• Refine Query
  • Source
  • Publication year
  • to
  • Language
  • 3
  • Tagged with
  • 3
  • 3
  • 2
  • 2
  • 2
  • 2
  • 2
  • 2
  • 2
  • 2
  • 2
  • 2
  • 2
  • 2
  • 2
  • About
  • The Global ETD Search service is a free service for researchers to find electronic theses and dissertations. This service is provided by the Networked Digital Library of Theses and Dissertations.
    Our metadata is collected from universities around the world. If you manage a university/consortium/country archive and want to be added, details can be found on the NDLTD website.
1

Caracterização de jatos moleculares supersônicos por espectrometria de massa e espectroscopia de alta resolução

Antonio Osny de Toledo 00 December 2001 (has links)
A molécula de SF6 em jato molecular supersônico é estudada por duas técnicas experimentais diferentes, visando observar os aglomerados gerados por resfriamento em expansão supersônica. Descrevemos e comentamos as montagens dos experimentos de caracterização do jato molecular supersônico, da espectrometria de massas associada a uma ionização do tipo multifotônica e da espectroscopia infravermelha de alta resolução. Os resultados experimentais de maior relevância são apresentados e discutidos.
2

Produção de nanopartículas de Au induzida por pulsos laser de femtossegundos formatados / Gold nanoparticles production induced by shaped femtosecond laser pulses

Ferreira, Paulo Henrique Dias 27 October 2011 (has links)
Neste trabalho investigamos a dinâmica de formação de nanopartículas de Au por pulsos de femtossegundos formatados (800 nm, 30 fs, 1 kHz e 2 mJ), induzida pela ionização da molécula de quitosana. Inicialmente desenvolvemos um sistema de formatação de pulsos ultracurtos que faz uso de um modulador espacial de luz, constituído por um arranjo linear de cristais líquidos, com o qual somos capazes de impor distintas modulações de fase ao pulso laser. Para monitorar o processo de produção de nanopartículas, montamos um sistema de excitação (pulsos de femtossegundos) e prova (luz branca), o qual permite a observação em tempo real do aparecimento da banda de plásmon e, consequentemente, da dinâmica de formação das nanopartículas. Resultados obtidos para pulsos não formatados (limitados por Transformada de Fourier) demonstraram que a formação de nanopartículas deve-se à ionização não linear da quitosana, a qual está relacionada à oxidação do grupo hidroxila para o grupo carbonila. Medidas de microscopia eletrônica de transmissão forneceram os tamanhos (entre 20 e 100 nm) e formatos (esferas, pirâmides, hexágonos, bastões, etc) das nanopartículas geradas. Ainda, nossos resultados revelaram que esta ionização é iniciada por absorção multifotônica, mais especificamente por absorção de 4 fótons. Utilizando pulsos formatados com fase espectrais constante, degrau e cossenoidal com diferentes frequências, investigamos a influência destes na formação de nanopartículas. Concluímos que os pulsos mais longos são mais favoráveis ao processo de ionização, e consequente redução dos íons de Au para a formação de nanopartículas metálicas. Este comportamento se deve, provavelmente, à redistribuição da energia absorvida para os modos vibracionais, o que é mais provável para pulsos mais longos. Assim, o método apresentado pode abrir novas maneiras para a formação de nanopartículas de metálicas, as quais podem ser mais exploradas dos pontos de vista aplicado e fundamental. / In this work we have studied the synthesis of Au nanoparticles using shaped ultrashort pulses (800 nm, 30 fs, 1 kHz and 2 mJ), induced by the ionization of the chitosan. Initially we developed a pulse shaping setup that uses a spatial light modulator (liquid crystals array), with which we are able to impose distinct phase mask to the laser pulse. In order to monitor the nanoparticles production process, we used a pump-probe system, consisting of femtosecond pulses (pump) and white light (probe), which allows the observation of the plasmon band enhancement and hence the nanoparticles formation dynamics. The results obtained by Fourier Transform limited pulses have shown that the nanoparticles formation is due to the nonlinear ionization of chitosan, which is related to hydroxyl group oxidation to the carbonyl group. Transmission electron microscopy measurements provided the sizes (20-100 nm) and shapes (spheres, pyramids, hexagons, rods, etc.) of the produced nanoparticles. Moreover, our results revealed that ionization is initiated by multiphoton absorption, more specifically by four photons absorption. Using pulses shaped with constant, step and cossenoidal (with different frequencies) spectral phase masks, we investigated their influence in the nanoparticles formation. We conclude that longer pulses are more favorable to the ionization process and, consequently, to the gold ions reduction for the synthesis of the metallic nanoparticles. This behavior is probably due to the redistribution of the absorbed energy to the vibrational modes, which is more likely for longer pulses. Therefore, the approach presented here can open new ways to produce metallic nanoparticles, which can be further explored from applied and fundamental points of view.
3

