Texas State University
Characterization of InAs Quantum Dots in InP Nanowires Using a Kelvin Probe Force Microscopy
Abstract
dc:description.abstractCoupled multiple quantum dots (QDs) have been attracting significant attention because of their use in quantum information processing. To fabricate coupled QD devices, we use semiconductor nanowires (NWs) which contains QDs inside. The nanowires typically exhibit diameters ranging from 30 to 60nm and lengths spanning from 1 to 3µm. To conduct a comprehensive characterization of these nanowires and fabricate the devices, it is imperative to transfer the NWs from the substrate on which they are grown (growth substrate) onto another substrate on which the devices are fabricated (device substrate). In the scanning electron microscope (SEM), a growth substrate and a device substrate are mounted to the same sample holder. To enhance the control in characterizing and testing nanowires, we used a sharp metallic (tungsten) probe having a tip radius of 0.5 µm with a taper angle 8-10 degrees for the NW transfer challenges that arise during the transfer process due to the substantial size difference between the probe and the nanowires. We applied a negative bias voltage of 4V to the probe for transferring these vertically grown nanowires. The process involves initially detaching the NWs from the growth substrate and then lifting them using a probe tip. Breaking nanowires using the electrostatic force is a delicate process because when dealing with highly flexible NWs, they tend to jump away due to the accumulated elastic energy at the breaking point. To address this, the nanowires are carefully broken near their bases. This is accomplished by gradually bringing the probe tip into contact with the base of an NW, and upon contact, gently applying a force by pushing the NW until the wire breaks. To release the nanowire, the probe tip is slowly positioned above the device substrate. Once the contact is detected between the NW and the device substrate, a positive bias voltage of 10V is applied to the probe tip. When the nanowire is held only at one of its ends, it promptly responds to the attractive forces of van der Waals emanating from the substrate, and the NW is released from the probe. After transferring the NWs, the Contact Potential difference(CPD) between the AFM tip and NWs is measured in Frequency Modulation (FM) KPFM by Pt deposited sharp tip.
Degree
thesis:*- Name thesis:degree_name
- Master of Science
- Level thesis:degree_level
- Masters
- Discipline thesis:degree_discipline
- Physics
- Department thesis:degree_department
- Physics
- Grantor
- Texas State University
- Year dc:date.issued
- 2024
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Dhakal, Ujjwal
- Advisor dc:contributor.advisor
-
- Miyahara, Yoichi
- Committee members dc:contributor.committeemember
-
- Satchell, Nathan
- Mahato, Dip N.
Subjects
dc:subject × 2Rights
- Language dc:language.iso
- en
Identifiers
dc:identifier.*- Dc Identifier Citation
- Dhakal, U. (2024). Characterization of InAs quantum dots in InP nanowires using a Kelvin probe force microscopy. [Master's thesis, Texas State University].