University of Leeds
High-Temperature Dielectrics Based on Tungsten Bronze Structured Niobate Ceramics
Abstract
dc:description.abstractA novel high temperature dielectric ceramic has been demonstrated based on strontium sodium niobate, Sr2NaNb5O15 (SNN1.0), which has the tungsten bronze crystal structure and shows relaxor-like weak frequency dispersion. Initial experiments involved co-doping with low levels of, Ca2+, Y3+ and Zr4+ to introduce chemical inhomogeneity to broaden the twin dielectric peaks (Curie peak at 305 ᵒC, and a low temperature peak at -15 ᵒC in SNN1.0). The resulting materials were observed to exhibit high and stable relative permittivity across the technologically important -55 to 300 ᵒC temperature range, with the aim of restricting the variation in permittivity to within the Electronics Industries Alliance R-type ±15 % value. Unlike previously reported materials with similar dielectric properties, the new dielectrics do not contain Bi or Pb. In principle this makes them compatible with base metal electrode multilayer ceramic manufacturing processing. For tri-doped compositions, Sr2-x-yCaxYxNaNb5-yZryO15 (SCNN-YZ) dielectric peaks became very diffuse. At x = y = 0.05, median εr values were 1310 +/-10 % from -65 to 300 °C, with dielectric loss tangents, tan δ, ≤ 0.035 from -34 to 378 °C. Microstructural analyses excluded core-shell mechanisms being responsible for the flattening of the εr –T response. A further series of experiments with individual dopants were performed to examine the reasons for peak suppression and attainment of Rtype stability in relative permittivity. It was also realised that SNN was a solid solution Sr2+xNa1-2xNb5O15 (SNN). On cooling from sintering temperatures the SNN1.0 composition, x = 0, lies outside the single phase solid solution region at room temperature and exists as a two phase mixture of the limiting solid solution composition, (x ~ 0.9), and a Sr modified NaNbO3 phase. Sodium deficient variants of SNN (Sr2.1Na0.8Nb5O15, SNN0.8) were therefore investigated to produce a single phase composition. Nevertheless, because the early tri-doped results were based on x = 0 (Sr2NaNb5O15) it was decided to continue to use this as a starting point from which to examine the effects of single-dopants. The single doping experiments indicated that A-site vacancies bring about a severe suppression of the Curie peak. However the presence of all three dopants is required to produce the near flat response which was observed for SCNN-YZ (x = y = 0.05). iv Although the dielectric properties of the SCNN-YZ ceramics appear favourable in terms of developing new high temperature capacitor materials, the presence of Na vacancies in the SNN solid compositions is a drawback. A greater problem was discovered in the latter months of the project. It had been reported in the literature that SNN was metastable below ~1200 °C. The significance of this for a capacitor application would depend on the kinetics of decomposition at capacitor operating temperature. Annealing experiments at 300 to 600 °C were initiated. At 600 °C after only 2 to 3 hours additional phases of SrNb2O6 and Sr2Nb10O27 form from the SNN1.0, indicating partial decomposition. At 400 °C there is evidence of decomposition in SNN0.8 after 24 weeks. Even at 300 °C, the upper working temperature of capacitors for some power electronics applications, there is tentative evidence of structural changes.
Degree
thesis:*- Name dc:type.qualificationname
- Ph.D
- Level dc:type.qualificationlevel
- doctoral
- Grantor dc:publisher.institution
- University of Leeds
- Year dc:date.issued
- 2022
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Brown, Thomas Anthony
- Advisors dc:contributor.advisor
-
- Milne, Steven
- Brown, Andy
Rights
- Language dc:language.dcterms_iso639_2
- eng
Identifiers
dc:identifier.*- Identifier
- uk.bl.ethos.879534