• Refine Query
  • Source
  • Publication year
  • to
  • Language
  • 6
  • 4
  • 3
  • 1
  • Tagged with
  • 17
  • 17
  • 4
  • 4
  • 4
  • 4
  • 4
  • 3
  • 3
  • 2
  • 2
  • 2
  • 2
  • 2
  • 2
  • About
  • The Global ETD Search service is a free service for researchers to find electronic theses and dissertations. This service is provided by the Networked Digital Library of Theses and Dissertations.
    Our metadata is collected from universities around the world. If you manage a university/consortium/country archive and want to be added, details can be found on the NDLTD website.
11

Estudo experimental do processo de rotomoldagem: efeitos sobre a morfologia e estabilidade dimensional / Experimental study of rotational moulding process: effect on the morphology and dimensional stability

Comisso, Tiago Boni 03 October 2011 (has links)
Made available in DSpace on 2017-07-21T20:42:45Z (GMT). No. of bitstreams: 1 Tiago Boni Comisso.pdf: 10111078 bytes, checksum: 8216bf27a8a3e1b801b4d8d101212fd8 (MD5) Previous issue date: 2011-10-03 / In the present study the warpage of rotationally molded parts of a linear low density polyethylene (LLDPE) was investigated. The effect of different processing factors as part thickness, cooling condition and diameter of the venting tube was evaluated. In addition to the rotational molding experiments, an alternative experimental technique, denominated “Hot Press”, was also applied to investigate the warpage of two different grades of LLDPE under typical rotational molding conditions, which means slow cooling from only one side. Crystallinity and spherulitic morphology along the thickness of the rotationally molded parts were studied by Differential Scanning Calorimetry and Polarized Light Optical Microscopy. It is shown that the warpage increases with the increase of the cooling rate. Increase of diameter of the venting tube is more effective in reducing the warpage of rotationally molded parts mainly for lower cooling rates. In hot press experiments the grade of LLDPE with lower melt flow index and higher flexural strength presented lower warpage. Part thickness affects the warpage in hot press experiments only for faster cooling rates. In general, crystallinity and spherulitic diameter are lower in positions along the rotationally molded part thickness where the cooling rate is faster. / No presente estudo o empenamento de peças de polietileno linear de baixa densidade (PELBD) moldadas por rotomoldagem foi investigado. O efeito de diferentes fatores como espessura da peça, taxa de resfriamento e diâmetro de tubo de ventilação foi avaliado. Em adição aos experimentos de rotomoldagem, uma técnica alternativa denominada “Hot Press” foi também aplicada para investigar o empenamento de dois diferentes PELBD sob condições típicas da rotomoldagem quanto ao resfriamento assimétrico. Cristalinidade e morfologia esferulítica ao longo da espessura das peças rotomoldadas foram avaliadas por Calorimetria Exploratória Diferencial (DSC) e Microscopia Ótica de Luz Polarizada. Verificou-se que o grau de empenamento aumenta com o aumento da taxa de resfriamento. O aumento do diâmetro do tubo de ventilação é mais efetivo na redução do empenamento principalmente em menores taxas de resfriamento. Nos experimentos de “Hot Press” o PELBD com menor índice de fluidez e maior módulo de flexão apresentou menor empenamento. Nos experimentos de “Hot Press” a espessura das peças afetou o empenamento somente para taxas de resfriamento mais rápidas. Em geral, a cristalinidade e o tamanho de esferulitos se mostraram menores nas posições ao longo da espessura das peças rotomodadas onde as taxas de resfriamento eram mais rápidas.
12

The urban hybrid, vol.1 and vol.2.

January 2004 (has links)
Tung Kwok Wah Henri. / "Architecture Department, Chinese University of Hong Kong, Master of Architecture Programme 2003-2004, design report." / Chapter 01. --- The Story Line --- p.p.01 - p.06 / Chapter 02. --- The System --- p.p.07 - p.08 / Chapter 03. --- Design Vol. 1 - the fabric --- p.p.09 - p.11 / Chapter 04. --- Design Vol. 2 - 1/2 park + 1/2 plant --- p.p.12 - p.26 / Chapter 05. --- The research part A - Newater plant (Singapore) --- p.p.27 - p.37 / Chapter 06. --- The researh part B - Water Background --- p.p.38 - p.48 / Chapter 07. --- The research part C - Rotomolding --- p.p.49 - p.57
13

Optimisation et simulation du rotomoulage réactif / Optimization and simulation of reactive rotational molding

