Spelling suggestions: "subject:"aluminium alloys."" "subject:"aluminium molloys.""
111 |
Vliv odplynění na kvalitu odlitků vyrobených technologií vysokotlakého lití / Influence of degasing on casting quality by high pressure castingMíšek, Jakub January 2017 (has links)
This thesis examines the influence of the degassing process on hydrogen contend and on the quality of part casted by high pressure casting technologies. The type of defects occurring in the casting is analyzed based on macrostructure and microstructure observations. For the overall assessment is used the statistical observation of the evolution trend of scrapping during the experiment. The results show that shortening of the degassing time may affect the incidence of porosity defect.
|
112 |
Vliv parametrů odplyňování na kvalitu Al odlitků / Influence of degassing parameters on quality of Al castingsJeřábek, Petr January 2018 (has links)
This master’s thesis is focused on optimalization of degassing parameters in the foundry plant and effect of these parameters on mechanical properties of Al-Si alloys. In practical part is used factorial experiment to research effect of degassing parameters on mechanical properties and dichte index. After optimalization the new process is validated by comparing with the previous one. This experiment was taken on AlSi7Mg0,6 alloy in foundry plant MESIT foundry, a.s.
|
113 |
Řízené naplynění taveniny a jeho vliv na vlastnosti a strukturu odlitků ze slitin hliníku / Controlled melt gassing and its influence on properties and structure of aluminum alloy castingsJagošová, Adriana January 2020 (has links)
The first chapter of the thesis deals with the occurrence of gases in the aluminum melt, what are their sources, what is the solubility of hydrogen in the aluminum melt and the formation of gas cavities. The second chapter divides the defects caused or associated with the presence of gases in the casting. They can be bubbles, shrinkage, or diluents. Pore morphology and its influence on mechanical properties are discussed. The third chapter deals with methods of melt degassing, either by vacuuming, bubbling with active or inert gases, or using special methods and preparations. In the fourth chapter methods for determination of hydrogen content in aluminum melt are divided into analytical methods, methods based on Sieverts law and indication methods. The fifth chapter deals with controlled gassing, its objectives and the preparations used for this purpose. The sixth chapter describes the experiment where the influence of the amount of Probat Fluss Micro 100 on the different casting thicknesses and its results were investigated using a test casting.
|
114 |
Kontrola svarových spojů nájezdových ramp / Inspection of welded joints of loading rampsErtl, Roman January 2020 (has links)
This master's thesis is focused on problem of welding of loading ramps and inspection of their welded joints. The aim of this thesis is to inspect the welds of loading ramps with regarding to the appearance of defects. The literature review of the research issues of the MIG welding technology and welding of aluminium and its alloys is described in this thesis. There is also described destructive and non-destructive inspection of welds that can be applied to inspection of loading ramps. Theoretical description is followed by an experimental part of the thesis. Experimental part is focused on the three destructive tests (the tensile, the macroscopic and the hardness test) of samples of loading ramps, which are made of EN AW-6005A T6.
|
115 |
Korozní ochrana slitin hliníku / Corrosion resistance of aluminum alloysKouba, Jan January 2012 (has links)
This diploma thesis deals with cerium-based conversion coatings for aluminium alloys. At first the mechanism of protection of metals by inhibitory substances is described in the theoretical section. The next chapter is devoted to application of lanthanide salts as cathodic corrosion inhibitors. Then the characterization of alloy AA 2024 follows. The main part is dedicated to the growth mechanism of the cerium-based mixed conversion coating on the alloy AA 2024. Finally, the factors affecting the character and the quality of obtained coatings are commented. In the experimental part an influence of the thermal activation together with the activation by a hydrogen peroxide was observed. The created film was characterized using SEM and EDS. The level of corrosion protection was evaluated by the polarization resistance measurement. erized using SEM and EDS. The level of corrosion protection was evaluated by the polarization resistance measurement.
|
116 |
Povrchové úpravy hliníkových slitin / Surface treatment of aluminum alloysPetr, Jiří January 2013 (has links)
The thesis is focused on the surface treatment used for the preparation of aluminium alloys for the adhesive bonding. The theoretical part can be divided into three chapters. The first of them deals with aluminium alloys, the second one speaks about the adhesive bonding. The surface treatment itself, especially the conversion coating issues, is discussed in the last chapter. The experimental part is focused on the optimalization of a two-step titanium and zirconium based conversion coating technology. In the first part, the aluminium alloy is analysed by the glow discharge optical emission spectroscopy. The second part of the experiment deals with the first step of the technology, acidic deoxidation. The objective was to examine the influence of the exposure time on the morphology of the alloy surface and the shear strength of adhesive joints. In the last part of the experiment, the conversion coatings are prepared and characterised by the scanning electron microscopy and energy dispersive spectroscopy.
