Spelling suggestions: "subject:"deslocalização"" "subject:"desmedicalização""
1 |
Craqueamento de hidrocarbonetos naftênicos sobre zeólitas HZSM-12 modificadas – rendimento e seletividade a olefinas levesSilva Júnior, José Roberto da 30 September 2015 (has links)
Submitted by Alison Vanceto (alison-vanceto@hotmail.com) on 2016-10-21T11:11:40Z
No. of bitstreams: 1
TeseJRSJ.pdf: 5314232 bytes, checksum: 9352e78958e9a2f45a12e9a77f564bdd (MD5) / Approved for entry into archive by Marina Freitas (marinapf@ufscar.br) on 2016-11-08T18:37:37Z (GMT) No. of bitstreams: 1
TeseJRSJ.pdf: 5314232 bytes, checksum: 9352e78958e9a2f45a12e9a77f564bdd (MD5) / Approved for entry into archive by Marina Freitas (marinapf@ufscar.br) on 2016-11-08T18:37:44Z (GMT) No. of bitstreams: 1
TeseJRSJ.pdf: 5314232 bytes, checksum: 9352e78958e9a2f45a12e9a77f564bdd (MD5) / Made available in DSpace on 2016-11-08T18:37:52Z (GMT). No. of bitstreams: 1
TeseJRSJ.pdf: 5314232 bytes, checksum: 9352e78958e9a2f45a12e9a77f564bdd (MD5)
Previous issue date: 2015-09-30 / Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES) / It was studied the catalytic performance of ZSM-12 zeolites modified by desilication in the
cracking of naphthenic hydrocarbons. ZSM-12 zeolites with nominal a SiO2/Al2O3 ratio were
synthesized during 96 or 144 h under hydrothermal conditions and the obtained zeolites were
treated with NaOH solutions under different conditions. The samples were characterized by
thermogravimetric analysis (TA), X-ray diffraction (XRD), scanning electron microscopy
(SEM), N2 physisorption, temperature programmed desorption of ammonia (NH3-TPD), 27Al
MAS NMR spectroscopy, energy-dispersive X-ray spectroscopy (EDX) and infrared
spectroscopy (Py-FTIR). The treatment with NaOH solutions under mild conditions was more
effective for the ZSM-12 zeolite synthesized during 96 h. For the HZ12-96-0,2 sample,
obtained by treatment at 35 °C with 0.2 mol.L-1 NaOH solution during 15 min, it was verified
an increase in the external surface area and the formation of mesopores in the range of 2 to 14
nm. On that zeolite occurred a higher yields to light olefins during the cracking of
cyclohexane at 400 °C and also in the cracking of methyl and ethylcyclohexane at 450 °C.
This result was mainly related to the higher density of acid sites exhibited by the HZ12-96-0,2
zeolite compared with the parent ZSM-12 one, as consequence of the applied alkaline
treatment. It was also verified that the ZSM-12 zeolites modified by more severe alkaline
treatment (0.5 or 1.0 mol.L-1 NaOH solution at 80 °C for 30 min) presented significant
increase of the external surface area and mesopores volume. The catalytic cracking of
cyclohexane, methylcyclohexane and ethylcyclohexane at 500 °C, as well as the physicochemical
characteristics of the MZ12-96-0,5 zeolite enhanced the formation of light olefins.
The highest yield to light olefins was obtained on that zeolite during the cracking of
ethylcyclohexane, which increased 9% when compared with the yield obtained on the not
modified HZSM-12 zeolite. The selectivity to light olefins on the studied HZSM-12 zeolites
was strongly influenced by presence of a side chain in the naphthenic ring (methyl or ethyl),
as well as by the employed cracking operating conditions. / Estudou-se o desempenho de zeólitas ZSM-12 modificadas por dessilicalização no
craqueamento de hidrocarbonetos naftênicos. Zeólitas ZSM-12 com razão SiO2/Al2O3 igual a
80 foram sintetizadas em 96 ou 144 h sob condições hidrotérmicas. As zeólitas ZSM-12
obtidas foram modificadas sob diferentes condições de tratamento alcalino com soluções de
NaOH e posteriormente caracterizadas por termogravimetria, difratometria de raios X,
microscopia eletrônica de varredura, fisissorção de nitrogênio, dessorção de amônia à
temperatura programada, ressonância magnética nuclear do 27Al, espectroscopia de energia
dispersiva de raios X e espectroscopia na região do infravermelho com adsorção de piridina.
O tratamento alcalino, sob condições mais brandas, foi mais efetivo para a zeólita ZSM-12
sintetizada em menor tempo de cristalização (96 h). Para a zeólita HZ12-96-0,2, obtida por
tratamento com solução de NaOH 0,2 mol.L-1 a 35 °C por 15 min, verificou-se um aumento
na área superficial externa e distribuição de tamanho de mesoporos entre 2 e 14 nm. Nessa
zeólita, ocorreu um maior rendimento a olefinas leves no craqueamento de cicloexano a 400
°C e, também, no craqueamento de metil- e etil-cicloexano realizado a 450 °C. Esse resultado
foi relacionado, principalmente, com a maior concentração de sítios ácidos na zeólita HZ12-
96-0,2, em relação à zeólita HZSM-12 precursora, como consequência do tratamento alcalino.
