Back to search

University of Thessaly (UTH)

Προοπτική συγκριτική μελέτη της φθοράς της αρθρούμενης - κινούμενης επιφάνειας από οξειδωμένο ζιρκόνιο (Oxinium) με διασταυρούμενο πολυαιθυλένιο στις ολικές αρθροπλαστικές ισχίου

Abstract

dc:description

Osteolysis resulting from wear debris is a major factor limiting long term survival of hip implants. Oxidized zirconium head (OxiniumTM) on crosslinked polyethylene (XLPE) is a modern bearing coupling, introduced to reduce wear debris. However several issues require further investigation: Does this bearing couple produce less wear debris than the combination of ceramic head on XLPE or conventional polyethylene (CPE)? What bearing couple has better clinical performance? A total of 199 patients who underwent total hip replacement for osteoarthtritis were evaluated clinically and radiologically, with a follow-up of 12- 16 years, by measuring in vivo, linear wear, linear wear rate, volumetric wear and volumetric wear rate by using PolyWare® software. All bearing couples showed a varying high bedding-in effect (plastic deformation of the liner) up to the second postoperative year. In this study, in vivo wear parameters were lower when the combination of OxiniumTM head on XLPE was used, at 5 and 10 years. Interestingly, wear parameters were higher than other bearing couples when the combination of CPE on XLPE was used and this seems to be related to the specific implants we used. Additionally, our study showed that both OxiniumTM heads (28 & 32 mm) presented equally low wear debris production, with no statistically significant difference between them. There was no differences between groups concerning clinical scores at final followup, while two patients (from ceramic head groups) are scheduled for revision operation as a result of osteolysis. Further larger-scale clinical studies should confirm these findings and evaluate osteolysis and revision rates in association with the use of this bearing coupling.

Degree

thesis:*
Grantor dc:publisher
University of Thessaly (UTH)
Year dc:date
2019

Author and committee

dc:creator, dc:contributor.*
Authors dc:creator
  • Karidakis, Georgios
  • Καρυδάκης, Γεώργιος

Subjects

dc:subject × 8

Rights

Language dc:language
gre

Identifiers

dc:identifier.*
Identifier
10.12681/eadd/45601

Chain of custody

source
Harvested from
Greek National Archive of PhD Theses
Base URL
phdtheses.ekt.gr/eadd_oai/request
Last updated
2026-11-18
Source record
OAI-PMH GetRecord
citation

Karidakis, Georgios; Καρυδάκης, Γεώργιος. Προοπτική συγκριτική μελέτη της φθοράς της αρθρούμενης - κινούμενης επιφάνειας από οξειδωμένο ζιρκόνιο (Oxinium) με διασταυρούμενο πολυαιθυλένιο στις ολικές αρθροπλαστικές ισχίου. University of Thessaly (UTH), 2019. http://hdl.handle.net/10442/hedi/45601