|
117 |
Vliv filtrů na plnění formy při odlévání slitin hliníku / Influence of filters on running of metal flowMakalouš, Jakub January 2008 (has links)
This study deals with influence of filters on running of aluminum metal flow. The main objective was to describe hydraulic resistances of assorted filters and running of silting filters by inclusions. Theoretical part generally describes filtration process and also filtration from the point of view of aluminum alloys and the most important characteristics of each type of alumina inclusions. Experimental part deals with flow rate tests, influence of filters on gassiness of melt and metallographic analysis. It was find out, that filter GEPHAL made minimal hydraulic resistance, on the other hand ceramic foam filters type LD made the maximal hydraulic resistance. It is necessary to reduce filtration surface for study running of silting filters by inclusions. Metallographic analysis showed amorphous alumina film inclusions, spinell Al2O3.2MgO, sludge and carbide of silicon.
|
118 |
Návrh a výroba příruby náboje zadního kola formule pomocí technologie CAD/CAM a dílenského CNC programování / Design and machining of the flange hub rear wheel of the formula by using CAD/CAM technology and CNC workshop programmingLučaník, Aleš January 2013 (has links)
This master's thesis deals with design and machining of the flange hub rear wheel of the formula by using CAD/CAM technology and CNC workshop programming. The introductory part provides theoretical description and characteristic of turning and milling technology. Further work describes aluminium alloys with focus on material which was used as a blank for machined workpiece. The practical part deals with design of flange in CAD software Autodesk Inventor, design of turning strategies in system ShopTurn and design of milling strategies in software PowerMILL. The final part of this thesis specifies realization of manufacturing on CNC lathe and CNC machining center in company BOSCH DIESEL s.r.o. in Jihlava. Last chapter is focused on techno-economic aspects of manufacturing.
|
119 |
Mikrostruktura a mechanické vlastnosti hliníkových slitin po intenzivní plastické deformaci / Microstructure and mechanical properties of aluminium alloys prepared by severe plastic deformationBajer, Jan January 2015 (has links)
New technologies of components assembling in car and aircraft industries and requests on improved mechanical and corrosion properties of metallic materials in the packing industry activate the utilization of highly innovative and unconventional manufacturing processes. There are only a limited number of processing, that retain the original material thickness and in an appropriate manner modify material properties. These are different types of annealing, severe plastic deformation methods or combination of both. In recent years constrained groove pressing (CGP) was devoloped with this method the grain size can be reduced from tens of micrometers to sub-micrometers. The present work is focused on a study of evolution of microstructure and mechanical properties of two alloys based on EN AW 3003 after CGP deformation and subsequent annealing.
|
120 |
Hot Tearing Susceptibility of Single-Phase Al-3.8 wt%Zn-1 wt%Mg Alloy Using the Constrained Rod Solidification Experiment: Influence of 1.2 wt%Fe Addition and Grain RefinementMaia Aguiar, Amanda January 2020 (has links)
The increasing global demand for a substantial lightweighting of automobiles to enable a reduction in the greenhouse gas (GHG) emissions and fuel consumption has led to the adaptation of the high strength Al wrought alloys such as the 2xxx and 7xxx series in near net-shaped manufacturing using the high pressure die casting (HPDC) process. However, the obstacle for this adaptation is the high susceptibility to hot tearing during the solidification of these alloys. A new structural Al alloy for high pressure die casting application was developed from the single-phase Al-Zn-Mg family; a high strength and ductile alloy that could be adapted to manufacturing automotive structural components using HPDC and help with a significant reduction in the overall curb-weight of an automobile and thereby increasing the vehicle fuel efficiency. The objective of this study was to enable a better understanding of the hot tearing phenomenon during solidification of the Al-3.8 wt%Zn-1 wt%Mg alloy, the effect of adding 1.2 wt% Fe to the alloy to improve the castability in HPDC process and the effect of adding Ti as a grain refiner of the primary Al phase during solidification of the alloy using Al-5 wt%Ti-1 wt%B master alloy. The constrained rod solidification (CRS) experiments were carried out to measure transient stress, transient strain, and transient temperature during solidification of the alloy. Improvements to the CRS experiments were also developed to obtain a repeatability of the acquired data. The computerized Tomography (CT) imaging was used to visually characterize the hot tearing. Hypothesis on the factors promoting the hot tearing tendencies in single-phase alloys solidified using net-shaped casting processes has been presented with evidence-based on transient stress-strain and thermal data curves obtained during the solidification experiments. / Thesis / Master of Applied Science (MASc)
|