Verificou-se, também, que as zeólitas ZSM-12 modificadas por tratamento alcalino, sob
condições mais severas (solução de NaOH 0,5 ou 1,0 mol.L-1
a 80 °C por 30 min), apresentaram
aumento significativo de área superficial externa e volume de mesoporos. O craqueamento de
cicloexano, metil- e etil-cicloexano realizado a 500 °C, assim como as características físicas e
químicas da zeólita MZ12-96-0,5, favoreceram a formação de olefinas leves. O maior
rendimento a olefinas leves ocorreu durante o craqueamento do etil-cicloexano sobre essa
zeólita, com aumento desse rendimento em torno de 9% quando comparado ao rendimento
obtido sobre a zeólita HZSM-12 não modificada. A seletividade a olefinas leves sobre as
zeólitas HZSM-12 preparadas neste estudo sofreu forte influência da presença da cadeia
lateral no anel naftênico (metil ou etil), assim como também das condições operacionais de
craqueamento empregadas.
|
2 |
Propriedades ácidas e texturais de zeólitas ZSM-5 dessilicalizadas ou desaluminizadas – análise do rendimento e seletividade a olefinas leves durante a transformação de cicloexano e metilcicloexanoDarim, Hélio Rubens Abdo 13 March 2015 (has links)
Submitted by Alison Vanceto (alison-vanceto@hotmail.com) on 2017-02-09T10:54:21Z
No. of bitstreams: 1
DissHRAD.pdf: 15161052 bytes, checksum: e10c4924acc9cc8afc5ecbec12ee85aa (MD5) / Approved for entry into archive by Ronildo Prado (ronisp@ufscar.br) on 2017-03-20T17:16:45Z (GMT) No. of bitstreams: 1
DissHRAD.pdf: 15161052 bytes, checksum: e10c4924acc9cc8afc5ecbec12ee85aa (MD5) / Approved for entry into archive by Ronildo Prado (ronisp@ufscar.br) on 2017-03-20T17:16:55Z (GMT) No. of bitstreams: 1
DissHRAD.pdf: 15161052 bytes, checksum: e10c4924acc9cc8afc5ecbec12ee85aa (MD5) / Made available in DSpace on 2017-03-20T17:24:11Z (GMT). No. of bitstreams: 1
DissHRAD.pdf: 15161052 bytes, checksum: e10c4924acc9cc8afc5ecbec12ee85aa (MD5)
Previous issue date: 2015-03-13 / Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq) / Nowadays, the Brazilian petroleum is extracted from very deep fields and possesses a high
naphthenic hydrocarbons composition, which imposes new challenges to refineries and
specially to the catalytic cracking process. In that process, the catalyst must act maximizing
the production of the highly demanded gasoline, diesel and light olefins from heavy fractions.
Taking into consideration the above discussed context, this work aimed to evaluate the effect
of basic or acid treatments applied on ZSM-5 zeolites (Si/Al=12 or 23) in the activity to
cyclohexane or methylcyclohexane transformation. XRD and 27Al-NMR showed that the dealuminated zeolites presented an increase in their crystallinity due to the extra-framework
aluminum lixiviation. On the other hand, in the desilicated zeolites occurred a decrease in
their crystallinity as a consequence of the extra-framework aluminum generation. MEV
images do not evidence any morphological change that could have been produced by the acid or basic treatments, however, the desilicated ZSM-5 zeolites treated under harder conditions
presented significant textural modifications. As expected, the chemical ICP analyses showed a
decrease in the Si/Al ratio in the desilicated zeolites and an increase of that ratio for those
dealuminated ones, being the last variation more significative in the external surface of the
zeolite crystals, as was evidenced by XPS analyses. Data from NH3-TPD showed that the
acid treatment resulted in a higher ratio of strong acid sites, which suffered more deactivation
during reaction. N2 fisisorption analyses of the ZSM-5 zeolites, showed that the desilication
done at higher temperature was more efficient to mesopore generation. In the cyclohexane
and methylcyclohexane transformation, the dealuminated zeolites were less active due to their lower aluminum content, nevertheless were more stable and presented a small increase to
light olefins selectivity. The desilicated ZSM-5 zeolites presented higher activity and higher
yield to light olefins that were supported by their lower Si/Al ratio and mainly by the presence
of mesoporosity that enhanced the reagents and products internal diffusivity. / A produção nacional de petróleo, extraído de jazidas cada vez mais profundas, possui um
elevado teor de hidrocarbonetos naftênicos, o que impõe novos desafios às refinarias
brasileiras e, em particular, ao processo de craqueamento catalítico. Nesse processo, o
catalisador deve maximizar a transformação das frações pesadas em produtos de alta demanda
como gasolina, diesel e olefinas leves. Nesse contexto, esta dissertação objetivou avaliar o
efeito de tratamentos de lixiviação ácida ou básica em zeólitas ZSM-5 (Si/Al=12 ou 23), na