Riviere, Sylvain 05 December 2012 (has links)
Le rotomoulage réactif est un procédé de fabrication de pièces creuses en polymère où la synthèse du matériau intervient pendant la mise en œuvre. Cette méthode présente plusieurs avantages comparée à la méthode traditionnelle utilisant des poudres thermoplastiques : réduction du temps de cycle, utilisation possible de matériaux techniques, et baisse de la consommation d'énergie et du coût des matières premières. Cependant le rotomoulage réactif est plus complexe à mettre en œuvre car la polymérisation provoque un changement important et rapide de la viscosité. Une des solutions pour optimiser ce procédé est de simuler l'écoulement du système réactif pendant la mise en œuvre.Pour ce travail nous avons utilisé un polyuréthane thermodurcissable. Des analyses thermiques et rhéologiques ont permis d'étudier les phénomènes de gélification et de vitrification du matériau et le diagramme Temps-Température-Transformation a été établi. Le comportement rhéocinétique du système a également été modélisé.Le procédé a été simulé en utilisant un code de calcul basé sur la méthode « Smoothed Particle Hydrodynamics » (SPH). Ce code a été développé par notre équipe et plusieurs améliorations ont été apportées au cours de cette étude. Pour effectuer des simulations plus réalistes en utilisant un plus grand nombre de particules, la première amélioration a consisté à accélérer la résolution des calculs. Ensuite l'évolution de la viscosité a été prise en compte grâce à l'utilisation d'un modèle rhéocinétique et une nouvelle condition limite a été développée pour simuler l'adhésion du polymère sur la paroi du moule. Les modifications nécessaires à la simulation d'écoulements 3D ont également été apportées au code SPH. / Reactive rotational molding is a process to manufacture hollow plastic parts where synthesis occurs during the shaping. This method has several advantages compared to traditional rotomolding using thermoplastic powders: shorter cycle time, possible use of high performance materials, and decrease of energy consumption and raw materials costs. However reactive rotational molding is more complex to implement mainly because of the important and quick change of viscosity occurring during polymerization. One of the solutions to optimize this process is to simulate the reactive system flow during processing.In this work we used thermoset polyurethane as reactive system. Thanks to thermal and rheological analysis, gelation and vitrification phenomena were studied and Time-Temperature-Transformation diagram was established. Material chemiorheological behavior was also modeled.The process has been simulated using a solver based on Smoothed Particle Hydrodynamics (SPH) method. This solver was developed in our research team and several improvements have been added during this study. To be able to simulate realistic flows with a high number of particles, the first improvement was to accelerate the resolution of calculations. Then the change of viscosity has been taken into account using a chemiorheological model and a new boundary condition was developed to simulate adhesion of polymer on the mold wall. To be able to simulate 3D flows, the needed modifications have been also added to the SPH solver.
14

Modélisation et simulation du rotomoulage réactif du polyuréthane / Modelling and simulation of reactive rotational of polyurethane

