Stilbeno mišinių su polimerais morfologijos ir elektrinių savybių tyrimai /

Abstract

dc:description

In today's world, organic semiconductors have attracted considerable scientific interest due to their mechanical flexibility, relatively simple synthesis, and the ability to tune electronic properties through molecular structure modification. These materials are used in organic light-emitting diodes (OLEDs), organic solar cells, and field-effect transistors. However, one of the main challenges in this field is understanding the relationship between material morphology and electrical properties. High quality crystalline structures provide more efficient charge transport, because molecules are positioned closer together and electron orbital overlap is better. This work investigates trans-stilbene — a molecule with a strong tendency to crystallize — blended with the polymer matrix PEPC (poly-N-epoxypropylcarbazole), which has active hole-transport properties via its carbazole groups. Using drop casting and spin coating techniques twenty-three trans-stilbene/PEPC composite samples were prepared on glass substrates with aluminium electrodes. Chlorobenzene (CB, Tv = 132 °C) and dichlorobenzene (DCB, Tv = 180 °C), which have different evaporation rates, were selected as solvents, thereby providing different conditions for crystallite formation. Various combinations of trans-stilbene to PEPC ratios (1:1, 1:2, 2:1, 3:1), concentrations (100–150 mg/ml), and spin speeds (600–900 rpm) were investigated. Sample morphology was characterised by polarised light microscopy in both parallel and crossed polariser configurations, layer thickness was determined by ellipsometry and the CELIV method, and photogenerated charge carrier mobility was measured by photo-CELIV using a 340 nm laser pulse. Spin coating was used as the main sample preparation method, due to significant layer non-uniformity produced by drop casting. Optical microscopy revealed that DCB-based samples formed more defined crystalline regions than CB-based samples, because slower evaporation rates of DCB allow more time for crystallites to grow. No crystallites were observed in CB samples even at 600 rpm. In DCB samples, the most active crystallisation was found at 800 rpm and crystallites were becoming smaller at lower speeds. Ellipsometry reliably determined the thickness of two samples: No. 5 (DCB, S:P = 1:2) at 0.18 &#956;m and No. 8 (CB, S:P = 1:2) at 0.39 &#956;m (MSE < 13). The most reliable DCB sample thicknesses were determined using the CELIV method: 0.111–0.140 &#956;m. Photo-CELIV measurements yielded photogenerated carrier mobilities of &#956; &#8776; 10&#8315;&#8312;–10&#8315;&#8311; cm²/(V·s) for DCB samples and slightly higher values of &#956; &#8776; 10&#8315;&#8311; cm²/(V·s) for CB samples. Additionally, varying the spin speed from 600 to 800 rpm in DCB and CB samples had no significant effect on carrier mobility, meaning that the morphological changes observed by optical microscopy in this speed range are not seen in the charge transport properties. Recombination parameters could not be determined due to a weak photoresponse.

Degree

thesis:*
Grantor dc:publisher
Institutional Repository of Vilnius University
Year dc:date
2026

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Žalalis, Matas,

Rights

dc:rights
Statement dc:rights
  • info:eu-repo/semantics/openAccess
Language dc:language
lit

Identifiers

dc:identifier.*

Chain of custody

source
Harvested from
Vilnius University
Base URL
epublications.vu.lt/oai
Last updated
2026-11-19
Source record
OAI-PMH GetRecord
related terms
citation

Žalalis, Matas,. Stilbeno mišinių su polimerais morfologijos ir elektrinių savybių tyrimai /. Institutional Repository of Vilnius University, 2026. https://repository.vu.lt/VU:ELABAETD308117433&prefLang=en_US