Abstract
dc:descriptionSilicon, a semiconductor that is used in a lot of devices, has a unique property, where if it interacts with a femtosecond laser pulse, a bright silicon specific ring is seen. This ring for decades was used to measure the laser beam diameter by considering, that the fluence needed to create these modifications is constant. In order to use this measurement correctly, it is important to know exactly what in what conditions could this specific modification appear. In this work, the aim was to determine how exactly the sample composition and laser parameters could affect the fluence thresholds needed to create the amorphization and re-crystallization areas that make up the ring. This was done by using six different samples (having different dopants and dopant concentrations) and affecting them with a femtosecond 1030 nm Yb:KGW laser to create matrices of amorphized/re-crystallized rings with a wide range of laser power and spot diameters. From the measurements, LIDT curves were created, and the calculated thresholds were compared. For a silicon wafer, the thresholds calculated were Φmod = 0.19 J/cm2 for amorphization and Φann = 0.26 J/cm2 for re-crystallization. The received results slightly differ from the values found in literature because of the different source’s parameters used. It was concluded, that indeed, that fluence threshold needed for these modifications is only dependent on the sample itself, where the threshold fluence varies slightly, if the material has increased amount of defects and the threshold increases significantly if the used sample is extremely pure. It was shown, that laser spot size does not notably affect the threshold, with two exceptions, increasing the spot’s size could lead to a higher probability of hitting a defect, and decreasing the threshold and tightly focusing laser light can increase the threshold. Furthermore, it was also observed, that the difference in fluence could mean, that there are different processes present in the appearance of the modification. All of this shows, that indeed, the amorphization ring could be used as a sort of a silicon sample fingerprint, representing its composition and purity for a set of source conditions.
Degree
thesis:*- Grantor dc:publisher
- Institutional Repository of Vilnius University
- Year dc:date
- 2021
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Šližiūtė, Gabija,
- Contributors dc:contributor
-
- Paipulas, Domas
Subjects
dc:subject × 1Rights
dc:rights- Statement dc:rights
-
- info:eu-repo/semantics/openAccess
- Language dc:language
- eng
Identifiers
dc:identifier.*- Repository record dc:identifier
- https://repository.vu.lt/VU:ELABAETD107205530&prefLang=en_US