Back to search

Freie Universität Berlin

Scherhaftfestigkeit von CAD/CAM-Hybridmaterialien für die subtraktive und additive Fertigung unter Verwendung verschiedener Reparaturprotokolle

Abstract

dc:description.abstract

Objectives: Clinical failures of CAD/CAM restorations such as chipping or fractures necessitate reliable intraoral repair options as an alternative to complete replacement. With the increasing use of additively manufactured (3D-printed) hybrid materials for definitive restorations, the question arises whether these materials demonstrate comparable repairability to subtractively manufactured (milled) materials. The aim of this in vitro study was to evaluate the shear bond strength (SBS) of different CAD/CAM hybrid materials for subtractive and additive manufacturing using three commercially available repair protocols and to investigate the influence of artificial aging by thermocycling. Methods: Two milled hybrid materials (Vita Enamic, VE; Voco Grandio Blocs, VG) and one experimental 3D-printed hybrid material (3D) were tested. Rectangular specimens (n = 180) were prepared following the principles of DIN EN ISO 10477. Three repair protocols were applied: Monobond Plus combined with Optibond FL (MO), GC Repair Kit consisting of G-Multi Primer and G-Premio Bond (GC), and Voco Cimara consisting of silane and adhesive (VC). Repairs were performed using a nanoceramic composite (Ceram.X Spectra ST). Half of the specimens per group (n = 10) underwent artificial aging by 30.000 thermocycles (5–55 °C). Shear bond strength was measured using a universal testing machine (RetroLine Z010, Zwick/Roell). Fracture surfaces were analyzed by light microscopy and scanning electron microscopy. Statistical analysis was performed using multi-factor ANOVA and post-hoc tests (α = 0.05). Results: The repair protocol and material type significantly influenced SBS. MO achieved the highest SBS values both before and after thermocycling, while GC consistently yielded the lowest values. Thermocycling significantly reduced SBS in milled materials (VE, VG) across almost all repair protocols. In contrast, the 3D-printed material showed an opposite effect: only the combination of GC with 3D demonstrated an increase in SBS after thermocycling. In 57 out of 60 specimens of the 3D-printed material, substrate failure occurred, indicating that the repair SBS exceeded the intrinsic strength of the material. Regarding failure modes, mixed adhesive-cohesive failures predominated before thermocycling, while adhesive failures became more prevalent after aging. 14 Conclusions: SBS was significantly influenced by material type and repair protocol. MO proved to be the most effective repair system for all tested materials. Thermocycling reduced SBS in milled materials, while the 3D-printed material demonstrated stable or improved repair bond strength after artificial aging. The results emphasize the need for material-specific repair strategies and suggest that additively manufactured hybrid materials represent a promising clinical alternative with regard to repairability.

Degree

thesis:*
Department dc:contributor.department
Charité - Universitätsmedizin Berlin
Year dc:date.issued
2026

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Milicevic, Marko
Committee member dc:contributor.committeemember
  • N.N.

Subjects

dc:subject × 8

Rights

dc:rights.accessrights
Statement dc:rights.accessrights
  • open access
Language dc:language
ger

Identifiers

dc:identifier.*
URN
urn:nbn:de:kobv:188-refubium-52671-9

Chain of custody

source
Harvested from
Freie Universität Berlin
Base URL
refubium.fu-berlin.de/oai/request
Last updated
2026-11-19
Source record
OAI-PMH GetRecord
citation

Milicevic, Marko. Scherhaftfestigkeit von CAD/CAM-Hybridmaterialien für die subtraktive und additive Fertigung unter Verwendung verschiedener Reparaturprotokolle. 2026. https://refubium.fu-berlin.de/handle/fub188/52671