Fosforu ir grafitiniu anglies nitridu modifikuoto redukuoto grafeno oksido sintezė ir tyrimas /
Abstract
dc:descriptionGraphene-based materials exhibit unique physical, chemical, and electrical properties that make them attractive for energy storage, photocatalysis, and electrochemical sensing applications. However, the synthesis of monolayer graphene requires complex and costly equipment, leading to the wider practical use of reduced graphene oxide (rGO), whose preparation is simpler and more affordable. Furthermore, the oxygen-containing functional groups remaining on the rGO surface create reactive sites that allow targeted modification. Among the most effective approaches for tuning rGO properties are heteroatom doping (e.g. with phosphorus, P-rGO) and composite formation with graphitic carbon nitride (g-C3N4). Although phosphorus-modified rGO and rGO/g-C3N4 composites have been extensively studied separately, the combination of both modification approaches within a single material remains largely unexplored. The aim of this work was to synthesize phosphorus- and graphitic carbon nitride-modified reduced graphene oxide via hydrothermal synthesis and to investigate the surface, structural, and morphological properties of the obtained samples. Graphene oxide was prepared using a modified Hummers method and g-C3N4 was obtained by thermal condensation of urea. Hydrothermal synthesis (180 °C, 20 h, aqueous medium) yielded four samples: rGO, P-rGO, rGO/g-C3N4, and P-rGO/g-C3N4, with H3PO4 used as the phosphorus source. The synthesized samples were characterized by X-ray photoelectron spectroscopy (XPS), Fourier-transform infrared spectroscopy (FTIR), Raman scattering spectroscopy, scanning electron microscopy (SEM), and Brunauer–Emmett–Teller (BET) analysis. XPS analysis confirmed effective hydrothermal reduction, as the C/O ratio increased from 2.12 in the GO sample to 6.19 in the rGO sample. It was also determined that after modification, the phosphorus content in the P-rGO sample (5.48 at%) exceeded the values reported in the literature under analogous synthesis conditions. FTIR bands at 1290, 1035, and 505 cm-1 confirmed the covalent incorporation of phosphorus through P–C and P–O–C bonds. In the rGO/g-C3N4 composite, a nitrogen content of 6.50 at% was identified together with N 1s components characteristic of the heptazine network of g-C3N4, while the FTIR peak at 810 cm⁻¹ confirmed the preservation of tri-s-triazine rings after hydrothermal treatment. Raman analysis confirmed that all modified samples exhibited a lower defect density within the sp² carbon sheet plane compared to unmodified rGO. BET analysis showed that hydrothermal reduction increased the specific surface area of rGO to 349 m2 g-1 with predominant ~3–5 nm mesopores, while g-C3N4 incorporation reduced this value to 103 m2 g-1. SEM analysis demonstrated that the morphology of the prepared samples differed significantly. GO exhibited lower crystallinity and a corrugated surface morphology, whereas rGO consisted of loosely packed wrinkled graphene sheets. In contrast, the rGO/g-C3N4 composite showed uniform coverage of the rGO surface with fine g-C3N4 particles. In the phosphorus-modified rGO sample, sheet agglomeration was observed due to phosphate functional groups, while the P-rGO/g-C3N4 composite exhibited a mixed morphology, with an agglomerated surface covered by fine g-C3N4 particles.
Degree
thesis:*- Grantor dc:publisher
- Institutional Repository of Vilnius University
- Year dc:date
- 2026
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Aušra, Modestas,
Rights
dc:rights- Statement dc:rights
-
- info:eu-repo/semantics/openAccess
- Language dc:language
- lit
Identifiers
dc:identifier.*- Repository record dc:identifier
- https://repository.vu.lt/VU:ELABAETD308331766&prefLang=en_US