Institutional Repository of Vilnius University
Formation of gan ridge waveguides for optical second harmonic generation /
Abstract
dc:descriptionThe fabrication of GaN ridge waveguides was investigated using photolithography and ICP-RIE, with a target ridge width of 20 µm, spacing of 30 µm, and final etch depth of 1910 nm. The work showed that the main technological difficulty is the stability of the whole pattern transfer chain: lithographic profile, mask formation, lift-off quality, mask durability, and sidewall preservation during a long chlorine based plasma etch. Four masking routes were compared: AZ3027 photoresist only, photoresist + SiO₂ hard mask, AZ3027 + Ni metal mask, and Ti 35ESX + Ni metal mask. The photoresist only route was limited by mask degradation, the SiO₂ hard mask route improved ridge definition but introduced residual mask material and was limited by etch depth, and the AZ3027 + Ni route confirmed the usefulness of a metal mask but suffered from lift-off and edge deformation problems. The Ti 35ESX + Ni route was therefore selected as the final process because it provides the most usable Ni mask formation route and enables full depth etching. However, SEM inspection showed that the intended Ti 35ESX undercut was not successfully formed, which likely contributed to Ni mask edge deformation. With this process, the full measured GaN layer thickness was etched, and SEM/EDX characterisation confirmed that GaN was removed from the trench regions down to the sapphire interface. The final structures therefore demonstrate a working fabrication route for GaN ridge waveguides with the selected 20 µm geometry. Optical characterisation also confirmed nonlinear optical response from the fabricated waveguides and reference planar waveguide. Under pumping at 1064 nm, the measured spectra showed an SHG peak near 532 nm. The SHG signal was measured as a function of pump wavelength, incidence angle, pump power, and λ/2 plate angle. At 41° incidence, 110 µW pump power produced 1.8 nW of measured SHG power, corresponding to an external conversion efficiency of about 0.0017%. The final process still requires improvement. Firstly the fabricated ridges showed unwanted top-surface porosity, which are attributed to local Ni mask degradation and mask-edge deformation during the long etching process. Secondly sidewall roughness was observed, which can be related to failed undercut formation and resulting metal mask edge roughness. The next process improvements should therefore focus on increasing Ni mask thickness, improving Ti 35ESX undercut formation and metal edge quality after lift-off. Overall, the thesis established a functional fabrication route and initial SHG measurement baseline, while also identifying the mask-related limitations that must be solved before moving toward smaller and lower-loss GaN ridge waveguides.
Degree
thesis:*- Grantor dc:publisher
- Institutional Repository of Vilnius University
- Year dc:date
- 2026
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Dailidėnas, Ignas,
Subjects
dc:subject × 1Rights
dc:rights- Statement dc:rights
-
- info:eu-repo/semantics/openAccess
- Language dc:language
- eng
Identifiers
dc:identifier.*- Repository record dc:identifier
- https://repository.vu.lt/VU:ELABAETD308116755&prefLang=en_US