1

Hidrogenação do ciclohexeno utilizando ferrocarbonilas como catalisadores

Buffon, Regina January 1988 (has links)
Neste trabalho foi estudada a hidrogenação catalítica do ciclohexeno, promovida por irradiação UV-Visível (À >280 nm), na presença de Fe(CO)5' Fe2 (CO)9 e Fe3 (CO)12. Foram obtidas freqüências de rotação máxima, após uma hora de fotólise, de 2,15 ± 0,11 h-1, para o Fe2 (CO)9' e 1,53 ± 0,08 h , para os sistemas Fe(CO)5' Fe3 (CO)12. A única espécie Fe(CO)n-x(◊)x' n = 5, detectada por infravermelho foi o Fe(CO)4(◊), presente em maior quantidade nas reações efetuadas a T ≤ O °C. Quando os testes catalíticos foram efetuados utilizando-se Fe3 (CO)12 impregnado em aluminas, Y ou neutra, não foi detectada hidrogenação do ciclohexeno, seja fotoquímica (T ≤ O °C ou T ambiente), seja termicamente (T = 80 + 2 °C). A utilização da espécie [HFe3(CO)11]- Et4N+, em solução, também não levou a formação do ciclohexano, evidenciando que o ânion [HFe 3 (CO)11]-' formado sobre a superfície da alumina, não é cataliticamente ativo para a hidrogenação do ciclohexeno, nas condições deste trabalho ([Fel/ [ciclohexeno] = 1/10, fluxo de hidrogênio). / In this work the hidrogenation of cyclohexene promoted by UV-visible irradiation (À > 280 nm) in the presence of Fe(CO)5' Fe2 (CO)g and Fe3 (CO)12 was studied. The maximum turnover rates obtained were 2,15 ± 0,11 h- 1 for Fe2 (CO)g and -1 1,53 ±0,08 h for the systems Fe(CO)5 and Fe 3 (CO)12' The only species Fe (CO) n-x (◊) x' n = 5, detected by infrared was Fe(CO)4 (◊), presented in larger quantities in the reactions at T ± O ºC. When the catalytical tests were performed with Fe 3 (CO) 12 impregnated in y or neutral alumina no hydrogenation of cyclohexene was detected, whether was it photochemical o o (at T ± 0° C or room temperature) or thermally (T = 80 ± 2 ºC) • Use of the species [HFe3 (CO)11]- Et4N+ in solution has also failed to form cyclohexane. This result suggests that the anion [HFe3 (CO)11]- formed in the alumina surface 1s not catalyt1cally active for the hydrogenation of cyclohexene in the condit1ons of this work ([Fe] / [Cyclohexene]) = 1/10, hydrogen flux).
2

