• Refine Query
  • Source
  • Publication year
  • to
  • Language
  • 36
  • 6
  • 6
  • 6
  • 6
  • 6
  • Tagged with
  • 36
  • 36
  • 34
  • 33
  • 28
  • 27
  • 27
  • 15
  • 15
  • 11
  • 9
  • 9
  • 9
  • 8
  • 6
  • About
  • The Global ETD Search service is a free service for researchers to find electronic theses and dissertations. This service is provided by the Networked Digital Library of Theses and Dissertations.
    Our metadata is collected from universities around the world. If you manage a university/consortium/country archive and want to be added, details can be found on the NDLTD website.
31

Resistência à fratura de diferentes núcleos de preenchimento com compósitos bulk fill em dentes com extensa destruição coronária /

Oliveira, Carlos Rangel de Moura January 2019 (has links)
Orientador: José Maurício dos Santos Nunes Reis / Resumo: Este estudo objetivou avaliar a resistência máxima e o padrão de fratura de diferentestécnicas para núcleo preenchimento associados a pinos de fibra de vidro em incisivoslaterais inferiores bovinos com extensa destruição coronária. Quarenta dentes forampreparados endodonticamente, divididos aleatoriamente em 4 grupos experimentais(n=10) e um pino de fibra de vidro (Whitepost DC0,5) foi cimentado com LuxaCore Zpara todos os grupos. A confecção dos núcleos de preenchimento foi realizada, apósobtenção de férula cervical de 1,0 mm, com: FOBF-Filtek One Bulk Fill; FZ350- FiltekZ350 XT; FBFF-Filtek Bulk Fill Flow; e LCZ-LuxaCore Z. Coroas totais de zircônia (YTZP) produzidas em CAD/CAM foram cimentadas com RelyX U200. Apósarmazenamento em água destilada a 37°C por 48 h, os corpos-de-prova foramsubmetidos a ciclos térmicos (10.000 ciclos, 5-55ºC, banhos de 30s) e, posteriormente,ao ensaio mecânico de resistência à fratura por força compressiva aplicada (1,0mm/min) em 135º ao longo eixo do dente em máquina eletromecânica (EMIC DL2000).A força máxima suportada por cada espécime foi registrada em Newton. O modo defratura foi classificado por meio de análise em lupa estereomicroscópica (30X). Osdados de resistência à fratura foram analisados pelo teste não paramétrico de KruskalWallis, seguido pelo post-hoc teste de Dunn. Os dados dos padrões de fratura foramanalisados pelo teste exato de Fisher (α=0,05). Não foram observadas diferençassignificativas (p>0... (Resumo completo, clicar acesso eletrônico abaixo) / Abstract: This study aimed to evaluate the ultimate fracture strength and failure modes of different core techniques associated with intraradicular fiberpost in bovine mandibular lateral incisors with extensive coronary destruction. Forty teeth were prepared endodontically, randomly divided into 4 experimental groups (n=10) and a fiberpost (Whitepost DC0.5) was cemented with LuxaCore Z for all groups. The core was confeccioned, after obtaining a 1.0 mm cervical ferrule, with: FOBF-Filtek One Bulk Fill; FZ350- Filtek Z350 XT; FBFF-Filtek Bulk Fill Flow; and LCZ-LuxaCore Z. Total zirconia crowns (Y-TZP) produced by CAD/CAM were cemented with RelyX U200. After storage in distilled water at 37ºC for 48 h, the specimens were submitted to thermal cycling (10,000 cycles, 5- 55ºC, 30 s dwell time) and, afterwards, to the mechanical test of compressive strength fracture (1.0 mm / min) at 135º along the tooth axis in electromechanical machine (EMIC DL2000). The ultimate load supported by each specimen was recorded in Newton. The fracture mode was classified by means of stereomicroscopic loupe analysis (30X). The fracture strength data were analyzed by the non-parametric Kruskal-Wallis test, followed by the post-hoc Dunn test. The data of the fracture modes were analyzed by Fisher's exact test (α=0.05). No significant differences (p>0.05) were observed among the FOBF, FZ350 and FBFF groups (mean ranks= 20.30, 12.20 and 23.20, respectively). LCZ (mean rank= 26.30) produced similar results to those... (Complete abstract click electronic access below) / Mestre
