dc:description

Reclaimed polystyrene ("Styrofoam") in combination with alkyd resin, paraffin wax and gum rosin were used in the form of solutions in organic solvent to improve water repellency and mechanical properties of wood. Polystyrene was used in concentrations of 5, 10, 15 and 20%, alkyd resin in a concentration of 5%, gum rosin was also used in a concentration of 5% and paraffin wax in a concentration of 0.5%. The impregnation of filter paper samples with the solutions showed that increasing the concentration of solid components of water repellent (W.R.) solutions resulted in an increase in the retention of the impregnated filter paper and increases the "grammage". Increasing "grammage" had the effect of reducing the absorption of water and increases the bursting strength, the bending resistance, the ring crush resistance and the compression strength. Having added the paraffin wax, rosin and alkyd resin in polystyrene solutions it was found that paraffin wax was more hydrophobic compared to polystyrene, alkyd resin, gum rosin, and gum rosin more hydrophobic than polystyrene and alkyd resin. The impregnation of the filter paper with solutions that contain alkyd resin and gum rosin improves all the mechanical properties were studied in comparison with the solutions containing paraffin wax. In order to study the influence of the weathering factors in W.R. solutions, wood specimens of pine and beech, with dimensions 2 cm radial x 2 cm tangential x 2 cm longitudinal, were used. After their impregnation they were exposed outdoors on cross section during the period November 2011-August 2012. In experimental water repellent (E.W.R.) solutions the concentrations of polystyrene were 10% and 20%, of alkyd resin and of gum rosin were 1.25 % and 2.5% and the concentration of paraffin wax was 0.5% (Treatments A, B, C, D). Also commercial water repellent (C.W.R.) solutions were used (Treatments G, H). Based on combination of the solutions and the way specimens were impregnated, the resulting sample treatments were 13 (A, B, C,….., M) as well as one untreated control (O). The study showed that the increase of the concentration of the solid ingredients of solutions resulted in an increase in the retention of the impregnated pine and beech specimens. The retention was found higher in pine compared with beech and in treatments with the commercial water repellents. The comparison based on the maximum tangential swelling (specimens were immersed in water for 180 min) showed that: In all treatments that were studied (W.R. solution of different combinations) higher concentrations (and retentions) are associated with lower values of tangential swelling for both wood species before and after the outdoor exposure. Also in all cases (W.R. solutions, wood species) the tangential swelling, after the exposure in weather conditions, increased. The treatments with the E.W.R. solutions were found less effective compared with the C.W.R. solutions, but in some cases E.W.R. solutions were better than the treatments with C.W.R solutions. Based on the appearance of radial checks observed in transverse surfaces of wood samples exposed in weather conditions, the best treatments (best wood protection, check avoidance) were found to be those with C.W.R. substances (H, I) and those with C.W.R. substances and E.W.R. solutions (L, M) in pine and in beech the best treatments were those with C.W.R. substances and E.W.R. solutions (L, M). Based on the theoretical times required for wood samples to attain half (1/2) and quarter (1/4) maximum swelling, was found that most effective treatments (more time required), for both wood species, were the treatments H, I (commercial solutions) and J, K, L, M treatments (experimental and commercial solutions). The evaluation of alterations of tangential surfaces of wood samples (with dimensions 0.6 cm radial x 2 cm tangential x 6 cm longitudinal), that were impregnated with W.R. solutions (Treatments A, B, C,……, M) and were exposed in weather conditions, showed that in all cases tangential surface checks were observed in an axial direction parallel to the length of the samples. Of all the treatments studied, the smallest effect of the weather conditions was observed in treatment I with C.W.R. solutions (G: water repellent and H: varnish). At last in poplar specimens impregnated with polystyrene solutions (concentration 20%) a relatively low improvement of specimen compression resistance and shear strength (SRplane radial) were observed (9.7% and 2.32% respectively) but with much higher improvement in hardness (28.72%) and in screw with drawl (38.22%).

Degree

thesis:*
Grantor dc:publisher
Aristotle University Of Thessaloniki (AUTH)
Year dc:date
2013

Author and committee

dc:creator, dc:contributor.*
Authors dc:creator
  • Foti, Dafni
  • Φώτη, Δάφνη

Subjects

dc:subject × 16

Rights

Language dc:language
gre

Identifiers

dc:identifier.*
Identifier
10.12681/eadd/29064

Chain of custody

source
Harvested from
Greek National Archive of PhD Theses
Base URL
phdtheses.ekt.gr/eadd_oai/request
Last updated
2026-11-18
Source record
OAI-PMH GetRecord
citation

Foti, Dafni; Φώτη, Δάφνη. Βελτίωση των ιδιοτήτων του ξύλου με ανακυκλώμενο πολυστυρένιο. Aristotle University Of Thessaloniki (AUTH), 2013. http://hdl.handle.net/10442/hedi/29064