Hamidi, Abdelmoumen 09 September 2015 (has links)
Le procédé du rotomoulage réactif est une technologie de fabrication de pièces creuses de taille et géométrie très variés. Une compréhension et une modélisation des phénomènes physiques qui interviennent dans les différentes étapes de la fabrication apportent une contribution importante à la maîtrise de ce procédé. Les travaux abordés dans cette thèse se situent dans le cadre d'un programme plus général visant le contrôle et le pilotage du rotomoulage réactif.Tout d'abord, une caractérisation et modélisation de la cinétique du polyuréthane thermodurcissable en mode dynamique est réalisé suivie par des mesures rhéologiques afin d'établir des lois rhéocinétique ainsi que des lois du comportement viscoélastiques du système réactionnel. Ces lois de comportement sont établies conformément aux conditions réelles de la mise en œuvre du matériau.Ensuite, nous simulons le procédé du rotomoulage en utilisant un code de calcul basé sur la méthode « Smoothed Particle Hydrodynamics » (SPH), développé par notre équipe, en implémentant des nouveaux paramètres physiques: le caractère non-newtonien du mélange réactionnel et les effets de tension superficielle.Le modèle de tension de surface en 2 et 3D développé dans cette thèse permet la détection explicite de l'interface séparant le fluide réactif de l'air. Puis, nous utilisons l'interpolation lagrangienne ou la régression circulaire pour construire la courbe d'interface en 2D et la surface d'interface en 3D sera reconstruite via la régression sphérique. Quant à la modélisation de l'écoulement du fluide non-newtonien, une loi de puissance décrivant l'évolution de la viscosité en fonction du taux de cisaillement a été intégrée dans le solveur pour décrire le caractère non-newtonien du mélange réactionnel durant sa mise en œuvre. Ces paramètres physiques implémentés dans le code ont été validé par une série de cas de tests en 2 et 3D.L'intégration des effets de tension de surface et la prise en compte du caractère non-newtonien du fluide réactif nous ont permis de mieux présenter la mouillabilité de la surface interne du moule et l'étalement des différentes couches du polymères.Mots clés : rotomoulage réactif, polyuréthane thermodurcissable, rhéocinétique, Smoothed Particle Hydrodynamics, tension de surface, fluide non-newtonien, simulation. / Reactive Rotational molding (RRM) is a process for manufacturing hollow plastic products with no weld lines, in virtually any shape, size, color and configuration, using biaxial rotation and high temperature. Understanding and modelling of physical phenomena provide a great contribution for process control that is the purpose of a more general program.Firstly, a characterization and the kinetic modeling of the thermoset polyurethane are performed in anisothermal conditions followed by rheological measurements in order to establish rheokinetik model and the the viscoelastic behavior of the reactive system according with RRM conditions.Afterwards, to simulate the RRM, Smoothed Particles Hydrodynamics (SPH) method is applied which is suited method to simulate the fluid flow with free surface such as occurs at RRM. This solver is developed by our team. Modelling and simulating reactive system flow depend on different parameters; the physical phenomena involved are: surface tension force and non-newtonian fluid behavior.The surface tension method has been successfully applied to simulate RRM using SPH solver taking into account free surface tension force. Surface tension force is given explicitly in the current model. After detecting the boundary particles, the interface is locally fitted by using Lagrangian interpolation polynomial or fitting circle in 2D and by using fitting sphere in 3D, respectively. To study the non-newtonian fluid flow during RRM, a power law describes the evolution of the viscosity versus shear rate was adopted to describe the viscoelastic nature of the reactive fluid during its shaping.The implementation of surface tension and viscoelasticity allows us to present the wettability of internal surface of the mold and the spreading of different polymers layers.Keywords : Reactive rotational molding, thermoset polyurethane, rheokinetik, Smoothed Particle Hydrodynamics, surface tension, non-newtonian fluid, simulation.
15

Caractérisation et mise en œuvre de systèmes réactifs polyamide et polyépoxyde formulés pour le rotomoulage de liners de stockage hyperbare / Characterization and transformation of polyamide and polyepoxyde reactive systems formulated for rotomolded liners of high pressure storage

Lecocq, Eva 21 December 2012 (has links)
Ce travail s’inscrit dans le développement de formulations performantes et processables pour les liners de réservoirs de stockage hyperbare. Une large gamme de formulations à base polyamide et polyépoxyde a ainsi été synthétisée en conditions contrôlées, représentatives du procédé de rotomoulage. Les systèmes polyamide ont été modifiés par copolymérisation statistique et les polyépoxydes par une phase dispersée micro- ou nano-structurée avec des thermoplastiques de haute Tg ou des copolymères blocs. Les propriétés morphologiques, thermiques, mécaniques et barrière de chaque formulation ont été caractérisées et confrontées au cahier des charges du matériau. En parallèle, l’influence des conditions opératoires et de la formulation sur les rhéocinétiques de polymérisation, de cristallisation, de gélification et/ou de séparation de phase a ainsi été établie. L’ensemble de ces résultats a été mis à profit afin d’identifier des relations structures – propriétés – processabilité en vue de l’application. Afin de valider le potentiel des formulations retenues, ces dernières ont été rotomoulées en conditions opératoires variables avec un suivi in situ de l’écoulement et ex situ de la viscosité. Ce travail a permis d’établir les fenêtres de processabilité de chaque formulation et de comprendre l’origine des défauts d’écoulement. / The aim of this present study is to develop efficient and processable formulations for the liners of high pressure storage tank. A wide range of formulations based on polyamide and polyepoxide has been synthesized under controlled conditions representative of the rotomolding process. The polyamide system has been modified by copolymerization and the polyepoxyde system by a micro- or nano-structured dispersed phase with high Tg thermoplastics or block copolymers. The morphological, thermal, mechanical and barrier properties of each formulation were characterized and compared to the specifications of the material. In parallel, the influence of operating conditions and formulation on the rheokinetics of polymerization, crystallization, gelation and / or phase separation has been established. All of these results have been exploited to identify structure - property - processability relationships for the application. To validate the potential of selected formulations, they were rotationally molded in variable operating conditions with flow monitoring and rheological measure. This work has established the processing windows of each formulation and has allowed an understanding of the origin of flow defects.
16

Elaboration et mise en forme de matériaux polymères à base de l’ε-caprolactame (PA6) par le procédé de rotomoulage réactif / Synthesis and processing of polymeric materials based on the ε-caprolactam (PA6) by reactive rotational molding process