32

Avaliação da customização por desgaste de pinos pré-fabricados de fibra de vidro / Evaluation of fibre posts submitted to customization of the apical portion

Ana Regina Cervantes Dias 25 January 2012 (has links)
O objetivo deste estudo foi avaliar pinos pré-fabricados de fibra de vidro (White Post DC/FGM) submetidos à customização por desgaste da porção apical. Experimento 1: 5 pinos n. 4 foram divididos em 5 grupos (G) de acordo com o instrumento de desgaste: GA - sem desgaste, GB- mini torno industrial (Dentsply), GC - ponta diamantada n. 3195F (KG Sorensen), GD - disco de lixa de granulação média (Sof-Lex/3M/ESPE), GE- alicate (Tramontina). Observou-se a micromorfologia dos pinos em microscópio eletrônico de varredura (ZEISS/DSM 960). Experimento 2: 60 pinos de diferentes diâmetros foram divididos em 6 grupos: G0 - pinos n. 0,5, G1 - pinos n. 1, G2 - pinos n. 2, G3 - pinos n. 3, G4 - pinos n.4, G5 - pinos n. 4 com terço apical desgastado com discos de lixa até o equivalente ao terço apical dos pinos n. 2. Os pinos foram submetidos ao teste de flexão de 3 pontos na máquina de ensaios universal (Instron 5500 R), conforme ISO 10477. Experimento 3: 20 caninos humanos permanentes sofreram tratamento endodôntico e remoção das coroas clínicas padronizando 15 mm de remanescente radicular. Os dentes foram incluídos em resina acrílica com simulação do ligamento periodontal, receberam férula de 2 mm e foram divididos em 2 grupos: GI - pinos n. 4 cimentados em condutos preparados com broca equivalente ao pino (FGM), GII - pinos n. 4 customizados no terço apical cimentados em condutos preparados com brocas (FGM) equivalentes aos pinos n. 2 em 10 mm e n. 4 em 5 mm. Os pinos foram cimentados com cimento resinoso (Rely X U100/3M/ESPE), os corpos de prova receberam coroas diretas de resina composta (Enforce Core/Dentsply) padronizadas com coras de policarbonato (TDV) e foram submetidos ao teste de resistência à fratura na Instron a 45da ferramenta cilíndrica, com força de 500 N aplicada a 2 mm da incisal na face palatina/lingual, com velocidade de 0,5 mm/min até falha. O padrão de fratura foi classificado em favorável ou desfavorável. Os resultados foram tratados estatisticamente por teste de análise de variância (ANOVA, p<0,05). Os resultados dos testes de flexão e fratura foram respectivamente: G0 - 58,406,40; G1 - 83,959,43; G2- 103,4219,17; G3 - 160,7817,30; G4 - 170,4711,28; G5 - 106,3521,96; GI - 303,0262,21 e GII - 402,81131,97. O padrão de fratura foi tratado por Mann-Whitney que observou semelhança estatística entre os grupos. Concluiu-se que o desgaste de pinos de fibra de vidro com pontas diamantadas ou discos de lixa produz alterações micromorfológicas aceitáveis. O corte com alicate deve ser evitado. A customização por desgaste da porção apical de pinos de fibra de vidro diminui a resistência à flexão a valores aceitáveis. Dentes restaurados com pinos de fibra de vidro customizados por desgaste possuem resistência à fratura superior a dentes restaurados com pinos intactos. A customização por desgaste facilita a adaptação do pino ao conduto radicular e preserva a estrutura dental. / The purpose of this study was to evaluate fibre posts (White Post DC/FGM) submitted to customization of the apical portion. Experiment 1: 5 #4 posts were divided into five groups (G) and submitted to different custom adaptation treatments: GA no surface treatment, GB- industrial shaping tool (Dentsply), GC- #3195 fine diamond bur (KG Sorensen), GD- medium-grain paper discs (Sof-Lex/3M/ESPE), GE pliers (Tramontina). The micromorphology of the posts was observed in a scanning electron microscope (ZEISS/DSM 960). Experiment 2: 60 posts of different diameters were divided into six groups: G0 #0.5 posts, G1 #1 posts, G2 #2 posts, G3 - #3 posts; G4 - #4 posts and G5 #4 posts submitted to custom adaptation of the apical portion with paper discs until the diameter was equivalent to #2 posts. The