Fatigue damage propagation in graphite/epoxy composites
Abstract
dc:descriptionA series of tests was performed to determine the increase in the crack length or fatigue damage of graphite/epoxy composites under tension-tension fatigue using traveling microscope, tetrabromoethane enhanced radiography and compliance techniques. Hercules As/3501-6 graphite fibre/epoxy prepreg was used to produce laminates which were subsequently cut into compact tension sample geometry. [90/0] ply configuration was used in the preparation of the laminates. Fatigue damage was observed to be in the form of a 'damage zone' rather than a single crack, which increased in size in both the 0° and 90° directions during fatigue. The damage followed three stages, during the whole fatigue life. The first stage was the acceleration; the intermediate stage was the deceleration and the final stage was the reacceleration of the damage. As a result of this behaviour the Paris approach was found to be non-valid for this material. Change in the compliance was observed during fatigue and this change revealed the same three stages as the development of the damage zone.
Degree
thesis:*- Name thesis:degree_name
- Master of Applied Science - MASc
- Level thesis:degree_level
- master's
- Discipline thesis:degree_discipline
- Materials Engineering
- Grantor dc:publisher
- University of British Columbia
- Year dc:date
- 1984
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Yavuz, Ömer
Rights
dc:rights- Statement dc:rights
-
- For non-commercial purposes only, such as research, private study and education. Additional conditions apply, see Terms of Use https://open.library.ubc.ca/terms_of_use.
- Language dc:language
- eng
Identifiers
dc:identifier.*- Handle dc:identifier
- http://hdl.handle.net/2429/24961