Abstract

dc:description

This study is part of a research project whose goal is to develop a process model for the production of aluminum alloy automotive bumpers. The problem originates from the industrial bumper manufacturing practice which uses aluminum alloys, AA7030.60 and AA7108.72 in particular. In the industrial production schedule, a forming (pre-deformation) process occurs after the solution heat treatment and water quenching, followed by a T6 ageing process. Due to the specific shape of the bumper product, the forming process introduces a heterogeneous distribution of deformation in the bumper. A systematic investigation of pre-deformation on the ageing behaviour of these alloys has been carried out. A series of pre-deformations (pre-strain from 0 to 1.2) was imposed on the materials, whose subsequent ageing responses were recorded in terms of the mechanical properties (yield stress, tensile strength, etc.) and electrical resistivity. Some transmission electron microscopy measurements were also conducted by other members of the research group. With a combination of these results the evolution of the material's microstructure and mechanical properties can be traced during the ageing process. Some of the significant results from the present study include the observation that the natural ageing response is reduced and the artificial ageing kinetics are accelerated for the pre-deformed alloys. Lower peak ageing strength is also observed for the pre-deformed alloys. These changes in the material behaviour are related to the changes in the microstructure when pre-deformation is present in the materials. At a microscopic level, dislocations are observed to arrange themselves into a loose cell structure. Pre-deformed alloys were observed to have larger average precipitate sizes. In addition, they also have different precipitate size distribution. For pre-deformed samples two peaks can be recognized in the precipitate size distribution curves, corresponding to the precipitates in the bulk and the precipitates at dislocation sites. Based on this study, it has been observed that deformation prior to artificial ageing leads to inferior final properties. A modified bumper manufacturing sequence is proposed in an attempt to eliminate this effect. However, further studies are needed to test the feasibility of the proposal.

Degree

thesis:*
Name thesis:degree_name
Master of Applied Science - MASc
Level thesis:degree_level
master's
Discipline thesis:degree_discipline
Materials Engineering
Grantor dc:publisher
University of British Columbia
Year dc:date
1999

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Huang, Jin

Rights

dc:rights
Statement dc:rights
  • For non-commercial purposes only, such as research, private study and education. Additional conditions apply, see Terms of Use https://open.library.ubc.ca/terms_of_use.
Language dc:language
eng

Identifiers

dc:identifier.*
Handle dc:identifier
http://hdl.handle.net/2429/9396

Chain of custody

source
Harvested from
University of British Columbia
Base URL
circle.library.ubc.ca/oai/request
Last updated
2026-11-19
Source record
OAI-PMH GetRecord
related terms
citation

Huang, Jin. The effect of pre-deformation on the ageing behavior of 7030.60 and 7108.72 alloys. master's thesis, University of British Columbia, 1999. http://hdl.handle.net/2429/9396