posts were submitted to a 3 point bending test in a universal testing machine (Instron/5500 R), according to ISO 10477. Experiment 3: 20 freshly extracted permanent healthy human canines with similar size were endodontically treated and the crowns were removed, leaving a remaining root length of 15 mm. The teeth were embedded in acrylic resin with simulation of the periodontal ligament, received a 2 mm ferule and were divided into two groups: G1- 10 #4 posts were cemented into post spaces prepared with #4 drill (FGM) at 10 mm, G2 - 10 #4 customized posts were cemented into root spaces prepared with #2 drill (FGM) at 10 mm and #4 drill (FGM) at 5 mm. The posts were cemented with resin cement (Rely X U100/3M/ESPE), and the teeth received direct crowns of composite resin (Enforce Core/Dentsply), standardized with polycarbonate crowns (TDV). The fracture strength was measured on an Instron, at 45 degrees to the long axis of the tooth, until fracture. The 500 N cylindrical load was applied to the buccal/lingual axis 2 mm below the incisal line, at crosshead speed of 0.5 mm/min. The fracture pattern was observed and classified as favorable or unfavorable. The results were submitted to ANOVA (p<0.05). Flexural strength and resistance to fracture data were, respectively: G0 58.40+6.40; G1 83.95+9.43; G2 103.42+19.17; G3 160.78+17.30; G4- 170.47+11.28; G5 106.35+21.96;GI 303.02+62.21 and GII 402.81+131.97. Fracture patterns were statistically similar according to Mann-Whitney test. It was concluded that customization of fibre posts with diamond burs or paper discs produces acceptable micromorphological changes. The cut of the post with pliers should be avoided. Grounding of the apical portion of fibre posts reduces the flexural strength to acceptable values. Teeth restored with grounded fiber posts have grater fracture strength than teeth restored with intact posts. Grounding of the post facilitates adaptation to root walls and preserves tooth structure.
33

Avaliação da customização por desgaste de pinos pré-fabricados de fibra de vidro / Evaluation of fibre posts submitted to customization of the apical portion

Ana Regina Cervantes Dias 25 January 2012 (has links)
O objetivo deste estudo foi avaliar pinos pré-fabricados de fibra de vidro (White Post DC/FGM) submetidos à customização por desgaste da porção apical. Experimento 1: 5 pinos n. 4 foram divididos em 5 grupos (G) de acordo com o instrumento de desgaste: GA - sem desgaste, GB- mini torno industrial (Dentsply), GC - ponta diamantada n. 3195F (KG Sorensen), GD - disco de lixa de granulação média (Sof-Lex/3M/ESPE), GE- alicate (Tramontina). Observou-se a micromorfologia dos pinos em microscópio eletrônico de varredura (ZEISS/DSM 960). Experimento 2: 60 pinos de diferentes diâmetros foram divididos em 6 grupos: G0 - pinos n. 0,5, G1 - pinos n. 1, G2 - pinos n. 2, G3 - pinos n. 3, G4 - pinos n.4, G5 - pinos n. 4 com terço apical desgastado com discos de lixa até o equivalente ao terço apical dos pinos n. 2. Os pinos foram submetidos ao teste de flexão de 3 pontos na máquina de ensaios universal (Instron 5500 R), conforme ISO 10477. Experimento 3: 20 caninos humanos permanentes sofreram tratamento endodôntico e remoção das coroas clínicas padronizando 15 mm de remanescente radicular. Os dentes foram incluídos em resina acrílica com simulação do ligamento periodontal, receberam férula de 2 mm e foram divididos em 2 grupos: GI - pinos n. 4 cimentados em condutos preparados com broca equivalente ao pino (FGM), GII - pinos n. 4 customizados no terço apical cimentados em condutos preparados com brocas (FGM) equivalentes aos pinos n. 2 em 10 mm e n. 4 em 5 mm. Os pinos foram cimentados com cimento resinoso (Rely X U100/3M/ESPE), os corpos de prova receberam coroas diretas de resina composta (Enforce Core/Dentsply) padronizadas com coras de policarbonato (TDV) e foram submetidos ao teste de resistência à fratura na Instron a 45da ferramenta