Skvaleno ir kitų reaktyviųjų plastiklių terminė migracija iš poliizopreno /
Abstract
dc:descriptionThe main aim of the bachelor’s thesis is to analyze and evaluate the resistance of plasticisers to degradation and migration from polyisoprene. Thermal migration of plasticisers depends on the rate of oxidation and acidity. The results showed that evaporation rate of plasticisers while polyisoprene membrane was exposed to heat were dependent on temperature, duration and type of metal. This study is based on thin film degradation experiments on a metal surface. The analyzed plasticizers were heated at 90 °C, 120 °C and 140 °C temperatures. Before and after each heating test, the plasticisers were weighed to calculate their weight loss, and their pH was measured to evaluate changes in acidity. The study allowed to determine that an increase in temperature and heating time forced processes of oxidation, destruction, weight loss and acidification. High molecular weight plasticisers have higher resistance to migration, their oxidation processes are slower, and their heating time before oxidation is longer. Oxidative processes of plasticisers on aluminum surfaces progress slower.
Degree
thesis:*- Grantor dc:publisher
- Institutional Repository of Vilnius University
- Year dc:date
- 2020
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Dadurkaitė, Gabrielė,
Rights
dc:rights- Statement dc:rights
-
- info:eu-repo/semantics/openAccess
- Language dc:language
- lit
Identifiers
dc:identifier.*- Repository record dc:identifier
- https://repository.vu.lt/VU:ELABAETD193302055&prefLang=en_US