McMaster University
THE EFFECT OF H2SO4 SURFACE PRE-TREATMENT ON THE STRESS CORROSION CRACKING OF MAGNESIUM ALLOY AZ31B
Abstract
dc:description.abstractThe stress corrosion cracking (SCC) behaviour of Mg alloy AZ31B was investigated with respect to surface condition. Salt fog U-bend testing was used to identify changes in SCC as a result of surface conditioning pre-treatments. Six surface conditions were investigated: as-received, mechanically-polished, sulphuric acid (H2SO4)-cleaned, mechanically-polished then H2SO4-cleaned, aged H2SO4-cleaned, and acetic acid (C2H4O2)-cleaned. Results showed that the rate of SCC was accelerated and the SCC mode was intergranular for all surface conditioning treatments involving H2SO4-cleaning. It was found that the accelerated intergranular SCC was a result of three contributing factors: a low pH, the presence of aggressive ions, and a porous film which allowed direct contact between the metal surface and the electrolyte. Characterization of the surfaces using potentiodynamic polarization and cross-sectional images of sample surfaces showed that in the absence of one of these three contributing factors intergranular SCC would not occur.
Degree
thesis:*- Department dc:contributor.department
- Materials Science and Engineering
- Year dc:date.issued
- 2015
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Wilson, Brycklin
- Advisors dc:contributor.advisor
-
- Kish, Joseph
- McDermid, Joseph
Subjects
dc:subject × 2Rights
- Language dc:language.iso
- en
Identifiers
dc:identifier.*- Identifier URI
- https://doi.org/10.71548/22713