atividade para a transformação de cicloexano ou metilcicloexano. Dados de DRX e 27Al-RMN
mostraram que as zeólitas desaluminizadas apresentaram um aumento da sua cristalinidade
devido à remoção de átomos de alumínio extra-rede, por outro lado, nas zeólitas
dessilicalizadas ocorreu uma redução da cristalinidade devido à geração de alumínio extra rede. As micrografias de MEV não evidenciaram modificação morfológica devido aos
tratamentos, entretanto nas amostras dessilicalizadas sob condições mais severas, houve significativa mudança das propriedades texturais. Como esperado, as análises químicas por ICP mostraram uma redução na razão Si/Al para as amostras dessilicalizadas e um aumento
dessa razão para as zeólitas desaluminizadas, sendo essa variação mais significativa na
superfície externa dos cristais, como mostraram resultados de XPS. As análises de DTP-NH3
mostraram que o tratamento ácido resultou numa maior proporção de sítios ácidos fortes, os
quais sofreram maior desativação durante a reação. Dados de fisissorção de N2 das zeólitas
mostraram que a dessilicalização em temperatura mais elevada foi mais eficiente na geração de mesoporos. Na transformação do cicloexano e do metilcicloexano, as zeólitas
desaluminizadas apresentaram menor conversão como resultado da diminuição do teor de
alumínio, entretanto tiveram maior estabilidade e apresentaram um ligeiro aumento na
seletividade a olefinas leves. As amostras dessilicalizadas apresentaram maiores conversões e rendimentos a olefinas leves, que se justificaram em função da diminuição da razão Si/Al, mas principalmente, como resultado da presença de mesoporosidade, que melhorou a difusão interna de reagentes e produtos.
|
3 |
Desenvolvimento de materiais híbridos micro-mesoporosos do tipo ZSM-12/MCM-MCM-41 para utilização no craqueamento de frações de petróleoSantana, Joselaine Carvalho 27 June 2014 (has links)
The development of micro-mesoporous hybrid aims to obtain materials with improved characteristics, since it tries to bring together to high acidity and thermal and hydrothermal stability of zeolites, with larger pore system and consequently better chance of diffusion of molecules within the mesoporous materials. Micro-mesoporous hybrid materials of ZSM-12/MCM-41 type with different micro and mesoporosity contributions were prepared by a procedure that uses the desilicalization of the zeolite in an alkaline medium, followed by recrystallization on the mesostructure, where the zeolite is used as the silica source in the formation of mesoporous phase. The ZSM-12 pure zeolite and MCM-41 pure were also prepared. The materials were characterized by X-ray diffraction, nitrogen adsorption-desorption at 77 K, scanning electron microscopy, infrared absorption spectroscopy and thermal analysis. The catalytic activity of these was analyzed in the catalytic cracking of cumene. The results shown that the methodology utilized is efficient to obtain hybrid materials of ZSM-12/MCM-41 type with micro-and mesoporosity optimized, and catalytic tests showed that the hybrid have the potential for cracking reactions, showing better results than the pure materials, pointing to it, the existing synergistic effect in these. / O desenvolvimento de híbridos micro-mesoporosos visa a obtenção de materiais com características melhoradas, uma vez que busca unir a elevada acidez e estabilidade térmica e hidrotérmica das zeólitas, com o maior sistema de poros e consequentemente melhor possibilidade de difusão de moléculas dos materiais mesoporosos. Materiais híbridos micro-mesoporosos do tipo ZSM-12/MCM-41 com diferentes contribuições de micro e mesoporosidade foram preparados por meio de um procedimento que se utiliza da dessilicalização de zeólitas em meio alcalino, seguida de recristalização em mesoestrutura, onde a zeólita é utilizada como fonte de sílica na formação da fase mesoporosa. A zeólita ZSM-12 pura e o MCM-41 puro também foram preparados. Os materiais foram caracterizados por difratometria de raios-X, adsorção-desorção de nitrogênio a 77 K, microscopia eletrônica de varredura, espectroscopia de absorção na região do infravermelho e análise termogravimétrica. A atividade catalítica destes foi analisada no craqueamento catalítico do cumeno. Os resultados obtidos através das técnicas de caracterização mostraram que a metodologia utilizada é eficiente para a obtenção de materiais híbridos do tipo ZSM-12/MCM-41 com contribuição de micro e mesoporosidade otimizadas, e os testes catalíticos mostraram que os híbridos têm potencial em reações de craqueamento, apresentando melhores resultados que os materiais puros, evidenciando com isso, o efeito sinérgico existente nestes.
|