Fe(III)-Fe(II) redox kinetics and their effects on 2205 duplex stainless steel crevice corrosion

Abstract

dc:description

This study investigates the electrochemical behavior of the Fe(III)/Fe(II) redox couple and its effect on the crevice corrosion resistance of 2205 duplex stainless steel (DSS) under hydrometallurgical conditions. The research is divided into two parts: redox kinetics and critical crevice temperature (CCT) evaluation. The kinetics of the Fe(III)/Fe(II) redox couple were examined in 0.5 M sulfuric acid at 25, 60 and 95 °C across Fe(III)/Fe(II) ratios of 1:10, 1:1, and 1000:1. A novel method previously applied to sulfide minerals was adapted to isolate the mixed potential for the first time on 2205 DSS. The reversible potential (Erev) was maintained within the passive region of DSS to minimize corrosion interference. Both potentiodynamic polarization (PDP) and immersion tests were conducted, showing 2205 DSS remained passive between 0–1 V vs. SHE under all tested conditions. No significant weight loss (<0.1 mm/y) or pitting was observed after 60-days of immersion at 95 °C under varying Fe(III)/Fe(II) ratios. Potentiostatic tests revealed well-defined Tafel regions with R² > 0.95. While temperature had only a slight effect on Erev at a 1:1 ratio (rising from 0.65 V to 0.68 V), the Fe(III)/Fe(II) ratio showed a strong logarithmic influence: from 0.60 V at 1:10 to 0.86 V at 1000:1. Erev always remained in the passive region, helping protect against localized corrosion. CCT testing revealed a clear inverse correlation between the Fe(III)/Fe(II) ratio and the critical crevice temperature (CCT) in the presence of chloride ions. In the absence of Fe(III)/Fe(II), the CCT decreased from 98.7 °C at 1 g/L Cl⁻ to 39.9 °C at 15 g/L. The presence of Fe(III)/Fe(II) further reduced the CCT by 10–20 °C at a 1:10 ratio, and by an additional 5–10 °C at 1:1 and 1000:1 ratios. Under the most aggressive condition—15 g/L NaCl with a 1000:1 Fe(III)/Fe(II) ratio—crevice corrosion occurred at room temperature. Elevated Fe(III) promoted anodic dissolution and passive film breakdown in crevices. Microscopy confirmed localized corrosion beneath crevice formers. OM revealed distinct crevice regions, and SEM-BSE imaging showed corrosion along α/γ phase boundaries, with ferrite (α) undergoing preferential attack due to galvanic effects.

Degree

thesis:*
Name thesis:degree_name
Master of Applied Science - MASc
Level thesis:degree_level
master's
Discipline thesis:degree_discipline
Materials Engineering
Grantor dc:publisher
University of British Columbia
Year dc:date
2025

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Zong, Pengfei
Contributors dc:contributor
  • Asselin, Edouard

Rights

dc:rights
Statement dc:rights
  • Attribution-NonCommercial-NoDerivatives 4.0 International
Language dc:language
eng

Identifiers

dc:identifier.*
Handle dc:identifier
http://hdl.handle.net/2429/92498

Chain of custody

source
Harvested from
University of British Columbia
Base URL
circle.library.ubc.ca/oai/request
Last updated
2026-11-19
Source record
OAI-PMH GetRecord
related terms
citation

Zong, Pengfei. Fe(III)-Fe(II) redox kinetics and their effects on 2205 duplex stainless steel crevice corrosion. master's thesis, University of British Columbia, 2025. http://hdl.handle.net/2429/92498