cilíndrica, com força de 500 N aplicada a 2 mm da incisal na face palatina/lingual, com velocidade de 0,5 mm/min até falha. O padrão de fratura foi classificado em favorável ou desfavorável. Os resultados foram tratados estatisticamente por teste de análise de variância (ANOVA, p<0,05). Os resultados dos testes de flexão e fratura foram respectivamente: G0 - 58,406,40; G1 - 83,959,43; G2- 103,4219,17; G3 - 160,7817,30; G4 - 170,4711,28; G5 - 106,3521,96; GI - 303,0262,21 e GII - 402,81131,97. O padrão de fratura foi tratado por Mann-Whitney que observou semelhança estatística entre os grupos. Concluiu-se que o desgaste de pinos de fibra de vidro com pontas diamantadas ou discos de lixa produz alterações micromorfológicas aceitáveis. O corte com alicate deve ser evitado. A customização por desgaste da porção apical de pinos de fibra de vidro diminui a resistência à flexão a valores aceitáveis. Dentes restaurados com pinos de fibra de vidro customizados por desgaste possuem resistência à fratura superior a dentes restaurados com pinos intactos. A customização por desgaste facilita a adaptação do pino ao conduto radicular e preserva a estrutura dental. / The purpose of this study was to evaluate fibre posts (White Post DC/FGM) submitted to customization of the apical portion. Experiment 1: 5 #4 posts were divided into five groups (G) and submitted to different custom adaptation treatments: GA no surface treatment, GB- industrial shaping tool (Dentsply), GC- #3195 fine diamond bur (KG Sorensen), GD- medium-grain paper discs (Sof-Lex/3M/ESPE), GE pliers (Tramontina). The micromorphology of the posts was observed in a scanning electron microscope (ZEISS/DSM 960). Experiment 2: 60 posts of different diameters were divided into six groups: G0 #0.5 posts, G1 #1 posts, G2 #2 posts, G3 - #3 posts; G4 - #4 posts and G5 #4 posts submitted to custom adaptation of the apical portion with paper discs until the diameter was equivalent to #2 posts. The posts were submitted to a 3 point bending test in a universal testing machine (Instron/5500 R), according to ISO 10477. Experiment 3: 20 freshly extracted permanent healthy human canines with similar size were endodontically treated and the crowns were removed, leaving a remaining root length of 15 mm. The teeth were embedded in acrylic resin with simulation of the periodontal ligament, received a 2 mm ferule and were divided into two groups: G1- 10 #4 posts were cemented into post spaces prepared with #4 drill (FGM) at 10 mm, G2 - 10 #4 customized posts were cemented into root spaces prepared with #2 drill (FGM) at 10 mm and #4 drill (FGM) at 5 mm. The posts were cemented with resin cement (Rely X U100/3M/ESPE), and the teeth received direct crowns of composite resin (Enforce Core/Dentsply), standardized with polycarbonate crowns (TDV). The fracture strength was measured on an Instron, at 45 degrees to the long axis of the tooth, until fracture. The 500 N cylindrical load was applied to the buccal/lingual axis 2 mm below the incisal line, at crosshead speed of 0.5 mm/min. The fracture pattern was observed and classified as favorable or unfavorable. The results were submitted to ANOVA (p<0.05). Flexural strength and resistance to fracture data were, respectively: G0 58.40+6.40; G1 83.95+9.43; G2 103.42+19.17; G3 160.78+17.30; G4- 170.47+11.28; G5 106.35+21.96;GI 303.02+62.21 and GII 402.81+131.97. Fracture patterns were statistically similar according to Mann-Whitney test. It was concluded that customization of fibre posts with diamond burs or paper discs produces acceptable micromorphological changes. The cut of the post with pliers should be avoided. Grounding of the apical portion of fibre posts reduces the flexural strength to acceptable values. Teeth restored with grounded fiber posts have grater fracture strength than teeth restored with intact posts. Grounding of the post facilitates adaptation to root walls and preserves tooth structure.
