Enhanced Toughness And Degradation Of Diblock Copolymer Modified Polylactide
Abstract
dc:description.abstractPoly(lactide) (PLA) is currently the most commercially successful bioderived synthetic polymer. However, applications of PLA are limited due to brittleness, which develops after about one day of physical aging at room temperature following melt processing. In this work, we first investigate the ability of low molecular weight poly(isoprene)-block-poly(ethylene oxide) (IO) diblock copolymers to toughen glassy PLA. Melt blending IO with PLA leads to submicron diameter macrophase-separated IO domains in the PLA matrix, stabilized by surfactant-like behavior associated with compatibility between the poly(ethylene oxide) (O) blocks and PLA. IO molecular weights that bracket the room temperature order-to-disorder transition temperature, Mn = 1.7–3.3 kg/mol, produce outstanding toughness with strains at break εb > 150%, which persists through 9 days of aging at room temperature. Higher molecular weight IO diblocks do not perform as well. We hypothesize that this behavior reflects two unique characteristics: (1) optimal particle sizes leading to cavitation and craze initiation when subjected to triaxial strain, and (2) draining of IO into the advancing crazes thereby stabilizing the porous craze structures. Experiments with melt mixed poly(isoprene) (I) homopolymer in PLA containing controlled particle sizes support this mechanism. Further experiments with poly(butadiene)-block-poly(ethylene oxide) (BO) and poly(ethylene oxide)-block-poly(butylene oxide) (PEO-PBO) lend general support to these conclusions. These results demonstrate a general strategy for designing block copolymer additives that toughen otherwise brittle plastics.In a second focus, we address restricted biodegradability of PLA, which generally requires industrial compost conditions due in part to an elevated glass transition temperature (Tg). We have previously demonstrated that addition of poly(ethylene oxide)-block-poly(butylene oxide) diblock copolymer (PEO-PBO) forms macrophase-separated rubbery domains in PLA that can impart significant toughness at 5 wt %. Now, we demonstrate that PEO-PBO/PLA blends exhibit substantial toughness for at least nine months - beyond the average lifetime of single-use packaging - even amidst oxidative degradation of PEO-PBO into polyether oligomers that are confined to macrophase-separated domains due to the glassy PLA matrix. Modest thermal annealing (~ 60 °C) enables a heat-triggered plasticization phenomenon, characterized by rapid solubilization of the degradation products into PLA, which lowers the blend Tg. Ultimately, heat-triggered plasticization allows for accelerated bulk PLA degradation in simulated seawater, which we attribute to enhanced chain mobility promoting water uptake and hydrolysis. These results demonstrate the potential of PEO-PBO as an “all-in-one” additive which toughens PLA during its useful lifetime then accelerates degradation in end-of-life.
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Larson, Matthew
Subjects
dc:subject × 4Rights
- Language dc:language.iso
- en
Identifiers
dc:identifier.*- Dc Identifier Citation
- Larson, Matthew. (2024). Enhanced Toughness And Degradation Of Diblock Copolymer Modified Polylactide. Retrieved from the University Digital Conservancy, https://hdl.handle.net/11299/279253.