Back to search

University of British Columbia

Optimizing profile geometry to reduce the checking, shelling and cupping of profiled softwood deck-boards exposed to natural weathering

Abstract

dc:description

Wooden deck-boards are susceptible to surface checking and distortion during weathering. Surface profiling is an effective physical pre-treatment to reduce the checking of boards, but it is less effective at reducing cupping, unless it is also used on the underside of boards. I hypothesize that the checking and cupping of softwood deck-boards exposed outdoors can be significantly reduced by optimizing the geometries of surface and sub-surface profiles. To test this hypothesis, I examine the effect of profile geometry and growth ring orientation on the checking and cupping of western larch deck-boards exposed outdoors. Standard and tall rib profiles were significantly more effective at restricting checking than other profile types, particularly when profiled boards were oriented pith-side-up. However, such growth ring orientation made larch deck-boards more susceptible to shelling, a severe defect caused by the separation of growth rings. Confocal profilometry and macro-photography were used to characterize the projection of separated latewood at deck-board surfaces. A negative correlation was revealed between the heights of protruding latewood and growth ring angle to the weathered surface of flat larch boards oriented pith-side-up. The number of shelled lanceolate-shaped tips at the peaks of profiled boards was more common in boards with rib profiles particularly those oriented pith-side-up. I conclude that profiled larch boards should be oriented bark-side-up rather than pith-side-up. Hence, there was a need to develop different sub-surface profiles to distinguish pith- and bark-sides of boards so that boards can be correctly oriented in decks with their bark-side facing uppermost. Pacific silver fir and western hemlock boards were chosen to test sub-surface grooving as an alternative to sub-surface profiling because previous studies had optimized surface profiles for both species. There was an unexpected effect of number of grooves on the cupping of hem-fir boards. Boards machined with an odd number of grooves that included a groove running down the centre-line of the underside of boards were less prone to cupping compared to boards with an even number of grooves. In conclusion, results demonstrate that checking and cupping of softwood deck-boards can be reduced by a combination of surface profiling and sub-surface grooving.

Degree

thesis:*
Name thesis:degree_name
Master of Science - MSc
Level thesis:degree_level
master's
Discipline thesis:degree_discipline
Forestry
Grantor dc:publisher
University of British Columbia
Year dc:date
2020

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Leung, Lukie Hon

Rights

dc:rights
Statement dc:rights
  • Attribution-NonCommercial-NoDerivatives 4.0 International
Language dc:language
eng

Identifiers

dc:identifier.*
Handle dc:identifier
http://hdl.handle.net/2429/76899

Chain of custody

source
Harvested from
University of British Columbia
Base URL
circle.library.ubc.ca/oai/request
Last updated
2026-11-19
Source record
OAI-PMH GetRecord
related terms
citation

Leung, Lukie Hon. Optimizing profile geometry to reduce the checking, shelling and cupping of profiled softwood deck-boards exposed to natural weathering. master's thesis, University of British Columbia, 2020. http://hdl.handle.net/2429/76899