34

Biodinamica restauradora de dentes tratados endodonticamente : analise por elementos finitos / Restorative biomechanical of endodontic treated teeth : finite element analysis

Santos Filho, Paulo Cesar de Freitas 04 June 2009 (has links)
Orientador: Luis Roberto Marcondes Martins / Tese (doutorado) - Universidade Estadual de Campinas, Faculdade de Odontologia de Piracicaba / Made available in DSpace on 2018-08-13T11:40:25Z (GMT). No. of bitstreams: 1 SantosFilho_PauloCesardeFreitas_D.pdf: 10660151 bytes, checksum: bd3f67697b369623400074dcf22ec01c (MD5) Previous issue date: 2009 / Resumo: O objetivo deste estudo foi desenvolver protocolo de modelagem tridimensional para incisivo central superior com aplicabilidade ao método de elementos finitos e avaliar o comportamento biomecânico de incisivo superior tratado endodonticamente e restaurado com retentores e coroa cerâmica por meio de análise por elementos finitos comparado ao dente hígido. Para geração do modelo 3D foi selecionado incisivo central superior hígido. Esmalte e dentina foram degradados em diferentes fases com ácido clorídrico-10%, e mapeados com scanner de contato 3D (Modela, Roland). Para o mapeamento do volume pulpar, a dentina foi seccionada longitudinalmente no sentido mesio-distal e realizado o escaneamento do espaço negativo referente à polpa. Os arquivos *.STL foram exportados para programa Bio-CAD (Rhinoceros-3D). Volumes de cada estrutura dental e técnicas restauradoras foram gerados por meio da associação de superfícies NURBS. Os modelos foram exportados para o programa de elementos finitos (FEMAP-NeiNastran), onde foi realizado o processo de malhagem, inserção das propriedades mecânicas e condições de contorno. Foram gerados 17 modelos, sendo um do dente hígido e 16 modelos de acordo com os 4 fatores em estudo: tipo de retentor em dois níveis: pino de fibra de vidro (PFV) e núcleo moldado fundido (NMF), extensão do retentor em dois níveis: 7,0mm (7,0) e 12,0mm (12,0), remanescente coronário em dois níveis: remanescente de 2,0mm (RE) e ausência de remanescente (ARE), enfraquecimento do canal radicular em dois níveis: ausência de enfraquecimento (AENF) e presença de enfraquecimento (ENF). Foi simulada aplicação de pressão constante no valor de 100N perpendicularmente à superfície palatina do incisivo. Os resultados foram analisados pelo critério de von Mises e tensão máxima principal. Os resultados obtidos mostraram que o modelo geométrico 3D desenvolvido é adequado para a análise por elementos finitos. Concluiu-se que o PFV apresenta distribuição homogênea das tensões mais semelhante ao dente hígido, enquanto o NMF apresentou grande concentração de tensão no interior do canal radicular. O fator extensão do retentor intra-radicular influenciou isoladamente apenas a distribuição de tensões do NMF. A presença de remanescente coronário sempre melhorou a distribuição de tensões. O enfraquecimento do canal radicular teve maior impacto na distribuição de tensões. / Abstract: The aim of this study was develop 3D model generation protocol for upper anterior teeth for finite element analysis and evaluate biomechanical behavior of endodontically treated incisor with finite element analysis compared to sound teeth. It was selected intact upper central incisor. Enamel and dentin were treated in different steps with cloridric acid 2% and scanned with 3D-contact scanner. The stereolithographics archives were exported to Bio CAD program. The volums of each dental structure and restorative techniques were generated by association of NURBS surfaces. The models were exported for finite element software, where were realized the meshed process, mechanical properties insertion and bondary conditions. It were generated 17 models, one was a sound incisor model and 16 models according to 4 studied factors: post type: glass fiber post (GFP) and cast post and core (CPC), post length: 7,0mm (7,0) e 12,0mm (12,0), ferrule: 2,0mm ferrule (FE) and absence of ferrule (AFE), weakness of root canal: absence of weakness (AWR) and weakened root (WR). It was simulated 100N loading application on the palatal surface with 135° angulation. The results were analised by Von Mises criteria and principal maximum tension. Obtained results showed that geometric model developed is appropriated for finite element analysis. It can be concluded that GFP showed homogeneous stress distribution like the sound incisor, while CPC showed stress concentration into root canal. The post length influenced only the CPC stress distribution. The ferrule always showed better stress distribution. The weakness of root showed the highest impact in stress distribution. / Doutorado / Dentística / Doutor em Clínica Odontológica