Barhoumi, Najoua 09 December 2013 (has links)
Cette thèse porte sur le rotomoulage réactif de polyamide 6. Ce procédé a la particularité de présenter des cycles thermiques relativement réduit et de fabriquer des polymères sur mesure contrairement à son homologue conventionnelle. La voie envisagée pour la synthèse in situ de PA6 est la polymérisation anionique de l’ε-caprolactame par ouverture de cycle. Le Caprolactamate de sodium et le bromure de caprolactame-magnésium ont été utilisés comme catalyseurs, et l’hexaméthylène dicarbamoyl dicaprolactame a été employé comme activateur. L’étude rhéocinétique de deux systèmes réactifs lactames qui ont été utilisé à différentes compositions et températures a permis de déterminer une formulation appropriée aux exigences du procédé (faible viscosité initiale du système réactif, temps de polymérisation court...). La simultanéité des phénomènes de polymérisation et de cristallisation aux faibles températures à été observé à l’aide des résultats du suivi cinétique par DSC. La mise en forme par la technique de rotomoulage a été réalisée sur une installation pilote de rotomoulage associée à un système d’acquisition de température par télémesure radio. La comparaison des propriétés des articles en PA 6 obtenus par voie réactive par rapport a ceux obtenus par voie fondue, a montré un gain au niveau du temps de cycle et une amélioration des propriétés mécaniques du matériau notamment dans le domaine des faibles déformations. Le rotomoulage de la bicouche PA6/PE-GMA a été ainsi étudié, le contrôle des mécanismes réactionnels mis en jeu à l’interface par rhéologie, durant la formation de la couche de polymère PA6 par voie anionique sur une couche de PE-GMA a été effectué dans un rhéomètre, une bonne adhésion à l’interface a été observé. La faisabilité d’élaboration de nanocomposite PA 6/argile par le procède de rotomoulage réactif a été testé, les caractérisations physico-chimiques et les observations morphologiques ont été étudiés afin d’évaluer l’état de dispersion et la nature des interactions. Durant cette étude, nous avons mesurés la faisabilité de l’intercalation et le gonflement de l’argile dans le monomère ε- caprolactame et estimer la possibilité d’avoir une morphologie exfolié des nanocomposites élaborés par le procédé de rotomoulage réactif. / A reactive rotational molding (RRM) process was developed to obtain a PA6 by activated anionic ring-opening polymerization of epsilon-caprolactam (APA6). Sodium caprolactamate (C10) and caprolactam magnesium bromide (C1) were employed as catalysts, and difunctional hexamethylene-1,6-dicarbamoylcaprolactam (C20) was used as an activator. The kinetics of the anionic polymerization of ε-caprolactam into polyamide 6 was monitored through dynamic rheology and differential scanning calorimetry measurements. The effect of the processing parameters, such as the polymerization temperature, different catalyst/activator combinations and concentrations, on the kinetics of polymerization is discussed. A temperature of 150°C was demonstrated to be the most appropriate. It was also found that crystallization may occur during PA6 polymerization and that the combination C1/C20 was well suited as it permitted a suitable induction time. Isoviscosity curves were drawn in order to determine the available processing window for RRM. The properties of the obtained APA6 were compared with those of a conventionally rotomolded PA6. Results pointed at lower cycle times and increased tensile properties at weak deformation. Additionally, rotational molding of the bilayer PA6/PE-GMA has been studied, the control of the reactions mechanisms involved in the interface by rheology , during formation of the anionically PA6 polymer layer on a PE- GMA layer was carried out in a rheometer , a good adhesion at the interface was observed. The feasibility of developing nanocomposite PA 6/clay by reactive rotational molding process has been tested; the physico-chemical characterization and morphological observations were studied to assess the state of dispersion and the nature of interactions. During this study, we measured the feasibility of intercalation and swelling the clay in the ε-caprolactam monomer and estimate the possibility of having morphology of exfoliated nanocomposites prepared by reactive rotational molding process.
17

Development of a Particle Flow Test for Rotational Molding

Whatcott, Russell B. 30 June 2008 (has links) (PDF)
One of the current testing method (the Dry Flow test) to qualify resin for use in production in the rotomolding process has been shown to have many flaws in both equipment and procedure. Research was done here to investigate a possible alternative that could eliminate some of these testing deficiencies. By reducing equipment and operator errors, the testing of materials becomes more valuable of an exercise. The Angular Flow test developed in this research can increase repeatability. By coming to understand the rotational molding process better, an evaluation that can give more valid information was devised.