Institutional Repository of Vilnius University
Stiklo tūrinis modifikavimas pikosekundinio lazerio impulsais ilgos nedifraguojančios zonos pluoštu /
Abstract
dc:descriptionNowadays the technology industry is looking for efficient ways to process dielectrics using a variety of glass processing methods. The work presents the intra-volume modification and glass cutting experiments of asymmetrical Bessel beam formed in a conical prism (axicon). Goal of the work: to study asymmetric methods of Bessel beam formation and their application for glass modification/cutting. Different beam filtering methods are compared: symmetrical beam, modulation of phase and amplitude masks, and tilting the axicon with respect to the optical axis. The experimental scheme consists of Atlantic laser with a pulse duration of 13 ps, an output pulse energy of 240 μJ, repetition rate of 200 kHz, and a wavelength of 1064 nm. The optical scheme also consists of a telescope (+150 mm and +100 mm), 4F system: +75 mm and +10 mm and relay lens was used to filter the Bessel beam in the Fourier plane (two +100 mm lenses). The angle of the axicon base is 10° and Bessel zone from the tip equals to 30 mm. Bessel-Gaussian beam characterization was measured after the 4F system. A CMOS camera with an 8.75 cm tube and an 8 mm lens was used for the beam characterization experiment. Without the filter and aperture, the experimental value of Zmax is 1.53 mm (width calculated at 0.32 Imax height). With the filter and aperture, the Zmax decreases to 0.89 mm and the non-diffractive zone does not change with continued use of the phase and amplitude masks. Modulation masks generated the transverse intensity with a central maximum and lateral maxima. Glass volume experiments showed that the maximum length of the modification was 1.5 mm with the symmetrical beam using 140 μJ impulse energy. Glass dicing experiments showed that the minimum bending strength is 15.7 MPa obtained with a 15° amplitude mask at a pitch of 8 μm. Tilting the axicon at an angle gives the lowest flexural strength region at 6-10 μm due to the crack length equaling to 18.8 μm. After separating the glass samples, the roughness of the surface was assessed and compared to literature. The minimum surface roughness was Ra = 0.095 μm and it was obtained with tilting the axicon 5°. Whereas symmetrical beam surface roughness equaled to 0.159 μm.
Degree
thesis:*- Grantor dc:publisher
- Institutional Repository of Vilnius University
- Year dc:date
- 2021
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Pipiras, Jokūbas,
- Contributors dc:contributor
-
- Dudutis, Juozas
Rights
dc:rights- Statement dc:rights
-
- info:eu-repo/semantics/openAccess
- Language dc:language
- lit
Identifiers
dc:identifier.*- Repository record dc:identifier
- https://repository.vu.lt/VU:ELABAETD107204597&prefLang=en_US