35

Efeito do tipo de pino, altura do remanescente coronário e carregamento na distribuição de tensões em prótese fixa de três elementos / Effect of post, ferule presence and loading on stress distribution in 3-unit fixed parcial denture

Silva, Gisele Rodrigues da, 1982- 12 July 2012 (has links)
Orientador: Luís Roberto Marcondes Martins / Tese (doutorado) - Universidade Estadual de Campinas, Faculdade de Odontologia de Piracicaba / Made available in DSpace on 2018-08-21T16:51:03Z (GMT). No. of bitstreams: 1 Silva_GiseleRodriguesda_D.pdf: 2969310 bytes, checksum: 065fbdffc0e741bd55d3cb562acde2e8 (MD5) Previous issue date: 2012 / Resumo: O objetivo deste estudo foi investigar a influência do retentor intrarradicular, altura do remanescente coronário e tipo de carregamento virtualmente simulado, no comportamento biomecânico de prótese fixa anterior de 3 elementos. Quatro modelos tridimensionais de elementos finitos foram criados comparando-se o tipo de retentor nos dentes pilares (fibra de vidro ou núcleo metálico fundido) e a altura do remanescente coronário (0 e 2 mm). Para simular o tipo de carregamento foram considerados dois níveis de aplicação da força: 1- simulação de contato protrusivo (PRT): 200 N distribuídos nas cristas marginais palatinas dos incisivos superiores, sendo 50 N em cada crista marginal, a 45o do longo eixo do dente e 2- simulação de contato em lateralidade canina (LAT): 200 N aplicados na palatina do canino a 15º. Todos os materiais foram considerados homogêneos, lineares, elásticos e isotrópicos com exceção do pino de fibra de vidro, que foi considerado transversalmente isotrópico. O problema estrutural foi solucionado computacionalmente pelo Método de Elementos Finitos (MEF), em análise estrutural estática. A coerência da simulação foi observada pela análise do deslocamento e pelas tensões de von Mises. O deslocamento foi analisado de forma qualitativa e quantitativa comparando-se a região de deslocamento máximo sofrido pela prótese. Em seguida, foram comparadas as tensões máximas principais ocorridas na região de conexão entre pôntico e dentes pilares, na raiz do incisivo central, do canino e nas interfaces pino-dentina radicular e núcleo de preenchimento-dentina. Concluiu-se que as tensões de tração são concentradas entre pôntico/ pilar e na palatina dos dentes pilares da prótese fixa anterior. Sendo que a protrusão gera maior concentração de tensão máxima principal de tração nos dentes pilares e gera deslocamento duas vezes maior do que a lateralidade. Ademais, a presença de remanescente coronário melhora a distribuição das tensões e o pino de fibra de vidro mostrou-se adequado em prótese fixa anterior de 3 elementos / Abstract: The aim of this study was to investigate the influence of post, load condition and ferule presence in abutment teeth on the stress distribution in the anterior three-unit fixed dental prosthesis (FDP) made of lithium dissilicate. Four three-dimensional finite element (FE) models were created comparing the type of post using on the abutment teeth in two levels (fiberglass post and cast post-and-core) and the coronal remaining in two levels (with or without ferule presence). Two load conditions were applied: 1- 200 N was distributed on palatine marginal ridge of incisive, with 50 N in each ridge, under a 45o angle with the long axis of the tooth, simulating the protrusive contact or 2- 200N was applied on palatine of canine at 15o. All materials were considered homogeneous, linear elastic, and isotropic, with the exception of the glass fiber post, which was considered transversally isotropic. Analysis by Finite Elements Method (FEM), was performed structural analysis. The displacement and Von Mises stress was applied to analyze the coherence o simulation. The displacement was analyzed by quality and quantity resuts in region of maximum prostheses displacement. Maximum principal stress was used as a criterion to compare the study factors. The stress distribution was compared in a descriptive way in the area of the connector, along the interface post/dentin and core/dentin and on abutment dentin teeth. In conclusion, the highest tensile stress was observed in the connector areas and on palatine abutments roots surfaces. The protrusion causes higher stress and displacement than canine guide. The ferrule presence in the abutment teeth reduced the maximum principal tensile stresses on tooth-restoration complex and the fiberglass post seems to improve the stress distribution on anterior 3-unit fixed-dental prostheses / Doutorado / Dentística / Doutora em Clínica Odontológica