Produção de nanopartículas de Au induzida por pulsos laser de femtossegundos formatados / Gold nanoparticles production induced by shaped femtosecond laser pulses

Paulo Henrique Dias Ferreira 27 October 2011 (has links)
Neste trabalho investigamos a dinâmica de formação de nanopartículas de Au por pulsos de femtossegundos formatados (800 nm, 30 fs, 1 kHz e 2 mJ), induzida pela ionização da molécula de quitosana. Inicialmente desenvolvemos um sistema de formatação de pulsos ultracurtos que faz uso de um modulador espacial de luz, constituído por um arranjo linear de cristais líquidos, com o qual somos capazes de impor distintas modulações de fase ao pulso laser. Para monitorar o processo de produção de nanopartículas, montamos um sistema de excitação (pulsos de femtossegundos) e prova (luz branca), o qual permite a observação em tempo real do aparecimento da banda de plásmon e, consequentemente, da dinâmica de formação das nanopartículas. Resultados obtidos para pulsos não formatados (limitados por Transformada de Fourier) demonstraram que a formação de nanopartículas deve-se à ionização não linear da quitosana, a qual está relacionada à oxidação do grupo hidroxila para o grupo carbonila. Medidas de microscopia eletrônica de transmissão forneceram os tamanhos (entre 20 e 100 nm) e formatos (esferas, pirâmides, hexágonos, bastões, etc) das nanopartículas geradas. Ainda, nossos resultados revelaram que esta ionização é iniciada por absorção multifotônica, mais especificamente por absorção de 4 fótons. Utilizando pulsos formatados com fase espectrais constante, degrau e cossenoidal com diferentes frequências, investigamos a influência destes na formação de nanopartículas. Concluímos que os pulsos mais longos são mais favoráveis ao processo de ionização, e consequente redução dos íons de Au para a formação de nanopartículas metálicas. Este comportamento se deve, provavelmente, à redistribuição da energia absorvida para os modos vibracionais, o que é mais provável para pulsos mais longos. Assim, o método apresentado pode abrir novas maneiras para a formação de nanopartículas de metálicas, as quais podem ser mais exploradas dos pontos de vista aplicado e fundamental. / In this work we have studied the synthesis of Au nanoparticles using shaped ultrashort pulses (800 nm, 30 fs, 1 kHz and 2 mJ), induced by the ionization of the chitosan. Initially we developed a pulse shaping setup that uses a spatial light modulator (liquid crystals array), with which we are able to impose distinct phase mask to the laser pulse. In order to monitor the nanoparticles production process, we used a pump-probe system, consisting of femtosecond pulses (pump) and white light (probe), which allows the observation of the plasmon band enhancement and hence the nanoparticles formation dynamics. The results obtained by Fourier Transform limited pulses have shown that the nanoparticles formation is due to the nonlinear ionization of chitosan, which is related to hydroxyl group oxidation to the carbonyl group. Transmission electron microscopy measurements provided the sizes (20-100 nm) and shapes (spheres, pyramids, hexagons, rods, etc.) of the produced nanoparticles. Moreover, our results revealed that ionization is initiated by multiphoton absorption, more specifically by four photons absorption. Using pulses shaped with constant, step and cossenoidal (with different frequencies) spectral phase masks, we investigated their influence in the nanoparticles formation. We conclude that longer pulses are more favorable to the ionization process and, consequently, to the gold ions reduction for the synthesis of the metallic nanoparticles. This behavior is probably due to the redistribution of the absorbed energy to the vibrational modes, which is more likely for longer pulses. Therefore, the approach presented here can open new ways to produce metallic nanoparticles, which can be further explored from applied and fundamental points of view.