Effect of Microstructure Changes on Mechanical Properties of La₆₆Al₁₄(Cu, Ni)₂₀ Amorphous and Crystalline AlloysZhang, Yong, Lee, Irene Mei Ling, Tan, Hao, Jing, Qin, Li, Yi 01 1900 (has links)
The microstructure, and phase selections of La₆₆Al₁₄(Cu, Ni)₂₀ alloy were studied by Bridgman solidifications, and composite materials of dendrites in amorphous matrix or micro- and nano- sized eutectic matrix were formed with different cooling rates. The volume fraction of the dendrite phase reaches a maximum at the cooling rate of about 15 K/s, the secondary dendrite arm spacing λ₂ decreases from 4.3 µm to 0.6 µm with the increasing of cooling rate R, and obeys the equation of λ₂R⁰.⁵⁷=1.74µm(K/s)R⁰.⁵⁷. The compression strength, as well as the elastic strain limit of the dendrite/amorphous matrix composite are 600 MPa, and 2.3%, respectively. Improved ductility was observed for the dendrite amorphous matrix composites with more dendrite phase by slow cooling rate. / Singapore-MIT Alliance (SMA)
|
Page generated in 0.1142 seconds