Control of diffusible weld metal hydrogen through arc chemistry modificationsDu Plessis, John. January 2006 (has links)
Thesis (M. Sc.(Metallurgy))-University of Pretoria, 2006. / Includes bibliographical references (leaves 62-65). Available on the Internet via the World Wide Web.
|
2 |
The melting point and viscosity of nickel smelter slagsDucret, Andrew Charles Unknown Date (has links) (PDF)
Western Mining Corporation produces nickel matte at the Kalgoorlie Nickel Smelter(KNS)from nickel sulphide concentrates within an integrated flash smelter.
|
3 |
Heat transfer through mould flux with titanium oxide additionsBothma, Jan Andries. January 2006 (has links)
Thesis (M.Eng.)(Metallurgical)--University of Pretoria, 2006. / Includes summary. Includes bibliographical references. Available on the Internet via the World Wide Web.
|
4 |
Materiais corretivos da acidez do solo no desenvolvimento inicial e nutrição da cultura da mamonaSantos, Carlos Lacy 17 December 2010 (has links)
Made available in DSpace on 2016-12-23T14:37:42Z (GMT). No. of bitstreams: 1
Carlos Lacy Santos.pdf: 610209 bytes, checksum: 3345388b917bb47a5a2901cd23eb9383 (MD5)
Previous issue date: 2010-12-17 / Este trabalho objetivou avaliar o uso de diferentes materiais corretivos de acidez do solo no desenvolvimento inicial e nutrição mineral da mamona em condição de casa de vegetação. O experimento foi montado num esquema fatorial 2x6, sendo dois Latossolos (LVA I e LVA II), e cinco materiais corretivos de acidez do solo (calcário, resíduo de mármore, escória de metalurgia, produto proveniente de algas marinhas, resíduo de rocha (50% mármore + 50% granito), e testemunha (sem aplicação de corretivo), num delineamento em blocos casualizados com quatro repetições. A mamoneira (cultivar IAC-80) foi cultivada por 45 dias em casa de vegetação, com duas plantas de mamona por vaso. Ao final do período procedeu-se a quantificação da matéria seca da parte aérea (folha e caule), matéria seca da raiz e volume de raízes e determinaram-se os teores e acúmulos de P, K, Ca e Mg na folha e no caule. Os dados foram submetidos à análise de variância e quando significativos foi utilizado o teste de F a 5 % de probabilidade para comparação das médias dos resultados através de contrastes. Os resultados mostraram que houve comportamento diferenciado dos materiais corretivos de acidez e dos solos sobre o desenvolvimento inicial e a nutrição mineral da mamoneira. Para ambos os solos, de maneira geral, o uso de materiais corretivos proporcionou maior desenvolvimento inicial da mamoneira em relação à testemunha (sem aplicação de corretivo), evidenciando a importância da correção da acidez do solo para a cultura. A aplicação de materiais corretivos da acidez promoveu uma redução dos teores de P, K na parte aérea da mamoneira, dado o efeito de diluição, pela maior produção de matéria seca. A aplicação dos materiais corretivos permitiu a elevação dos teores Ca e Mg na parte aérea da mamoneira em relação à testemunha, somente no solo LVA II, o qual apresentava, originalmente, menor disponibilidade destes nutrientes em relação ao LVA I (Tabela 1). De maneira geral, os maiores valores de acúmulo dos nutrientes ocorreram nos tratamentos que proporcionaram maior produção de matéria seca, com destaque para os corretivos resíduo de mármore e resíduo de mármore (50%) + resíduo de granito (50%) que promoveram maior acúmulo de K, Ca e Mg tanto na folha quanto no caule da mamoneira, no LVA II. A utilização de materiais corretivos em solos ácidos cultivados com mamoneira demonstrou potencial no desenvolvimento inicial e na nutrição mineral desta cultura nas condições avaliadas / This study aimed to evaluate the use of different correctives materials of Soil acidity in the initial development and mineral nutrition in castor bean crops greenhouse condition. The experiment was a factorial scheme of 2x6, two soils Oxisols (LVA I and II), and five of corrective materials of soil acidity (limestone, marble waste, metallurgy slag, product from seaweed, waste rock (50% + 50% marble granite), and control (without application of lime) in a randomized block design with four repetitions. The Castor tree (IAC-80), cultivated for 45 days in a greenhouse, two plants of castor bean by vessel. At this time we proceeded to quantify the dry matter of the shoot (leaf and stem), root dry matter and root volume and measured the contents and accumulation of P, K, Ca and Mg in leaves and stem. Data were subjected to analysis of variance and significant when we used the F test at 5% probability to compare the average of results through contrasts. The results showed different behaviors of the materials for acidity of soil on the mineral nutrition and initial development of castor bean. For both soils, in general, the use of corrective materials provided greater initial development of castor bean in relation to control (without application of corrective), highlighting the importance of acidity in the soil for this culture. The application of corrective materials promoted a reduction of acidity of P, K in the shoot of castor beans, given the dilution effect, by the higher dry matter production. The application of corrective materials allowed high levels of Ca and Mg in shoots of castor bean in relation the control, only the soil LVA II, which originally presented lower nutrient availability in relation to the LVA I (Table 1). In Generally, the higher accumulation of nutrients occurred in the treatments that showed higher dry matter production, especially the Marble and lime residue, marble residue (50%) + granite waste (50%) that promoted a higher accumulation of K, Ca and Mg in both the leaf and the stem of the castor bean, the LVA II. The use of corrective materials in acid soils cultivated with castor bean showed a potential in the initial developent and mineral nutrition of this crop under the conditions evaluated
|
5 |
Ein Beitrag zur Verschlackung von MgO in sekundärmetallurgischen SchlackenBrüggmann, Christian 29 April 2011 (has links)
Die vorliegende Arbeit behandelt Aspekte der Verschlackung von MgO in sekundärmetall-urgischen Schlacken. Mittels FactSage© wird eine Berechnung der Löslichkeit von MgO in Kalksilikat- und Kalkaluminatschlacke bei 1600, 1650 und 1700°C durchgeführt. Die Ergebnisse werden leicht handhab- und ablesbar dargestellt. Die Verschlackung eines porösen MgO-Probekörpers in einer an MgO ungesättigten und an MgO gesättigten Kalkaluminat-schlacke wird bei 1600°C thermogravimetrisch verfolgt. Der Verschlackungsvorgang wird maßgeblich durch die Mechanismen der Teilchendesintegration und Ostwald-Reifung in der infiltrierten Mikrostruktur beeinflusst. Das komplexe Zusammenspiel von Zerfall und Auflösung wird nach einem Modell von W. Gans an feuerfestes Material (MgO) angepasst und modelliert. Der Einfluss von Teilchendesintegration und Ostwald-Reifung auf den voreilenden Verschleiß im 3-Phasenkontakt (Marangoni-Konvektion) wird quantifiziert. Ferner wird ein einfaches Modell zur Abschätzung des voreilenden Verschleißes dargelegt.
|