower field-effect mobility (µ<sub>FE</sub> ≈ 4.8 cm<sup>2</sup> V<sup>−1</sup> s<sup> −1</sup> ) yet the most stable behaviour, with small hysteresis (< 0.2 V) and reduced trap density (N<sub>trap</sub> ∼ 3 × 10<sup>12</sup> cm<sup>−2</sup> ), consistent with hydrogen-assisted defect passivation. By contrast, films deposited at 300 <sup>◦</sup>C are denser and yield higher mobility (µ<sub>FE</sub> ≈ 8.7 cm<sup>2</sup> V<sup>−1</sup> s <sup>−1</sup> ), but suffer from substantially increased hysteresis (> 1.0 V) and higher trap density (N<sub>trap</sub> > 1 × 10<sup>13</sup> cm<sup>−2</sup> ). Capacitance–voltage (C–V) analysis shows a dielectric constant of k ≈ 8.2 and a stable oxide capacitance (C<sub>ox</sub> ≈ 7.5 × 10<sup>−7</sup> F cm<sup>−2</sup> ). Under positive bias stress (PBS, +10 V) in the dark, significant charge trapping is observed with ∆V<sub>TH</sub> up to +2.3 V, whereas negative bias stress (NBS) in the dark is comparatively weak (∆V<sub>TH</sub> > −0.2 V), consistent with limited de-trapping dynamics in p-Si gated structures. Optical excitation at 365 nm (photon energy ∼3.4 eV) profoundly alters the stress response through photo-generated carriers. Under illumination, PBS exhibits an initial rapid ∆V<sub>TH</sub> shift (e.g., ∼ +0.8 V within 60 s), followed by partial saturation consistent with enhanced de-trapping. Conversely, NBS becomes strongly destabilising, producing large negative shifts (e.g., −1.5 V after 1 h) accompanied by marked subthreshold-slope degradation. These results demonstrate that illumination accelerates both trapping and de-trapping processes and highlights the dynamic charge balance at the Al<sub>2</sub>O<sub>3</sub>/ZnO interface. By synthesising structural, chemical, and electrical analyses, this thesis establishes a comprehensive reliability map for Al<sub>2</sub>O<sub>3</sub>/ZnO TFTs under BEOL-compatible conditions. Three practical design strategies are proposed: (i) gate-geometry engineering to mitigate field crowding and suppress edge-initiated percolation leakage, (ii) interface/dielectric optimisation using lower deposition temperatures (typically ≲ 200 <sup>◦</sup>C) to leverage hydrogen-assisted passivation, and (iii) control of plasma chemistry during PEALD to reduce sub-oxide defects. Collectively, these principles provide a pathway to stabilise oxide TFTs for 3D-HI platforms, flexible electronics, and low-power integrated systems.

Degree

thesis:*
Name dc:type.qualificationname
Ph.D.
Level dc:type.qualificationlevel
doctoral
Grantor dc:publisher.institution
University of Southampton
Year dc:date.issued
2026

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Zeng, Jiale
Advisor dc:contributor.advisor
  • Chong, Harold
ORCID person:identifier.orcid

Rights

Language dc:language
English, eng

Chain of custody

source
Harvested from
University of Southampton
Base URL
eprints.soton.ac.uk/cgi/oai2
Last updated
2026-11-19
Source record
OAI-PMH GetRecord
related terms
citation

Zeng, Jiale. Low-temperature Al2O3/ZnO thin-film transistors for 3D heterogeneous integration: interface engineering, bias stress instability, and reliability mechanisms. doctoral thesis, University of Southampton, 2026.