Institutional Repository of Vilnius University
Dielectric dispersion of composites based on potassium sodium niobate and m-type and z-type hexaferrites /
Abstract
dc:descriptionSimas Jurelevičius Dielectric dispersion of composites based on potassium sodium niobate and M - type and Z - type hexaferrites. In this work, a dielectric spectroscopic analysis of composite multiferroic ceramics composed of M - and Z - type hexaferrites and 20% potassium–sodium niobate (KNN) was performed. The samples under investigation were BaZ80KNN20, BaM80KNN20, and SrM80KNN20 composites. The main goal of the work was to investigate the dielectric and electrical properties of these materials and their dependences on frequency and temperature. Dielectric spectroscopy measurements were carried out over a wide frequency (from 20 Hz to 1 GHz) and temperature (from room temperature up to 600 K) ranges, using the “HP Precision LCR Meter” and the “Agilent RF Network Analyzer” as our main measurement instruments. From the complex impedance data, the values of complex dielectric permittivity, dielectric losses, electric modulus, and electrical conductivity were calculated. In addition, the DC conductivity was determined, which was then used to calculate the activation energies. The results showed that all composites exhibit pronounced dielectric dispersion at low frequencies, which is associated with Maxwell–Wagner interfacial polarization. This manifests as an increase in dielectric permittivity at low frequencies with increasing temperature. BaZ80KNN20 and BaM80KNN20 composites exhibited better charge carrier reversibility compared to the SrM80KNN20 composite. Relaxation processes were analysed using the Cole–Cole approximation, with which the mean relaxation times were defined and their temperature dependence. It was found that within the investigated frequency and temperature range, only interfacial relaxation processes are fully observable, and that complete dipolar relaxation processes are visible only in BaZ80KNN20 and SrM80KNN20 composites up to a temperature of 400 K. Further investigations were focused on the analysis of interfacial relaxation processes. The dependence of conductivity on frequency with increasing temperature was investigated. It was observed that with increasing frequency, the conductivity values increase exponentially. With increasing temperature, this exponential increase weakens, as the plateau region of the curve extends. The plateau region corresponds to DC conductivity, while the exponential increase corresponds to AC conductivity. Using Jonscher’s power law, AC conductivity values were determined for each material during both heating and cooling. Using Arrhenius analysis, the logarithm of DC conductivity was plotted as a function of inverse temperature, and by fitting a linear fit, activation energies were obtained for heating and cooling cycles. The obtained values are: SrM80KNN20: heating cycle – 0.61 ± 0.04 eV, cooling cycle – 0.38 ± 0.01 eV; BaZ80KNN20: heating cycle – 0.63 ± 0.02 eV, cooling cycle – 0.59 ± 0.01 eV; BaM80KNN20: heating cycle – 0.31 ± 0.008 eV, cooling cycle – 0.31 ± 0.007 eV.
Degree
thesis:*- Grantor dc:publisher
- Institutional Repository of Vilnius University
- Year dc:date
- 2026
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Jurelevičius, Simas,
Subjects
dc:subject × 1Rights
dc:rights- Statement dc:rights
-
- info:eu-repo/semantics/openAccess
- Language dc:language
- eng
Identifiers
dc:identifier.*- Repository record dc:identifier
- https://repository.vu.lt/VU:ELABAETD277691718&prefLang=en_US