Skulptūrinių anizotropinių sluoksnių struktūros tyrimas ir taikymas fazinių plokštelių formavimui /
Abstract
dc:descriptionIntegrated laser systems are the foundation of modern optical equipment. As modern laser and optical systems technologies advance, optical elements are becoming the limiting factor for progressively more complex high-power systems. For more than 30 years, the Glancing Angle Deposition technique (GLAD) has been under continual development, introducing morphology control of a thin-film. GLAD employs self-shadowing phenomena to generate nanoscaled coatings with various vertical chiral, columnar, and other porous thin-film architectures. By altering the orientation of the substrate in regard to the vapor flux, morphological changes, porosity, and birefringence of the films can be adjusted. However, to form optically transparent waveplates that are resistant to laser-induced damage with exact retardance, reliable birefringence measurements of anisotropic layers and the incorporation of dense layers are necessary. An electron beam evaporation technique was used to form anisotropic SiO2 layers at different deposition angles of 66°, 68°, 70°, 72°, 74°, 76°, 80° and 84°. After investigation it was observed, that layers evaporated at 74° have the highest retardation of Δ = 0.042°/nm for 355 nm wavelength. Also, different multilayer coatings were formed to determine the optimal deposition angle of dense layers. The results suggest that coatings with dense interlayers deposited at an angle of 30° show 5.88% higher retardation values for the 355 nm wavelength compared to the structure when the dense layers are formed at an angle of 0°. Finally, λ/4 waveplate for 355 nm wavelength was designed and fabricated with optical transmittance values reaching T > 95% for both polarizations (reflection from the back surface ~4%) and retardance corresponding to Δ = 87.4°. Compared to other commercially available components, the produced element was characterized by low mechanical stresses 𝜎 = 11.2 MPa and high laser-induced damage threshold LIDT = 54.5 J/cm2 (at 355 nm wavelength, 2 ns). However, further developments are still needed in order to improve the repeatability of the deposition process.
Degree
thesis:*- Grantor dc:publisher
- Institutional Repository of Vilnius University
- Year dc:date
- 2023
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Slipkauskas, Mantas,
Rights
dc:rights- Statement dc:rights
-
- info:eu-repo/semantics/openAccess
- Language dc:language
- lit
Identifiers
dc:identifier.*- Repository record dc:identifier
- https://repository.vu.lt/VU:ELABAETD158213085&prefLang=en_US