Institutional Repository of Vilnius University
Optinių padėklų paviršiaus šiurkštumo kontrolės ir jo įtakos aukšto atspindžio dangų optiniams nuostoliams tyrimas /
Abstract
dc:descriptionNew ultrashort pulse laser systems require high quality optical components with minimal optical losses. High finesse mirrors, typically manufactured using Ion Beam Sputtering (IBS), are essential for laser beam steering. However, the final performance of such mirrors depends not only on the theoretical coating design but also heavily on the initial substrate topography. The aim of this work is to investigate the influence of initial substrate preparation on the optical properties of high reflection dielectric coatings. Fused silica substrates with varying values of surface roughness were prepared using different polishing processes. Superpolishing was done using different concentrations of CeO2 polishing slurry to achieve sub-angstrom roughness. Highly reflective Ta2O5/SiO2 dielectric coatings, optimized for the 1064 nm wavelength, were deposited using IBS technology. Multi-scale analysis methods were applied to accurately measure and compare surface topography effects on coating characteristics. Data from the Atomic Force Microscope (AFM), White Light Interferometer (WLI), and Low Coherence Interferometer (LCI) were combined to construct a Master Power Spectral Density (PSD) function. Furthermore, total optical losses and final reflectivity were evaluated using Cavity Ring-down(CRD)method. Thermal effects and stability of the coatings were tested after annealing at 350 °C. The study yielded several key conclusions, all highlighting the fundamental role of the initial surface. First, the optimization of the superpolishing process revealed that the highest quality initial surface is achieved using a 0.05 % CeO2 slurry. Second, evaluating the thermal stability of the coatings it was demonstrated that central wavelength change (from 1060,6 nm to 1065,3 nm) was predicted correctly by the layer modeling program. Third, the multi-scale Master PSD analysis applied before coating deposition revealed that combining LCI, WLI, and AFM data enables full characterization of the initial substrate across the entire spatial frequency spectrum, proving that the superpolishing process effectively minimizes defect amplitudes only at high spatial frequencies while leaving significant macroscopic waviness in the low-frequency range. Finally, CRD measurements empirically confirmed that total optical losses are exclusively infuenced by the initial surface quality across the entire spatial frequency spectrum. The super-polished substrate ensured minimal scattering, achieving a maximum reflectivity of 99.993 % with only 68,4 ppm total losses, whereas the poor roughness substrate more than doubled the optical losses (148.4 ppm).
Degree
thesis:*- Grantor dc:publisher
- Institutional Repository of Vilnius University
- Year dc:date
- 2026
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Šidlauskas, Kipras,
Rights
dc:rights- Statement dc:rights
-
- info:eu-repo/semantics/openAccess
- Language dc:language
- lit
Identifiers
dc:identifier.*- Repository record dc:identifier
- https://repository.vu.lt/VU:ELABAETD308118602&prefLang=en_US