36

Influencia do reembasamento com resina composta na resistencia a extrusão de retentores intra-radiculares de fibra de vidro / Influence of resin composite relining on the extrusion strengh of intraradicular fiber glass posts

Pedrosa Filho, Celso de Freitas 24 November 2006 (has links)
Orientador: Luis Roberto Marcondes Martins / Tese (doutorado) - Universidade Estadual de Campinas, Faculdade de Odontologia de Piracicaba / Made available in DSpace on 2018-08-07T21:42:27Z (GMT). No. of bitstreams: 1 PedrosaFilho_CelsodeFreitas_D.pdf: 1514708 bytes, checksum: 68479f75bac6f0d3bdbb5ec943719f31 (MD5) Previous issue date: 2006 / Resumo: Neste estudo avaliou-se a resistência ao cisalhamento por extrusão de pinos de fibra de vidro, reembasados ou não com compósito, cimentados com cimento resinoso em dentina intra-radicular, avaliando os segmentos cervical, médio e apical. Selecionaram-se 20 incisivos bovinos com dimensões semelhantes, removendo a porção coronária, padronizando o comprimento das raízes em 16 mm. Após, incluiu-se as raízes em resina acrílica, realizando tratamento endodôntico e, então o preparo dos espaços para os pinos, dividindoas, em seguida, aleatoriamente em dois grupos com dez amostras cada. Os elementos do grupo 1 receberam pinos de fibra de vidro somente cimentados, e do grupo 2 pinos de fibra de vidro reembasados com compósito e posteriormente cimentados. Ao término dos procedimentos de cimentação, realizou-se a secção dos segmentos radiculares, submetendo, então, os corpos-de-prova ao teste push-out em máquina de ensaios universal, através de ponta ativa cilíndrica com 1 mm de diâmetro, à velocidade de 0,5 mm/min, até extrusão do retentor. Obteve-se os seguintes valores médios de resistência de união, em MPa: grupo 1, terços cervical = 6,24 ± 2,68(b), médio = 4,27 ± 2,00(b) e apical = 4,46 ± 2,82(b); grupo 2, terços cervical = 11,83 ± 1,69(a), médio = 11,81 ± 3,86(a) e apical = 10,39 ± 2,44(a). Submeteram-se os valores à análise de variância e ao teste de Tukey com nível de significância de 5%, indicadas acima através de letras diferentes. Os pinos de fibra de vidro reembasados com compósito apresentaram valores estatisticamente superiores de união em todos os segmentos radiculares quando comparados com pinos somente cimentados. Observou-se também a ausência de diferença significativa entre os terços radiculares avaliados para cada grupo distintamente. Os resultados demonstraram que a técnica de reembasamento mostrou-se efetiva em melhorar a retenção do pino de fibra de vidro estudado / Abstract: This study evaluated the bond strength of fiber posts, relined or not with composite resin, luted with resinous cement to radicular dentin, evaluating cervical, median and apical root segments. Twenty bovine incisors, with similar dimensions, were selected and cut 16 mm from the apical limit. The roots were embedded in acrylic resin and the radicular canals were root treated and post space prepared with a depth of 9 mm. Samples were randomly assigned to two groups of ten roots each. Group 1 received glass fiber posts (Fibrekor) luted with dual-cure resin cement (RelyX ARC) in association with a bonding system (Adper Single Bond). In Group 2 the same type of posts were relined with composite (P-60) for further cementation with the same materials used in Group 1. After cementation procedures roots were sectioned transversally and three sections, from cervical, medium and apical thirds were obtained. Push-out test was performed in a universal testing machine with a 1 mm diameter steel rod at cross-head speed of 0,5 mm/min until post extrusion. Collected data was statistically analyzed by twoway ANOVA and Tukey HSD test (p<0,05). The measured retention strengths for cervical, medium and apical thirds were: Group 1, 6.24 ± 2.68(b), 4.27 ± 2.00(b) and 4.46 ± 2.82(b) ; Group 2, 11.83 ± 1.69(a), 11.81 ± 3.86(a) and 10.39 ± 2.44(a). Glass fiber composite relined posts presented statistically higher retention values in cervical, medium and apical thirds when compared to non-relined posts. Within each group, no differences were found among radicular thirds. The results indicate that the tested technique showed effective improvement of glass fiber post retention strength / Doutorado / Dentística / Doutor em Clínica Odontológica