Back to search

University of Toronto

Thermodynamics of Impurity Removal in Solvent Refining of Silicon

Abstract

dc:description.abstract

In a new approach to metallurgical refining of silicon by solvent refining, iron has been successfully utilized as the getter element. Unlike most metallic impurities, phosphorus and boron have relatively large distribution coefficients that render them unresponsive to solidification refining processes. Consequently it is crucial to study the efficiency of phosphorus and boron removal through solvent refining with iron. This research focuses on thermodynamics of phosphorus and boron distribution between silicon crystals and the iron-silicon melt. Aiming to establish the thermodynamic fundamentals of the process, the present study was performed to investigate the distribution coefficient of phosphorus and boron between silicon and the alloy melt. Based on the values obtained for distribution coefficient of phosphorus and boron at different temperatures, impurity removal is 2-3 times more effective compared with conventional directional solidification process. The values of interaction parameter of phosphorus on iron were obtained as -5297±359 (1310 °C), -4324±292 (1260 °C) and -2893±268 (1210 °C). The values of interaction parameter of boron on iron were: -813±53 (1310 °C), -830±92 (1260 °C), -863±91 (1210 °C). Large negative values obtained for both interaction parameters, indicate strong affinity between iron and either phosphorus or boron. Self interaction parameter of phosphorus were as follows: 243±38 (1310 °C), 137±22 (1260 °C) and 18±2 (1210 °C), indicating the repulsion between phosphorus atoms. Self interaction parameter of boron were as follow: -96±12 (1310 °C), -111±28 (1260 °C) and -159±45 (1210 °C) implying an attraction between boron atoms in silicon. The distribution coefficient of phosphorus at infinite dilution were obtained as: 0.34±0.01 (1310 °C), 0.28±0.01 (1260 °C) and 0.24±0.00 (1210 °C). The same parameter for boron were: 0.49±0.01 (1310 °C), 0.41±0.03 (1260 °C) and 0.33±0.04 (1210 °C). Henrian activity coefficient of phosphorus and boron in solid silicon were also estimated.

Degree

thesis:*
Department dc:contributor.department
Materials Science and Engineering
Year dc:date.issued
2015

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Tafaghodikhajavi, Leili
Advisor dc:contributor.advisor
  • Barati, Mansoor

Subjects

dc:subject × 4

Identifiers

dc:identifier.*
Handle dc:identifier.uri
https://hdl.handle.net/1807/69509

Chain of custody

source
Harvested from
University of Toronto
Base URL
utoronto.scholaris.ca/server/oai/request
Last updated
2026-11-19
Source record
OAI-PMH GetRecord
citation

Tafaghodikhajavi, Leili. Thermodynamics of Impurity Removal in Solvent Refining of Silicon. 2015. https://hdl.handle.net/1807/69509