Back to search

The Ohio State University

Chromium-free consumable for welding stainless steel: corrosion perspective

Abstract

dc:description

Arc welding of stainless steels generates welding fumes containing carcinogenic hexavalent chromium. To mitigate this problem, a Cr-free filler metal needs to be developed to reduce the health risks for welding stainless steel. Ni-Cu alloy, Monel K400, was selected initially based on its galvanic compatibility with types 304 and 316 SS in chloride environments Type 304L (UNS S30403) stainless steel plate was successfully welded with Monel filler wire, resulting in high quality welds with no cracks. The welds survived long term exposure in 0.1 M NaCl with no evidence of corrosion. However, segregated regions in weld that are rich in Cu are the weak spots for corrosion susceptibility. The effects of alloying elements on the corrosion properties of Ni-Cu alloy were investigated to optimize the composition of a Cr-free consumable for welding of stainless steels. Cyclic polarization experiments were performed in 0.1 M NaCl on Ni-base alloys containing different amounts of Cu, Pd, Mo, Fe, and Cr. The localized corrosion behavior improved as the Cu content decreased from 30 to 5 wt%. The addition of 1 wt% Pd ennobled the alloy and greatly improved the localized corrosion properties. The optimized composition is a Ni-based alloy containing 5-10 wt% Cu and 1 wt% Pd. Ni-10Cu-1Pd alloy across the entire dilution range exhibited higher repassivation potential than Type 304L stainless steel in 0.1 M NaCl solution. The repassivation potential was also higher in aerated solutions with chloride concentrations of 105 through 35000 ppm. The breakdown behavior of Bead-On-Plate weld was similar to that of Type 308L welds. After 31 days exposure of samples with crevice-formers in 500 and 1000 ppm chloride solutions, the Bead-On-Plate weld showed much shallower attack than the 308L weld. The passive film on Ni-10Cu-1Pd alloy mainly consisted of outer Ni-hydroxide and inner oxide, but the noble elements of Pd and Cu did not contribute to the formation of the passive film. However, Pd catalyzed the reduction of Cu at the bottom of the artificial pit, which enhanced the cathodic reaction and thus ennobled the deactivation potential making stable pit growth more difficult.

Degree

thesis:*
Name thesis:degree_name
Doctor of Philosophy
Level thesis:degree_level
doctoral
Discipline thesis:degree_discipline
Materials Science and Engineering
Grantor dc:publisher
The Ohio State University
Year dc:date
2005

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Kim, Yeong Ho
Advisor dc:contributor.advisor
  • Frankel, Gerald

Subjects

dc:subject × 17

Rights

dc:rights
Statement dc:rights
  • unrestricted
  • This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
Language dc:language
English

Identifiers

dc:identifier.*

Chain of custody

source
Harvested from
OhioLINK
Base URL
etd.ohiolink.edu/acprod/odb_etd/ws/oai/oai
Last updated
2026-11-27
Source record
OAI-PMH GetRecord
citation

Kim, Yeong Ho. Chromium-free consumable for welding stainless steel: corrosion perspective. doctoral thesis, The Ohio State University, 2005. http://rave.ohiolink.edu/etdc/view?acc_num=osu1133285376