Hidrogenação do ciclohexeno utilizando ferrocarbonilas como catalisadores

Buffon, Regina January 1988 (has links)
Neste trabalho foi estudada a hidrogenação catalítica do ciclohexeno, promovida por irradiação UV-Visível (À >280 nm), na presença de Fe(CO)5' Fe2 (CO)9 e Fe3 (CO)12. Foram obtidas freqüências de rotação máxima, após uma hora de fotólise, de 2,15 ± 0,11 h-1, para o Fe2 (CO)9' e 1,53 ± 0,08 h , para os sistemas Fe(CO)5' Fe3 (CO)12. A única espécie Fe(CO)n-x(◊)x' n = 5, detectada por infravermelho foi o Fe(CO)4(◊), presente em maior quantidade nas reações efetuadas a T ≤ O °C. Quando os testes catalíticos foram efetuados utilizando-se Fe3 (CO)12 impregnado em aluminas, Y ou neutra, não foi detectada hidrogenação do ciclohexeno, seja fotoquímica (T ≤ O °C ou T ambiente), seja termicamente (T = 80 + 2 °C). A utilização da espécie [HFe3(CO)11]- Et4N+, em solução, também não levou a formação do ciclohexano, evidenciando que o ânion [HFe 3 (CO)11]-' formado sobre a superfície da alumina, não é cataliticamente ativo para a hidrogenação do ciclohexeno, nas condições deste trabalho ([Fel/ [ciclohexeno] = 1/10, fluxo de hidrogênio). / In this work the hidrogenation of cyclohexene promoted by UV-visible irradiation (À > 280 nm) in the presence of Fe(CO)5' Fe2 (CO)g and Fe3 (CO)12 was studied. The maximum turnover rates obtained were 2,15 ± 0,11 h- 1 for Fe2 (CO)g and -1 1,53 ±0,08 h for the systems Fe(CO)5 and Fe 3 (CO)12' The only species Fe (CO) n-x (◊) x' n = 5, detected by infrared was Fe(CO)4 (◊), presented in larger quantities in the reactions at T ± O ºC. When the catalytical tests were performed with Fe 3 (CO) 12 impregnated in y or neutral alumina no hydrogenation of cyclohexene was detected, whether was it photochemical o o (at T ± 0° C or room temperature) or thermally (T = 80 ± 2 ºC) • Use of the species [HFe3 (CO)11]- Et4N+ in solution has also failed to form cyclohexane. This result suggests that the anion [HFe3 (CO)11]- formed in the alumina surface 1s not catalyt1cally active for the hydrogenation of cyclohexene in the condit1ons of this work ([Fe] / [Cyclohexene]) = 1/10, hydrogen flux).
3

Hidrogenação do ciclohexeno utilizando ferrocarbonilas como catalisadores

Buffon, Regina January 1988 (has links)
Neste trabalho foi estudada a hidrogenação catalítica do ciclohexeno, promovida por irradiação UV-Visível (À >280 nm), na presença de Fe(CO)5' Fe2 (CO)9 e Fe3 (CO)12. Foram obtidas freqüências de rotação máxima, após uma hora de fotólise, de 2,15 ± 0,11 h-1, para o Fe2 (CO)9' e 1,53 ± 0,08 h , para os sistemas Fe(CO)5' Fe3 (CO)12. A única espécie Fe(CO)n-x(◊)x' n = 5, detectada por infravermelho foi o Fe(CO)4(◊), presente em maior quantidade nas reações efetuadas a T ≤ O °C. Quando os testes catalíticos foram efetuados utilizando-se Fe3 (CO)12 impregnado em aluminas, Y ou neutra, não foi detectada hidrogenação do ciclohexeno, seja fotoquímica (T ≤ O °C ou T ambiente), seja termicamente (T = 80 + 2 °C). A utilização da espécie [HFe3(CO)11]- Et4N+, em solução, também não levou a formação do ciclohexano, evidenciando que o ânion [HFe 3 (CO)11]-' formado sobre a superfície da alumina, não é cataliticamente ativo para a hidrogenação do ciclohexeno, nas condições deste trabalho ([Fel/ [ciclohexeno] = 1/10, fluxo de hidrogênio). / In this work the hidrogenation of cyclohexene promoted by UV-visible irradiation (À > 280 nm) in the presence of Fe(CO)5' Fe2 (CO)g and Fe3 (CO)12 was studied. The maximum turnover rates obtained were 2,15 ± 0,11 h- 1 for Fe2 (CO)g and -1 1,53 ±0,08 h for the systems Fe(CO)5 and Fe 3 (CO)12' The only species Fe (CO) n-x (◊) x' n = 5, detected by infrared was Fe(CO)4 (◊), presented in larger quantities in the reactions at T ± O ºC. When the catalytical tests were performed with Fe 3 (CO) 12 impregnated in y or neutral alumina no hydrogenation of cyclohexene was detected, whether was it photochemical o o (at T ± 0° C or room temperature) or thermally (T = 80 ± 2 ºC) • Use of the species [HFe3 (CO)11]- Et4N+ in solution has also failed to form cyclohexane. This result suggests that the anion [HFe3 (CO)11]- formed in the alumina surface 1s not catalyt1cally active for the hydrogenation of cyclohexene in the condit1ons of this work ([Fe] / [Cyclohexene]) = 1/10, hydrogen flux).