Back to search

University of Toronto

Interface Properties of the Amorphous Silicon/Crystalline Silicon Heterojunction photovoltaic cell

Abstract

dc:description.abstract

Amorphous-crystalline silicon (a-Si:H/c-Si) heterojunctions have the potential of being a very high efficiency silicon photovoltaic platform technology with accompanying cost and energy budget reductions. In this research a heterojunction cell structure based on a-Si:H deposited using a DC saddle field plasma enhanced vapour deposition (DCSF PECVD) technique is studied, and the a-Si:H/c-Si and indium tin oxide/a-Si:H interfaces are examined using several characterization methods.Photocarrier radiometry (PCR) is used for the first time to probe the a-Si:H/c-Si junction. PCR is demonstrated as a carrier lifetime measurement technique - specifically, confirming carrier lifetimes above 1 ms for 1-5 Ohm.cm phosphorous-doped c-Si wafers passivated on both sides with 30 nm of i-a-Si:H. PCR is also used to determine surface recombination velocity and mobility, and to probe recombination at the a-Si:H/c-Si interface, distinguishing interface recombination from recombination within the a-Si:H layer or at the a-Si:H surface.A complementary technique, lateral conductivity is applied over a temperature range of 140 K to 430 K to construct energy band diagrams of a-Si:H/c-Si junctions. Boron doped a-Si:H films on glass are shown to have activation energies of 0.3 to 0.35 eV, tuneable by adjusting the diborane to silane gas ratio during deposition. Heterojunction samples show evidence of a strong hole inversion layer and a valence band offset of approximately 0.4 eV; carrier concentration in the inversion layer is reduced in p-a-Si:H/i-a-Si:H/c-Si structures as intrinsic layer thickness increases, while carrier lifetime is increased.The indium tin oxide/amorphous silicon interface is also examined. Optimal ITO films were prepared with a sheet resistance of 17.3 Ohm/square and AM1.5 averaged transmittance of 92.1%., for a film thickness of approximately 85 nm, using temperatures below 200 degrees celcius. Two different heat treatments are found to cause crystallization of ITO and to change the properties of the underlying a-Si:H film.Finally, an open circuit voltage of 699 mV was achieved using DCSF PECVD in the tetrode configuration to fabricate a metal/ITO/p-a-Si:H/i-a-Si:H/n-c-Si/i-a-Si:H/n+-a-Si:H/metal photovoltaic cell on a texturized wafer. The 4 cm2 cell had an efficiency of 16.5%, a short circuit current of 36.4 mA/cm2 and a fill factor of 64.7%.

Degree

thesis:*
Department dc:contributor.department
Electrical and Computer Engineering
Year dc:date.issued
2015

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Halliop, Basia
Advisor dc:contributor.advisor
  • Kherani, Nazir P

Subjects

dc:subject × 6

Identifiers

dc:identifier.*
Handle dc:identifier.uri
https://hdl.handle.net/1807/69015

Chain of custody

source
Harvested from
University of Toronto
Base URL
utoronto.scholaris.ca/server/oai/request
Last updated
2026-11-19
Source record
OAI-PMH GetRecord
citation

Halliop, Basia. Interface Properties of the Amorphous Silicon/Crystalline Silicon Heterojunction photovoltaic cell. 2015. https://hdl.handle.net/1807/69015