UCL (University College London)
Spatiotemporal X-ray Techniques for the Quantification of Lithium-Ion Battery Degradation
Abstract
dc:description.abstractBattery technology is becoming increasingly crucial in achieving global targets for electrified transportation and the deployment of renewable energy, therefore, the demand for batteries with high energy density and extended lifespan is continuously growing. One promising solution is high nickel containing layered cathodes, with NMC811 (Li1[Ni1-x-yMnxCoy]O2, x=0.1 and y=0.1) presenting as the premier candidate for ubiquitous adoption of electric vehicles. This cathode chemistry has the potential to significantly enhance the energy density of next-generation lithium-ion batteries. Nevertheless, NMC811 faces a notable challenge; they can experience a substantial decrease in capacity during cycling, particularly when subjected to high-voltage and high-temperature conditions. Cracking in secondary particles has been suggested to cause reduced performance due to insufficient connection between particles and the conductive architecture in the electrode matrix, as well as fresh surface exposure to electrolyte and subsequent oxygen release accompanied by electrolyte oxidation. Establishing the nature of crack generation, formation, and propagation is paramount to understanding the degradation modes that govern decline in battery performance. Cracking has several possible origins; however, it can be classified in two general cases: mechanically induced, during manufacturing, or electrochemically induced, during operation. This thesis looks to design novel spatial resolved in situ techniques using X-ray imaging and diffraction that will help us understand the true nature of cracks development and suggest possible mitigation solutions to reduce cracking detrimental to the battery’s performance. Cracking is intrinsically linked to the crystal structures underpinning the whole battery’s operation and these layered crystals have complex volumetric expansion properties as a function of lithium content. Thus, NMC crystallographic expansion properties in both polycrystalline and single crystal morphologies are also presented here. Thought to have extended life cycle due to their resistance to cracking, the single crystal materials diffraction is measured in operando to further grasp the volumetric behaviour that may be at the heart of cracking phenomena
Degree
thesis:*- Level dc:type.qualificationlevel
- Doctoral
- Grantor dc:publisher.institution
- UCL (University College London)
- Year dc:date.issued
- 2024
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Parks, Huw CW
Rights
- Language dc:language
- en, eng
Identifiers
dc:identifier.*- Repository record dc:identifier.uri
- https://discovery.ucl.ac.uk/id/eprint/10200857/