Back to search

Institutional Repository of Vilnius University

Kietųjų tirpalų xBZN(1-x)BT plačiajuostės dielektrinės spektroskopijos tyrimai /

Abstract

dc:description

Relaxor ferroelectrics can be used in diverse applications, for example, energy storage and conversion. This makes the investigation of various ferroelectrics an important objective. Relaxor additives are added to ferroelectric solid solutions to alter their characteristics. However, commonly used lead zirconate titanate is allowed to be utilized only in limited applications due to health concerns raised by the European Parliament and the Council on RoHS. Because of these legislative enforcements, demand for lead-free analogues has appeared and they were heavily studied in the previous decade. One of these materials, bismuth zinc niobate – barium titanate, x(Bi(Zn2/3Nb1/3)O3)-(1-x)BaTiO3 (BZNBTx % in short) has received interest as a high-capacity relaxor dielectric material. These ceramics have different composition regimes depending on concentration x. In the present work, the dielectric properties of four different concentrations x are analyzed: 1 %, 2 %, 3 % and 3.4 %. Ceramics were analyzed in the 20 Hz – 30 GHz frequency range and in the 125 K – 500 K temperature range. For measuring in the 20 Hz – 1 MHz frequency range HP LCR meter 4284A was used. Whereas for the 2.8 MHz – 1 GHz band, a coaxial line shorted with a capacitor was used and for measurement of complex reflection coefficient Agilent RF network analyzer 8714ET was utilized. Dielectric rods were made from samples and were put in the waveguide, then reflection and transmission coefficients were measured in the 26 GHz – 39 GHz frequency range using scalar network analyzer Elmika R2400. The measurements of dielectric permittivity were performed during the cooling cycle at lower than 1 K/min temperature decline rate. Piezoelectric measurements were performed using Aixacct TF analyzer 2000. From the result examination, we can conclude that 1 % BZN – 99 % BT has similar dielectric constant and piezoelectric characteristics to the classical barium titanate ceramics. The pattern was noticed that increasing bismuth zinc niobate concentration x decreases the temperature at which real part of dielectric permittivity 𝜀′ peaks. This corresponds to the results of other researches. It was also observed that the dielectric anomaly decreases more gradually with increasing BZN concentrations. According to frequency dependencies of complex dielectric constant, it was found that relaxations occur in the 10 MHz – 30 GHz frequency band. Judging from acquired low activation energy Ea ~ 0,11 eV relaxations are probably related to domain wall movement. At last, it was recorded that an increase of additive concentration x leads to polarization and displacement hysteresis broadening, remanent and spontaneous polarization enlargement.

Degree

thesis:*
Grantor dc:publisher
Institutional Repository of Vilnius University
Year dc:date
2023

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Šatkauskas, Eidvidas,

Rights

dc:rights
Statement dc:rights
  • info:eu-repo/semantics/openAccess
Language dc:language
lit

Identifiers

dc:identifier.*

Chain of custody

source
Harvested from
Vilnius University
Base URL
epublications.vu.lt/oai
Last updated
2026-11-19
Source record
OAI-PMH GetRecord
related terms
citation

Šatkauskas, Eidvidas,. Kietųjų tirpalų xBZN(1-x)BT plačiajuostės dielektrinės spektroskopijos tyrimai /. Institutional Repository of Vilnius University, 2023. https://repository.vu.lt/VU:ELABAETD192834285&prefLang=en_US