Back to search

University of British Columbia

Biomimetic synthesis of poly(propylene-fumarate)-calcium phosphate composites for tissue engineering

Abstract

dc:description

A novel in-situ co-precipitation process for the synthesis of poly(propylene-fumarate)-calcium phosphate composites was developed. In this process the calcium phosphate phase nucleates and grows in the presence of poly(propylene-fumarate) (PPF), in a novel two-solvent system including tetrahydrofuran (THF) and water. It was found that the presence of the organic solvent (THF) does not affect the phase evolution of the calcium phosphate. Both in the presence and absence of THF crystalline dicalcium phosphate dihydrate (DCPD, brushite) and poorly crystalline hydroxyapatite (HAp) form, and transform to crystalline HAp after 24 hours of synthesis time. Contrary to the organic solvent, PPF has a significant influence on the calcium phosphate phase that forms in its presence. It is found that PPF provides a template for the formation of the calcium phosphate phase through a coordination bond between the calcium ion and the carbonyl group of the polymer. As a result of this templating, hydroxyapatite can form in a significantly shorter period of time (~1 hr) compared to the system where PPF is not present (24 hrs). The nature of the calcium phosphate phase that forms in the presence of PPF depends on the molecular weight and concentration of PPF. High concentration of PPF in the composite (e.g. 80%) stabilizes an amorphous calcium phosphate (ACP) phase and hinders its transformation to crystalline apatite, while low concentration of PPF (e.g. 5%) promotes the formation of crystalline apatite. Higher molecular weight PPF (Mw = 4500) is found to be more efficient in stabilizing the amorphous phase compared to lower molecular weight PPF (Mw = 1800). While high molecular weight PPF stabilizes ACP, low molecular weight PPF promotes its conversion to crystalline apatite. TEM observations revealed that flake-like hydroxyapatite crystals form in the absence of PPF while spherical ACP particles form in a composite containing 80% PPF. The ACP nano-particles (50-100 nm in diameter) are homogeneously distributed within the PPF matrix. The PPF-calcium phosphate composite can crosslink into a 3D structure by UV irradiation.

Degree

thesis:*
Name thesis:degree_name
Doctor of Philosophy - PhD
Level thesis:degree_level
doctoral
Discipline thesis:degree_discipline
Materials Engineering
Grantor dc:publisher
University of British Columbia
Year dc:date
2006

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Hakimi Mehr, Dorna

Rights

dc:rights
Statement dc:rights
  • For non-commercial purposes only, such as research, private study and education. Additional conditions apply, see Terms of Use https://open.library.ubc.ca/terms_of_use.
Language dc:language
eng

Identifiers

dc:identifier.*
Handle dc:identifier
http://hdl.handle.net/2429/18259

Chain of custody

source
Harvested from
University of British Columbia
Base URL
circle.library.ubc.ca/oai/request
Last updated
2026-11-19
Source record
OAI-PMH GetRecord
related terms
citation

Hakimi Mehr, Dorna. Biomimetic synthesis of poly(propylene-fumarate)-calcium phosphate composites for tissue engineering. doctoral thesis, University of British Columbia, 2006. http://hdl.handle.net/2429/18259