Fällning av kisel från avloppsvatten vid Hellisheidarvirkjun - experimentell studie / Experiments with precipitation of silica from waste water at Hellisheiðarvirkjun

This report is about the experiments with mixing of the separated water and the vacuum pump seal water at Hellisheiði power plant. This is done to prevent silica scaling and clogging in pipes and reinjection wells as well as eliminating vacuum pump seal water from the plant. The experiments were done in four stages: the first stage comprised of tests with different flows of separated water at 70°C, the second stage was carried out by mixing the separated water at 70°C and the seal water with different amounts of the seal water, the third and the fourth stages were like the first and second but with the separated water at 120°C. The results show that this method is good if the mixture is around 50/50 separated water and seal water, to control the silica scaling in the separated water and to be able to reinject the seal water with the separated water. This does not eliminate the silica scaling in all of the separated water because the amount of separated water is much more than the amount of seal water that comes from the plant.

Identiferoai:union.ndltd.org:UPSALLA1/oai:DiVA.org:kth-170628
Date January 2015
CreatorsÓLAFSDÓTTIR, VERA SÓLVEIG
PublisherKTH, Skolan för kemivetenskap (CHE)
Source SetsDiVA Archive at Upsalla University
LanguageSwedish
Detected LanguageEnglish
TypeStudent thesis, info:eu-repo/semantics/bachelorThesis, text
Formatapplication/pdf
Rightsinfo:eu-repo/semantics/openAccess

Page generated in 0.0018 seconds