Back to search

University of Sheffield

Improving the solid electrolyte interphase using pre-lithiation

Abstract

dc:description.abstract

This Thesis focuses on the use of pre-lithiation to influence properties of the solid electrolyte interphase (SEI) and it’s effects on the cycle life of the cells under investigation. Chapter 3 was the result of several experiments investigating the pre-lithiation of graphite. This work demonstrated that the material used for pre-lithiation could be different to the electrolyte and deliver the improved performance over simple pre-lithiation in the electrolyte. This opens the possibility for new pre-lithiation routes of electrodes that result in a lower resistance, longer lasting SEI than can be achieved with solely the electrolyte. Chapter 4 applies the same principles to Si based anodes. This found that whilst the initial capacity of these cells could be increased but the cells suffered from excessive capacity fade. This was found to be a result of SEI cracking/ reformation removing the benefits of a pre-lithiated SEI. Chapter 5 uses the information from chapter 4 to track the SEI reformation process using electrochemical impedance spectroscopy (EIS). This experiment found that the presence of FEC in the electrolyte lowered the resistance of the SEI, even when they were not pre-lithiated in their presence. The reverse was true when it was in the pre-lithiated SEI but not the electrolyte. Chapter 6 looked at pre-lithiated hard carbon electrodes as Na-ion anodes. It was found that pre-lithiated hard carbon anodes had a lower capacity as pre-lithiation time increased. The pre-lithiated electrodes had much greater capacity than the un-lithiated hard carbon which suffered from rapid capacity fade. The solubility of the pre-lithiated SEI was investigated, and it was found that allowing the cell to rest for extended periods increased the capacity of the anode with lower SEI resistance.

Degree

thesis:*
Name dc:type.qualificationname
Ph.D
Level dc:type.qualificationlevel
doctoral
Grantor dc:publisher.institution
University of Sheffield
Year dc:date.issued
2021

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Atkinson, Daniel
Advisors dc:contributor.advisor
  • Howse, Jonathan
  • Cumming, Denis
ORCID person:identifier.orcid

Rights

Language dc:language.dcterms_iso639_2
eng

Identifiers

dc:identifier.*
Identifier
uk.bl.ethos.844247

Chain of custody

source
Harvested from
White Rose University Consortium
Base URL
etheses.whiterose.ac.uk/cgi/oai2
Last updated
2026-11-18
Source record
OAI-PMH GetRecord
related terms
citation

Atkinson, Daniel. Improving the solid electrolyte interphase using pre-lithiation. doctoral thesis, University of Sheffield, 2021.