Back to search

University of Nevada - Reno

Hydrogen Permeation and Crystallization Kinetics of Ni-based Amorphous Alloy Membranes

Abstract

dc:description.abstract

Amorphous Ni-based alloy membranes show great promise as inexpensive, hydrogen-selective membrane materials. One of the main barriers to the commercial uptake of these materials is their tendency to crystallize during long-term operation at elevated temperatures, a process which decreases strength, durability and permeability. In this study, a series of Ni<sub>100-x</sub>Zr<sub>x</sub> (where x = 36.3 or 70 at.%), (Ni<sub>0.6</sub>Nb<sub>0.4</sub>)<sub>100-x</sub>Zr<sub>x</sub> and (Ni<sub>0.6</sub>Nb<sub>0.3</sub>Ta<sub>0.1</sub>)<sub>100-x</sub>Zr<sub>x</sub> (where x = 0, 10, 20 or 30 at.%) amorphous alloy membranes were prepared by melt spinning. The glass transition and crystallization kinetics of the amorphous alloy membranes have been studied under non-isothermal and isothermal conditions using differential scanning calorimetry (DSC). The activation energies (E<sub>x</sub>) of crystallization were determined using Kissinger and Ozawa equations. A Johnson-Mehl-Avrami equation has also been applied for isothermal kinetics and corresponding time-temperature-transformation (TTT) diagrams are plotted. Intermetallic phases and surface morphology after the thermal treatment have been identified by X-ray diffraction (XRD) and scanning electron microscopy (SEM). The crystallization temperature, T<sub>x</sub>, for the eutectic Ni<sub>63.7</sub>Zr<sub>36.3</sub> and the near-eutectic Ni<sub>30</sub>Zr<sub>70</sub> alloys for a 10 K/min DSC heating rate were determined as 841.2 K and 668.9 K, respectively. The Arrhenius plot obtained for the Ni<sub>63.7</sub>Zr<sub>36.3</sub> alloy yielded E<sub>x</sub>=374.1 kJ/mol which is higher than the value for the Ni<sub>30</sub>Zr<sub>70</sub> alloy (E<sub>x</sub>=353.3 kJ/mol). The activation energy of the ternary Ni<sub>60</sub>Nb<sub>20</sub>Zr<sub>20</sub> alloy using Kissinger and Ozawa equations (517 kJ/mol and 505 kJ/mol) are higher than those of the binary Ni-Zr alloys (374.1 kJ/mol and 353.3 kJ/mol), and also the crystallization temperature (871.6 K) of the Ni<sub>60</sub>Nb<sub>20</sub>Zr<sub>20</sub> alloy is higher than those of binary Ni-Zr alloys at the heating rate of 10 K/min. In (Ni<sub>0.6</sub>Nb<sub>0.4</sub>)<sub>100-x</sub>Zr<sub>x</sub> (where x = 0, 10, 20 or 30 at.%) alloys, T<sub>x</sub> continuously decreased with increasing Zr concentration. The value of E<sub>x</sub> increased up to 10 at.% Zr addition, then decreased, which is consistent with the decrease in T<sub>x</sub>. In addition, the values of T<sub>x</sub> and E<sub>x</sub> increased with increasing Ta content in the (Ni<sub>0.6</sub>Nb<sub>0.3</sub>Ta<sub>0.1</sub>)<sub>100-x</sub>Zr<sub>x</sub> alloys.Hydrogen permeation properties of Ni-based amorphous alloy membranes were investigated over the 573-673 K temperature range at different hydrogen partial pressures. The linear relationship between the hydrogen permeation flux and the hydrogen partial pressure difference across the membrane indicates that permeation was controlled by diffusion through the bulk membrane. The effect of Zr concentration on the hydrogen permeability, the thermal stability and hydrogen embrittlement was also investigated. The hydrogen permeability of the (Ni<sub>0.6</sub>Nb<sub>0.4</sub>)<sub>70</sub>Zr<sub>30 </sub>alloy was higher (7.0 x 10<super>-9</super> mol m<super>-1</super> s<super>-1</super> Pa<super>-0.5</super>) than those of the (Ni<sub>0.6</sub>Nb<sub>0.4</sub>)<sub>90</sub>Zr<sub>10</sub> and Ni<sub>60</sub>Nb<sub>40</sub> alloys at 623 K (1.2 x 10<super>-9</super> and 4.9 x 10<super>-11</super>, respectively), but decreased with decreasing Zr concentration. The permeability of the alloy with Ta, (Ni<sub>0.6</sub>Nb<sub>0.3</sub>Ta<sub>0.1</sub>)<sub>70</sub>Zr<sub>30</sub> at 623 K was slightly lower (3.9 x 10<super>-9</super> mol m<super>-1</super> s<super>-1</super> Pa<super>-0.5</super>) than (Ni<sub>0.6</sub>Nb<sub>0.4</sub>)<sub>70</sub>Zr<sub>30</sub> alloy, but resulted in improved thermal stability and hydrogen embrittlement.

Degree

thesis:*
Level thesis:degree_level
Doctorate Degree
Department thesis:degree_department
Chemical and Materials Engineering
Year dc:date.issued
2011

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Kim, Sang-Mun
Advisor dc:contributor.advisor
  • Chandra, Dhanesh
Committee members dc:contributor.committeemember
  • Li, Qizhen
  • Raja, Krishnan Selva
  • Chien, Wen-Ming
  • Daemen, Jaak J.K.

Subjects

dc:subject × 4

Rights

dc:rights
Statement dc:rights
  • In Copyright(All Rights Reserved)
  • Author(s)

Identifiers

dc:identifier.*
Handle dc:identifier.uri
http://hdl.handle.net/11714/3926

Chain of custody

source
Harvested from
University of Nevada - Reno
Base URL
scholarwolf.unr.edu/server/oai/request
Last updated
2026-11-19
Source record
OAI-PMH GetRecord
citation

Kim, Sang-Mun. Hydrogen Permeation and Crystallization Kinetics of Ni-based Amorphous Alloy Membranes. Doctorate Degree thesis, 2011. http://hdl.handle.net/11714/3926