Back to search

University of South Florida

Failure Analysis of High Nickel Alloy Steel Seal Ring Used in Turbomachinery

Abstract

dc:description

The system of upper high nickel alloying steel seal ring and lower high nickel alloying steel seal ring, installed in the grooves of turbine, can extend out and fit with the wall of valve cage, resulting in forming a good seal under the pressure. In the project, the failure steel seal ring is considered. This situation had threatened the safety of the whole steam turbine system. The purpose of this study is to identify the failure cause of the steel seal ring used in nuclear steam turbines. New high nickel steel alloy seal ring was compared with the failed seal ring. The dimensions of macroscopic ring with clearly plastic deformation were measured using calipers. Surface morphology of ring was observed by optical microscopy through metallographic analysis. There is a lot of precipitation in the grain boundaries of used seal ring, along with smaller grain size than the new seal ring. To explore the composition of precipitation, scanning electron microscopy (SEM) with energy-dispersive spectrometer (EDS) were used. The results indicated that the concentration of titanium (Ti) and molybdenum (Mo) was higher in the precipitation of used seal ring. At the same time, the hardness and elastic modulus of used seal ring were reduced, measured by nanoindentation test. In-situ SEM tensile testing were used to record and analyze the generation of crack source and crack development under applied load. The reasons of the seal ring failure can be answered because of these experimental results at both macroscopic and microscopic scales. The main reason of the seal ring failure is a combination of long-term stress and elevated temperature during turbine operation. Complex work environment caused recrystallization and recovery, resulting in grain refinement and secondary phase precipitation. Further embodiment, recrystallization and recovery caused the elastic modulus and hardness of used seal ring decrease. Moreover, a lot of secondary phase precipitates appeared at grain boundaries during use. The appearance of secondary phase precipitates become the weakest part of used seal ring. The applied load lead to seal ring failure from the formation of microvoids to microvoids aggregated becoming microcracks until to the appearance of cracks at macroscopic scale. These changes of microscopic structure ultimately reflected in critical plastic deformation of used seal ring.

Degree

thesis:*
Name thesis:degree_name
Master of Science (M.S.)
Level thesis:degree_level
Thesis
Discipline thesis:degree_discipline
Engineering
Grantor
University of South Florida
Year dc:date
2017

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Wang, Wenbo
Contributors dc:contributor
  • Alex Volinsky, Ph.D.
  • Wenjun Cai, Ph.D.
  • Venkat R. Bhethanabotla, Ph.D.

Subjects

dc:subject × 6

Identifiers

dc:identifier.*
Repository record dc:identifier
https://digitalcommons.usf.edu/etd/6635

Chain of custody

source
Harvested from
University of South Florida
Base URL
digitalcommons.usf.edu/do/oai/
Last updated
2026-11-19
Source record
OAI-PMH GetRecord
citation

Wang, Wenbo. Failure Analysis of High Nickel Alloy Steel Seal Ring Used in Turbomachinery. Thesis thesis, University of South Florida, 2017. https://digitalcommons.usf.edu/etd/6635