Polypropylene/thermoplastic polyurethane blends for high voltage applications

Abstract

dc:description.abstract

This work presents the influence of varying thermoplastic polyurethane (TPU) and maleic anhydride (MA) concentrations on the structure and properties of isotactic polypropylene (iPP)/TPU blends. The study aims to elucidate structure-property relationships in iPP-based blends and evaluate their potential for high voltage (HV) applications.<br/>The first stage of this study examined how different contents of TPU are associated with changes in the morphology, thermal, mechanical, and electrical properties of iPP-based blends. The results showed that incorporation of TPU had no significant effect on the thermal characteristics of the blends, with comparable melting and crystallization temperatures and crystal thickness to iPP, and only minor changes in iPP phase crystallinity. However, higher TPU fraction led to more pronounced phased phase separation and morphological inhomogeneity, characterized by the enlargement of TPU-rich regions areas increasing from approximately 95 to 870 μm2 and increased heterogeneity in the crystalline features. This is attributed to the poor compatibility between iPP and TPU phase. Although TPU incorporation improved the flexibility of iPP, higher TPU contents were accompanied by reductions in tensile strength and elongation at break, with the 50/50 blend exhibiting brittle behaviour. The formation of heterogeneous interfacial morphology introduces electrically weak regions, resulting in substantial reductions in characteristic alternating current (AC) and direct current (DC) breakdown strength (BDS) of 21.7-61.1% and 40.1-67.7%, respectively, relative to iPP. Increasing TPU content also increased the permittivity and dielectric loss, suggesting more pronounced interfacial polarization. Meanwhile, the conductivity increased and the transition field (Et) shifted towards lower electric fields, suggest facilitated field-assistant charge transport. This was accompanying with greater space charge accumulation and local electric field distortion. In addition, higher TPU contents were associated with an increase in physical defects arising from morphological heterogeneity and shallow trapping states, facilitating faster charge dissipation during depolarization and reducing residual charge accumulation.<br/>To address the structure heterogeneity observed in non-compatibilized iPP/TPU blends, maleic anhydride grafted polypropylene (MA-PP) was introduced as a compatibilizer, and the second stage further investigated the morphological changes and the above-mentioned properties of compatibilized iPP/TPU blend. The addition of MA resulted the formation of imide structure between urethane N-H groups in TPU hard segments and the anhydride carbonyl (C=O) in MA groups. In addition, MA additions of up to 1 wt.% promoted a more homogeneous morphology and a narrower crystal size distribution while suppressing TPU domains agglomerates, reflecting improved compatibility between the blend phases. The more uniform morphology was accompanied by significant improvements in both mechanical and electrical performance, while the thermal characteristics were not substantially altered. Specifically, compared with the corresponding non-compatibilized blends, an appropriate amount of MA promoted improved flexibility and tensile strength. For instance, in 90/10 system, 0.2-0.4 wt.% MA further reduced Young’s modulus by approximately 6.3% and increased the strain at break to 556%, comparable to iPP. At 1 wt.% MA, the ultimate tensile strength (UTS) increased to 33.9 MPa, close to that of iPP (34.0 MPa). For the 70/30 and 50/50 blends, 0.4 wt.% MA substantially increased the strain at break to 521% and 576% and the UTS to 31.9 and 32.0 MPa, respectively. In terms of electrical performance, the maximum increases in AC and DC BDS ranged from 28.5.9-58.2% and 28.9-65.0%, respectively, across the three blend systems. The addition of 0.2-0.4 wt.% MA caused no significant increase dielectric permittivity at power frequency and 1 kHz, while slightly reducing dielectric loss relative to the non-compatibilized blends at power. In addition, MA contents up to 1 wt.% reduced conductivity and shifted Eₜ towards higher electric fields in the 90/10 and 70/30 systems. Furthermore, reduced physical defects were associated with a lower trap population, suppressing space charge accumulation and lower the residual charge after depoling.<br/>Overall, the study establishes relationships between morphology, thermal, mechanical and electrical performance of iPP/TPU/MA-PP blends. increasing TPU content intensified phase separation and structural heterogeneity, improving flexibility but compromising mechanical and electrical performance, while having only minor effects on thermal characteristics. appropriate MA-PP contents mitigated these structural inhomogeneities and consequently improved both mechanical and electrical properties. The findings highlight the potential of compatibilized PP-based insulation materials for HV applications including cable accessories such as joints and terminations, as well as capacitors, attributable to the favourable combination of mechanical flexibility and electrical performance exhibited by these blends.

Degree

thesis:*
Name dc:type.qualificationname
Ph.D.
Level dc:type.qualificationlevel
doctoral
Grantor dc:publisher.institution
University of Southampton
Year dc:date.issued
2026

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Wang, Xiaobing
Advisors dc:contributor.advisor
  • Andritsch, Thomas
  • Vryonis, Orestis
  • Saeedi, Istebreq

Rights

Language dc:language
English, eng

Identifiers

dc:identifier.*

Chain of custody

source
Harvested from
University of Southampton
Base URL
eprints.soton.ac.uk/cgi/oai2
Last updated
2026-11-19
Source record
OAI-PMH GetRecord
related terms
citation

Wang, Xiaobing. Polypropylene/thermoplastic polyurethane blends for high voltage applications. doctoral thesis, University of Southampton, 2026. https://doi.org/10.5258/SOTON/01/T294