SrAl4O7:Eu2+ kietafazė sintezė ir liuminescencinių savybių tyrimas /

Abstract

dc:description

Solid state synthesis and luminescent properties of SrAl4O7:Eu2+ In recent times the amount of research done on luminescent oxide materials has grown exponentially due to their potential application in various fields, such as luminescent paint, plasma displays, LED technology, safety markings and watches that glow in the dark, medical diagnostics. Among those materials, strontium aluminates doped with various rare-earth ions have piqued the interest of many scientists recently due to their thermal and chemical stability, excellent quantum efficiency and great potential in the field of long-lasting emission materials. This research covers the synthesis and luminescent properties of SrAl4O7:Eu2+. This luminescent material was made using the solid-state synthesis method. It is noticable that until very recently the general consensus was that pure SrAl4O7 could not be successfully synthesized using this method. By using an appropriate ratio of reagents, heating program and temperature, a flux, and most importantly grinding the mixed initial materials really thoroughly for an extended period of time a pure SrAl4O7 phase was achieved. During the following syntheses different amounts of europium (III) oxide were introduced into the reaction mixtures, which were heated in a reductive atmosphere, in order to dope the strontium dialuminate with various concentrations of Eu2+ ions. The resulting series of samples had their luminescent properties examined with a spectrometer. The absorbtion and emission spectra displayed similar tendencies – the intensity of both absorption and emission peaks increased with the increase of Eu2+ amounts in the samples, the peaks themselves moved towards longer wavelenghts with increasing concentrations of europium as well (476-488nm interval for emission and 353-370nm for absorbtion), most likely due to the overlap of the absorbtion and emission spectra. SrAl4O7:Eu2+ displayed some afterglow, but it decreased in intesity rather quickly (the emission intensity was halved in 0.2-3.4s depending on the amount of europium in the sample), so further experiments, where SrAl4O7 would be co doped with Eu2+ and Dy3+ in order to increase the length of afterglow are required.

Degree

thesis:*
Grantor dc:publisher
Institutional Repository of Vilnius University
Year dc:date
2020

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Lašinskas, Lukas,

Rights

dc:rights
Statement dc:rights
  • info:eu-repo/semantics/openAccess
Language dc:language
lit

Identifiers

dc:identifier.*

Chain of custody

source
Harvested from
Vilnius University
Base URL
epublications.vu.lt/oai
Last updated
2026-11-19
Source record
OAI-PMH GetRecord
related terms
citation

Lašinskas, Lukas,. SrAl4O7:Eu2+ kietafazė sintezė ir liuminescencinių savybių tyrimas /. Institutional Repository of Vilnius University, 2020. https://repository.vu.lt/VU:ELABAETD193301793&prefLang=en_US